Ageing kinetics and strength of airborne-particle abraded 3Y-TZP ceramics

被引:40
|
作者
Cotic, Jasna [1 ]
Jevnikar, Peter [1 ]
Kocjan, Andraz [2 ]
机构
[1] Univ Ljubljana, Fac Med, Dept Prosthodont, Hrvatski Trg 6, SI-1000 Ljubljana, Slovenia
[2] Jozef Stefan Inst, Dept Nanostruct Mat, Jamova 39, SI-1000 Ljubljana, Slovenia
关键词
Zirconia; Airborne-particle abrasion; Low-temperature degradation; Phase transformation; Flexural strength; LOW-TEMPERATURE DEGRADATION; Y-TZP CERAMICS; STABILIZED TETRAGONAL ZIRCONIA; HYDROTHERMAL DEGRADATION; DENTAL APPLICATIONS; PHASE-TRANSFORMATION; DAMAGE;
D O I
10.1016/j.dental.2017.04.014
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective. The combined effects of alumina airborne-particle abrasion and prolonged in vitro ageing on the flexural strength of 3Y-TZP ceramic have been studied. The aim was to identify the different effects on the surface and subsurface regions that govern the performance of this popular bioceramic known for its susceptibility to low-temperature degradation (LTD). Methods.<bold> </bold>As-sintered or airborne-particle abraded 3Y-TZP discs were subjected to ageing at 134 degrees C for up to 480 h. Biaxial flexural strength was measured and the relative amount of monoclinic phase determined using X-ray diffraction. The transformed zone depth (TZD) was observed on cross-sections with scanning electron microscopy coupled with a focused ion beam. Segmented linear regression was used to analyze the flexural strength and TZD as functions of the ageing time. Results. A two-step linear ageing kinetics was detected in airborne-particle abraded specimens, reflecting the different microstructures through which the LTD proceeds into the bulk. A 10 mu m thick altered zone under the abraded surface was involved in both the surface strengthening and the increased ageing resistance. When the zone was annihilated by the LTD, the strength of the ceramic specimens and the speed of LTD returned to the values measured before abrasion. Even at prolonged ageing times, the strength of abraded groups was not lower than that of as-sintered groups. Significance. Both the ageing kinetics and the flexural strength were prominently affected by airborne-particle abrasion, which altered the subsurface microstructure and phase composition. Airborne-particle abrasion was not harmful to the 3Y-TZP ceramics stability. (C) 2017 The Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:847 / 856
页数:10
相关论文
共 50 条
  • [41] Stability of 3Y-TZP nano zirconia powder after hydrothermal ageing treatment
    Ahmed, Shafique
    Zou, Lifong
    Yan, Haixue
    ADVANCES IN APPLIED CERAMICS, 2022, 121 (5-8) : 159 - 165
  • [42] Influence of Aging on Biaxial Flexural Strength and Hardness of Translucent 3Y-TZP
    Moqbel, Nawal M.
    Al-Akhali, Majed
    Wille, Sebastian
    Kern, Matthias
    MATERIALS, 2020, 13 (01) : 27
  • [43] In vivo ageing of zirconia dental ceramics - Part II: Highly-translucent and rapid-sintered 3Y-TZP
    Cotic, Jasna
    Kocjan, Andraz
    Panchevska, Sanja
    Kosmac, Tomaz
    Jevnikar, Peter
    DENTAL MATERIALS, 2021, 37 (03) : 454 - 463
  • [44] Degradation resistance of 3Y-TZP ceramics sintered using spark plasma sintering
    Chintapalli, R.
    Marro, F. G.
    Valle, J. A.
    Yan, H.
    Reece, M. J.
    Anglada, M.
    5TH INTERNATIONAL EEIGM/AMASE/FORGEMAT CONFERENCE ON ADVANCED MATERIALS RESEARCH, 2009, 5
  • [45] Effect of holding time on the mechanical properties and microstructural evaluation of 3Y-TZP ceramics
    Golieskardi, M.
    Satgunam, M.
    Ragurajan, D.
    JOURNAL OF THE AUSTRALIAN CERAMIC SOCIETY, 2017, 53 (02) : 1001 - 1006
  • [46] Effect of testing parameters on wear properties of alumina strengthen 3Y-TZP ceramics
    Zhao, Shihai
    Xin, Shaobo
    Wang, Xiaohui
    Liang, Xiaoping
    HIGH-PERFORMANCE CERAMICS IV, PTS 1-3, 2007, 336-338 : 2468 - +
  • [47] Effect of BaTiO3 addition on structures and mechanical properties of 3Y-TZP ceramics
    Yang, B
    Chen, XM
    Liu, XQ
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2000, 20 (08) : 1153 - 1158
  • [48] Characterization of 3Y-TZP/TiO2 hybrid experimental dental ceramics
    Miranda, Ranulfo Benedito de Paula
    Ussui, Valter
    Lazar, Dolores Ribeiro Ricci
    de Lima, Nelson Batista
    Marchi, Juliana
    Cesar, Paulo Francisco
    CERAMICS INTERNATIONAL, 2023, 49 (10) : 15734 - 15740
  • [49] Comparative analysis of flexural strength of 3D printed and milled 4Y-TZP and 3Y-TZP zirconia
    Kyung, Kyu-Young
    Park, Ji-Man
    Heo, Seong-Joo
    Koak, Jai-Young
    Kim, Seong-Kyun
    Ahn, Jin-Soo
    Yi, Yuseung
    JOURNAL OF PROSTHETIC DENTISTRY, 2024, 131 (03): : 529.e1 - 529.e9
  • [50] PRESSURELESS BONDING OF 3Y-TZP TO TITANIUM
    KOGURE, E
    HOSHINO, H
    IIDA, T
    MITAMURA, T
    NIPPON SERAMIKKUSU KYOKAI GAKUJUTSU RONBUNSHI-JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1988, 96 (11): : 1057 - 1065