Effect of Mg17Al12 precipitate on corrosion behavior of AZ91D magnesium alloy

被引:45
|
作者
Ko, YJ [1 ]
Yim, CD
Lim, JD
Shin, KS
机构
[1] Hyundai Motor Co, R&D Div, Mat Res Team, Kyonggi Do 445706, South Korea
[2] Kia Motors Co, Kyonggi Do 445706, South Korea
[3] Seoul Natl Univ, Sch Mat Sci & Engn, BK21 Mat Educ & Res Div, Seoul 151742, South Korea
[4] POSTECH, CAAM, Pohang 790784, South Korea
来源
关键词
Mg17Al12; precipitate; magnesium alloy; corrosion behavior; heat treatment;
D O I
10.4028/www.scientific.net/MSF.419-422.851
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructure of an AZ91D magnesium alloy mainly consists of Mg17Al12 phase and magnesium matrix. Although the Mg17Al12 phase is a principal precipitate in the Mg-Al alloy system, its role on corrosion behavior has not yet been systematically investigated. In the present study, the effect of Mg17Al12 phase on corrosion behavior of an AZ91D magnesium alloy was investigated in a quantitative manner. A wide range of volume fraction of the Mg17Al12 phase was obtained by varying aging temperature and time after solution heat treatment. The corrosion potential measurements and salt spray tests were carried out on the specimens with various volume fractions of the Mg17Al12 phase. The results of these tests showed that the corrosion resistance increased with increasing volume fraction of the Mg17Al12 phase. It was found that the network structure of the Mg17Al12 phase increased the corrosion resistance of an AZ91D alloy by acting as an effective barrier against corrosion.
引用
收藏
页码:851 / 856
页数:6
相关论文
共 50 条
  • [41] BENEFIT EFFECT OF LOW ADDITION YTTRIUM ON THE PHASE αmg AND EUTECTIC αmg + γ(Mg17Al12) IN AZ91 ALLOY
    Mikusek, D.
    Rapiejko, C.
    Andrzejczak, A.
    Pacyniak, T.
    ARCHIVES OF METALLURGY AND MATERIALS, 2021, 66 (01) : 57 - 63
  • [42] Fretting wear behavior of AZ91D magnesium alloy
    陈安华
    黄伟九
    李兆峰
    Transactions of Nonferrous Metals Society of China, 2006, (S3) : 1879 - 1883
  • [43] Hot tearing behavior of AZ91D magnesium alloy
    Honggang Zhong
    Zenghuang Lin
    Qingyou Han
    Jiangfeng Song
    Meicheng Chen
    Xiangru Chen
    Lijuan Li
    Qijie Zhai
    Journal of Magnesium and Alloys, 2024, 12 (08) : 3431 - 3440
  • [44] Fretting wear behavior of AZ91D magnesium alloy
    Chen An-hua
    Huang Wei-jiu
    Li Zhao-feng
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1879 - S1883
  • [45] Effect of Pb Addition on the Discontinuous and Continuous Mg17Al12-β Precipitate During Solidification of AZ91 Magnesium Alloy
    Boby, Arun
    Pillai, U. T. S.
    Pai, B. C.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2013, 66 (02) : 105 - 108
  • [46] Interaction Between Basal Slip and a Mg17Al12 Precipitate in Magnesium
    Liao, Min
    Li, B.
    Horstemeyer, M. F.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2014, 45A (08): : 3661 - 3669
  • [47] Effect of Pb Addition on the Discontinuous and Continuous Mg17Al12-β Precipitate During Solidification of AZ91 Magnesium Alloy
    Arun Boby
    U. T. S. Pillai
    B. C. Pai
    Transactions of the Indian Institute of Metals, 2013, 66 : 105 - 108
  • [48] Heat treatment and kinetics of precipitation of β-Mg17Al12 phase in AZ91 alloy
    Fatmi, M.
    Djemli, A.
    Ouali, A.
    Chihi, T.
    Ghebouli, M. A.
    Belhouchet, H.
    RESULTS IN PHYSICS, 2018, 10 : 693 - 698
  • [49] Tensile and fatigue behavior of AZ91D magnesium alloy
    Bag, A
    Zhou, W
    JOURNAL OF MATERIALS SCIENCE LETTERS, 2001, 20 (05) : 457 - 459
  • [50] Investigation on aging behavior of AZ91D magnesium alloy
    Liu, Guanjun
    Li, Wenfang
    Peng, Jihua
    ADVANCES IN SUPERALLOYS, PTS 1 AND 2, 2011, 146-147 : 1386 - +