Static SIMS studies of carboxylic acids on gold and aluminium-magnesium alloy surfaces

被引:12
|
作者
Miller, DJ [1 ]
Sun, L
Walzak, MJ
McIntyre, NS
Chvedov, D
Rosenfeld, A
机构
[1] Univ Western Ontario, Western Sci Ctr, Surface Sci Western, London, ON N6A 5B7, Canada
[2] Alcan Int Ltd, Kingston Res & Dev Ctr, Kingston, ON K7L 5L9, Canada
关键词
ToF-SIMS; carboxylic acids; aluminium-magnesium alloys; magnesium soap formation; C-type crystals;
D O I
10.1002/sia.1556
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Static secondary ion mass spectrometry was used to study the surface reactions and lateral distributions of fatty carboxylic acid molecules on sputter-deposited gold and aluminium surfaces, as well as commercial aluminium-magnesium alloy surfaces, cleaned using UV/ozone. Films were prepared by spin coating dilute solutions of stearic acid and lauric acid onto the above surfaces. These carboxylic acids were shown to react with the oxide formed on the aluminium and aluminum-magnesium alloy substrates to produce a deprotonated acid anion, stabilized by the formation of a magnesium soap on the aluminium-magnesium alloy surface. Secondary ion imaging of stearic acid films revealed the formation of C-type crystals. Copyright (C) 2003 John Wiley Sons, Ltd.
引用
收藏
页码:463 / 476
页数:14
相关论文
共 50 条
  • [21] EFFECT OF HYDROEXTRUSIVE DEFORMATION ON STRUCTURE AND PROPERTIES OF AN ALUMINIUM-MAGNESIUM AGEING ALLOY
    KOMAROVA, MF
    LERINMAN, RM
    BUYNOV, NN
    BULYCHEV, DK
    RODIONOV, KP
    YELAGIN, VI
    FEDEROV, VM
    PHYSICS OF METALS AND METALLOGRAPHY-USSR, 1969, 27 (02): : 99 - &
  • [22] Influence of natural seawater variables on the corrosion behaviour of aluminium-magnesium alloy
    Marques, M. J. F.
    Benedetti, A.
    Castelli, F.
    Delucchi, M.
    Faimali, M.
    Delsante, S.
    Valenza, F.
    Garaventa, F.
    Pavanello, G.
    Basseguy, R.
    BIOELECTROCHEMISTRY, 2023, 149
  • [23] Thermal oxidation induced during laser cleaning of an aluminium-magnesium alloy
    Th. Dimogerontakis
    R. Oltra
    O. Heintz
    Applied Physics A, 2005, 81 : 1173 - 1179
  • [24] Thermal oxidation induced during laser cleaning of an aluminium-magnesium alloy
    Dimogerontakis, T
    Oltra, R
    Heintz, O
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2005, 81 (06): : 1173 - 1179
  • [25] FORMATION AND ANNEALING BEHAVIOUR OF MULTI-FAULTED LOOPS IN AN ALUMINIUM-MAGNESIUM ALLOY
    KRITZINGER, S
    SMALLMAN, RE
    DOBSON, PS
    ACTA METALLURGICA, 1969, 17 (01): : 49 - +
  • [26] Evaluation of tensile behaviour of 5754 aluminium-magnesium alloy at cold and warm temperatures
    Ozturk, F.
    Toros, S.
    Pekel, H.
    MATERIALS SCIENCE AND TECHNOLOGY, 2009, 25 (07) : 919 - 924
  • [27] Investigation of the Explosive Characteristics of Ammonium Nitrate and Aluminium-Magnesium Alloy Powder Mixtures
    Paszula, Jozef
    Maranda, Andrzej
    Kukfisz, Bozena
    Putko, Paulina
    ENERGIES, 2022, 15 (23)
  • [28] Propagation mode of Portevin Le Chatelier plastic instabilities in an aluminium-magnesium alloy
    Zeghloul, A
    MlihaTouati, M
    Bakir, S
    SCRIPTA MATERIALIA, 1996, 35 (09) : 1083 - 1087
  • [29] Machine learning-based precise monitoring of aluminium-magnesium alloy dust
    Zhao, Fengyu
    Gao, Wei
    Lu, Jianxin
    Jiang, Haipeng
    JOURNAL OF LOSS PREVENTION IN THE PROCESS INDUSTRIES, 2024, 92
  • [30] NICOTINIC ACID AS AN INHIBITOR FOR CORROSION OF ALUMINIUM-MAGNESIUM ALLOY IN HYDROCHLORIC ACID SOLUTIONS
    SUBRAMAN.DV
    CHAR, TLR
    ANTI-CORROSION, 1967, 14 (06): : 14 - &