NEW ASPECTS CONCERNING Co-Cr ALLOYS

被引:0
|
作者
Ardelean, Lavinia [1 ]
Reclaru, Lucien [2 ]
Bortun, Cristina Maria [1 ]
Ghiban, Brandusa [3 ]
Rusu, Laura Cristina [1 ]
机构
[1] Victor Babes Univ Med & Pharm, Timisoara, Romania
[2] PXGroup, La Chaux De Fonds, Switzerland
[3] Politehn Univ, Bucharest, Romania
来源
METALURGIA INTERNATIONAL | 2010年 / 15卷 / 09期
关键词
cobalt-chromium dental alloys; corrosion; microstructure; phase analysis; hardness properties; electrochemical testing;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A new generation of cobalt-chronnum alloys doped with precious metals (Au, Pt, Ru) recently came on the market with the idea to improve the corrosion resistance The goal of this study was to verify this hypothesis, by testing 4 different such alloys Different investigations were carried out microstructural identification of the constituents by energy-dispersive X-ray spectroscopy, hardness values determination and electrochemical testing. The microstructures of alloys A and D exhibited round "inclusions" with a diameter up to 0 1 mm The hardness values for all 4 tested alloys are lower than of Co-Cr classical alloy Potentiodynanuc polarization curves in linear system of alloys A to D in comparison with a conventional Co-Cr alloy reveal important differences in the behavior of the studied alloys (A- D) as compared to the conventional Co-Cr alloy From the point of view of corrosion behaviour, the classical Co-Cr alloy is the best material followed by the alloys B and C with addition of respectively 4 % and 25 % precious metals The worst alloys were A and D, with only addition of 2 % of Au Due to their poor behaviour, using the dental Co-Cr alloys enriched with precious metals, as an alternative to conventional Co-Cr alloys, is not justified
引用
收藏
页码:31 / 35
页数:5
相关论文
共 50 条
  • [21] Stability of bioactivated Co-Cr alloys in biological environment
    Sovar, M. M.
    Ducu, C.
    Iordachescu, D.
    Demetrescu, I.
    BIOCERAMICS, VOL 20, PTS 1 AND 2, 2008, 361-363 : 737 - +
  • [22] Transition from external to internal oxidation of Co-Cr alloys
    He, YD
    Ma, J
    Li, ZW
    Gao, W
    MATERIALS RESEARCH INNOVATIONS, 2005, 9 (04) : 106 - 108
  • [23] Metal-on-metal wear testing of Co-Cr alloys
    Wang, KK
    Wang, A
    Gustavson, LJ
    COBALT-BASE ALLOYS FOR BIOMEDICAL APPLICATIONS, 1999, 1365 : 135 - 144
  • [24] Soldering and refusing influence on fatigue strength of Co-Cr alloys
    Henriques, GEP
    Consani, S
    Rollo, JMDA
    Silva, FA
    JOURNAL OF DENTAL RESEARCH, 1997, 76 (05) : 998 - 998
  • [25] CASTING VARIABLES AND MECHANICAL-PROPERTIES OF CO-CR ALLOYS
    PADDON, JM
    BATCHELOR, RF
    WILSON, AD
    JOURNAL OF DENTAL RESEARCH, 1975, 54 : L113 - L113
  • [26] ETCHING PATTERNS OF CO-CR ALLOYS FOR BONDED CAST RESTORATIONS
    EKSTRAND, K
    RUYTER, IE
    JOURNAL OF DENTAL RESEARCH, 1987, 66 (09) : 1479 - 1484
  • [27] In vitro biocompatibility of Co-Cr alloys with different content of copper
    Department of Prosthetics School of Stomatology, China Medical University, Shenyang
    110002, China
    不详
    110002, China
    不详
    110002, China
    不详
    110002, China
    不详
    110011, China
    不详
    110016, China
    Cailiao Yanjiu Xuebao, 8 (627-633):
  • [28] Flexible and Tough Superelastic Co-Cr Alloys for Biomedical Applications
    Odaira, Takumi
    Xu, Sheng
    Hirata, Kenji
    Xu, Xiao
    Omori, Toshihiro
    Ueki, Kosuke
    Ueda, Kyosuke
    Narushima, Takayuki
    Nagasako, Makoto
    Harjo, Stefanus
    Kawasaki, Takuro
    Bodnarova, Lucie
    Sedlak, Petr
    Seiner, Hanus
    Kainuma, Ryosuke
    ADVANCED MATERIALS, 2022, 34 (27)
  • [29] Electrochemical behavior of Co-Cr and Ni-Cr dental cast alloys
    Viswanathan S. SAJI
    Han-Cheol CHOE
    TransactionsofNonferrousMetalsSocietyofChina, 2009, 19 (04) : 785 - 790
  • [30] Electrochemical Properties of Ni-Cr and Co-Cr Alloys Used in Prosthodontics
    Pochrzast, M.
    Marciniak, J.
    Wrobel, K.
    Baczkowski, B.
    ENVIRONMENTAL DEGRADATION OF ENGINEERING & MATERIALS ENGINEERING AND TECHNOLOGIES, 2012, 183 : 143 - +