Direct Rolling of TiCp/Ti-6Al-4V Composite for Improved Microstructure, Mechanical Properties, and High-Temperature Oxidation Resistance

被引:2
|
作者
Jia, Yi [1 ,2 ]
Zhang, Changjiang [2 ,3 ]
Zhang, Shuzhi [2 ,3 ]
Feng, Hong [3 ]
Han, Fuyin [3 ]
Han, Jianchao [1 ,2 ]
Cong, Yan [4 ]
Chen, Yuyong [4 ]
机构
[1] Taiyuan Univ Technol, Coll Mech & Vehicle Engn, Taiyuan 030024, Peoples R China
[2] Minist Educ, Engn Res Ctr Adv Met Composites Forming Technol &, Taiyuan 030024, Peoples R China
[3] Taiyuan Univ Technol, Coll Mat Sci & Engn, Taiyuan 030024, Peoples R China
[4] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
direct rolling; mechanical properties; microstructure; oxidation resistance; titanium matrix composites; TENSILE PROPERTIES; TI-6AL-4V/TIC COMPOSITE; CYCLIC OXIDATION; HEAT-TREATMENT; BEHAVIOR; ALLOYS;
D O I
10.1002/adem.202100079
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Herein, the 5 vol% TiCp/Ti-6Al-4V composite is prepared by induction skull melting (ISM) and direct rolling in near-beta phase region. The microstructure, mechanical properties, and high-temperature oxidation behavior of the as-cast and as-rolled composites are systematically investigated. The investigations of microstructure reveal that the as-cast coarse alpha/beta lamellar matrix microstructure is translated to refined bimodal microstructure after direct rolling. And the coarse and segregated TiC particles tend to be refined and uniformly distributed in the matrix. Tensile test results exhibit that a well-matched strength and elongation is obtained after direct rolling. The tensile strength at room temperature (RT) and high temperature (650 degrees C) increases to 1291.9 and 472.5 MPa, respectively, while the as-rolled composite maintains a good elongation of 6.7% and 26.8%, respectively. The strengthening mechanism can be attributed to grain boundary strengthening and the load-bearing capability of TiC. Isothermal oxidation test indicates that as-rolled composite exhibits better oxidation resistance than as-cast composite both at 550 and 650 degrees C. The improved oxidation resistance is mainly a result of the significant refinement of oxides and consequently retarding the diffusion process.
引用
收藏
页数:10
相关论文
共 50 条
  • [31] Effect of Initial Microstructure on High-Temperature Dynamic Deformation of Ti-6Al-4V Alloy
    Gangireddy, Sindhura
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (10): : 4581 - 4594
  • [32] Effect of Initial Microstructure on High-Temperature Dynamic Deformation of Ti-6Al-4V Alloy
    Sindhura Gangireddy
    Metallurgical and Materials Transactions A, 2018, 49 : 4581 - 4594
  • [33] HIGH-TEMPERATURE NITROGEN IMPLANTATION OF TI-6AL-4V .1. MICROSTRUCTURE CHARACTERIZATION
    KUSTAS, FM
    MISRA, MS
    WEI, R
    WILBUR, PJ
    KNAPP, JA
    SURFACE & COATINGS TECHNOLOGY, 1992, 51 (1-3): : 100 - 105
  • [34] Chemical oxidation of Ti-6Al-4V for improved wear and corrosion resistance
    Biswas, A.
    Srikant, P. V. S.
    Manna, I.
    Chatterjee, U. K.
    Majumdar, J. Dutta
    SURFACE ENGINEERING, 2008, 24 (06) : 442 - 446
  • [35] Microstructure and properties of titanium and Ti-6Al-4V with and without TiCp reinforcement deformed by transformation superplasticity
    Schuh, C
    Zimmer, W
    Dunand, DC
    CREEP BEHAVIOR OF ADVANCED MATERIALS FOR THE 21ST CENTURY, 1999, : 61 - 70
  • [36] High-temperature oxidation and its kinetics study of Ti-6Al-4V alloys in air
    Takahashi T.
    Minamino Y.
    Hirazawa H.
    Ouchi T.
    Keikinzoku/Journal of Japan Institute of Light Metals, 2016, 66 (06): : 306 - 311
  • [37] High temperature mechanical behaviour of TiC particulate reinforced Ti-6Al-4V composite
    Zhu, SJ
    Mukherji, D
    Chen, W
    Lu, YX
    Wang, ZG
    Wahi, RP
    PROGRESS IN MECHANICAL BEHAVIOUR OF MATERIALS (ICM8), VOL 3: ADVANCE MATERIALS AND MODELLING OF MECHANICAL BEHAVIOUR, 1999, : 815 - 817
  • [38] Effect of Direct Rolling Process on Microstructure and Mechanical Properties of the Electron Beam Cold Hearth Melting Ti-6Al-4V Alloy
    Zhang, Haoze
    Yi, Jianhong
    Wang, Junsheng
    Xiao, Han
    Wang, Meng
    Wang, Wei
    METALS, 2022, 12 (12)
  • [39] Microstructure and mechanical properties of plasma sprayed HA/YSZ/Ti-6Al-4V composite coatings
    Khor, KA
    Gu, YW
    Pan, D
    Cheang, P
    BIOMATERIALS, 2004, 25 (18) : 4009 - 4017
  • [40] Analysis of microstructure and mechanical properties of additive repaired Ti-6Al-4V by Direct Energy Deposition
    Shrestha, Sulochana
    Panakarajupally, Ragavendra P.
    Kannan, Manigandan
    Morscher, Gregory
    Gyekenyesi, Andrew L.
    Scott-Emuakpor, Onome E.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 806