This study evaluated the effect of air-blowing variables on the microtensile bond strength (mu TBS) of two all-in-one adhesives. A bonding agent was applied to the flat dentin surface of extracted bovine teeth, and the surface left undisturbed for 20 seconds. Gentle or intensive air-blowing was applied for five seconds, and the adhesive photopolymerized for 10 seconds. Resin composite paste was placed and cured after each bonding treatment. Specimens were subjected to mu TBS test with a crosshead speed of 1.0 mm/min. Data were statistically analyzed using ANOVA, followed by Bonferroni post hoc test. When Clearfil tri-S Bond was bonded to dentin, the mu TBS value of specimens applied with intensive air-blowing was significantly higher than that applied with gentle air-blowing (p < 0.01). On the other hand, with Fluoro Bond Shake One, the mu TBS value of specimens applied with intensive air-blowing was significantly lower than that applied with gentle air-blowing (p < 0.01).
引用
收藏
页码:664 / 668
页数:5
相关论文
共 50 条
  • [31] The effect of organic solvents on one-bottle adhesives' bond strength to enamel and dentin
    Reis, AF
    Oliveira, MT
    Giannini, M
    De Goes, MF
    Rueggeberg, FA
    OPERATIVE DENTISTRY, 2003, 28 (06) : 700 - 706
  • [32] Effect of bur-cut dentin on bond strength using two all-in-one and one two-step adhesive systems
    Koase, K
    Inoue, S
    Noda, M
    Tanaka, T
    Kawamoto, C
    Takahashi, A
    Nakaoki, Y
    Sano, H
    JOURNAL OF ADHESIVE DENTISTRY, 2004, 6 (02): : 97 - 104
  • [33] Relationship between water status in dentin and interfacial morphology in all-in-one adhesives
    Yoshida, Eiji
    Uno, Sigeru
    Nodasaka, Yoshinobu
    Kaga, Msayuki
    Hirano, Susumu
    DENTAL MATERIALS, 2007, 23 (05) : 556 - 560
  • [34] Influence of hydrostatic pulpal pressure on the microtensile bond strength of all-in-one self-etching adhesives
    Hosaka, Keiichi
    Nakajima, Masatoshi
    Monticelli, Francesca
    Carrilho, Marcela
    Yamauti, Monica
    Aksornmuang, Juthatip
    Nishitani, Yoshihiro
    Tayh, Franklin R.
    Pashley, David H.
    Tagami, Junji
    JOURNAL OF ADHESIVE DENTISTRY, 2007, 9 (05): : 437 - 442
  • [35] Two-year bond strengths of "all-in-one" adhesives to dentine
    Walter, Ricardo
    Swift, Edward J., Jr.
    Nagaoka, Hiroko
    Chung, Yunro
    Bartholomew, Whitley
    Braswell, Krista M.
    Pereira, Patricia N. R.
    JOURNAL OF DENTISTRY, 2012, 40 (07) : 549 - 555
  • [36] Relationship between air-blowing duration and bond strengths of three adhesive systems to dentin after thermal aging
    Daneshmehr, Leila
    Ozer, Fusun
    Mante, Francis K.
    Blatz, Markus B.
    DENTAL MATERIALS JOURNAL, 2013, 32 (05) : 767 - 774
  • [37] EFFECT OF SURFACE-TREATMENT ON BOND STRENGTH OF DENTIN ADHESIVES
    STANGEL, I
    OSTRO, E
    BENKO, J
    JOURNAL OF DENTAL RESEARCH, 1986, 65 : 174 - 174
  • [38] Effect of light intensity for adhesives on shear bond strength to dentin
    Shinkai, Koichi
    Suzuki, Shiro
    Katoh, Yoshiroh
    DENTAL MATERIALS JOURNAL, 2008, 27 (05) : 660 - 665
  • [39] Effect of moisture on shear bond strength of dentin adhesives.
    Arellano, A
    Lopes, LMP
    LopezAreal, B
    Leitao, J
    JOURNAL OF DENTAL RESEARCH, 1997, 76 (05) : 1110 - 1110
  • [40] The Effect of Endodontic Irrigants on the Microtensile Bond Strength of Dentin Adhesives
    Yurdaguven, Haktan
    Tanalp, Jale
    Toydemir, Burcu
    Mohseni, Kambiz
    Soyman, Muebin
    Bayirli, Guenduez
    JOURNAL OF ENDODONTICS, 2009, 35 (09) : 1259 - 1263