Temperature and concentrations limits for fullerenes C60 and C70 as polymer degradation inhibitors

被引:0
|
作者
Troitskii, BB [1 ]
Khokhlova, LV [1 ]
Konev, AN [1 ]
Denisova, VN [1 ]
Novikova, MA [1 ]
Lopatin, MA [1 ]
机构
[1] Russian Acad Sci, Razuvaev Inst Organomet Chem, Nizhnii Novgorod 603950, Russia
关键词
D O I
暂无
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
For the thermal and thermooxidative degradation in fullerene (C-60, C-70)-Polymer (PMMA, polystyrene) systems, concentration limits were observed for the stabilizing effect of fullerenes that depend on the solubility of the fullerene in a polymer: for polystyrene and PMMA, these values are 4 x 10(-3) and 8 x 10(-3) Mol/kg of fullerene, respectively. Thermal and thermooxidative degradation occurred in the presence of fullerenes were also characterized by the existence of temperature limits for the effective action of inhibitors. For polystyrene-based systems containing C-60 or C-70, the temperature limit of thermal degradation was 380degreesC; for PMMA-based systems, this parameter amounted to 339 and 336degreesC for C-60 and C-70, respectively. For the thermooxidative degradation of these polymers and a polycarbonate, the temperature range 335-340degreesC was the highest temperature limit for fullerene C-60 as an antioxidant, which was much lower than 370degreesC, the temperature corresponding to the onset of the intense oxidation of fullerene.
引用
收藏
页码:951 / 956
页数:6
相关论文
共 50 条
  • [21] Estimation of the efficiency of the C60 and C70 fullerenes as inhibitors of the radical chain oxidation of cumene
    Galimov, Dim, I
    Gazeeva, Dilara R.
    Sabirov, Denis Sh
    Bulgakov, Ramil G.
    FULLERENES NANOTUBES AND CARBON NANOSTRUCTURES, 2023, 31 (02) : 176 - 181
  • [22] Distribution of C60 and C70 fullerenes in the extraction system (C60 + C70)-α-pinene-ethanol-H2O
    O. V. Arapov
    N. D. Abovskii
    N. A. Charykov
    V. I. Seregin
    K. V. Nekrasov
    V. I. Gerasimov
    Russian Journal of Applied Chemistry, 2006, 79 : 166 - 168
  • [23] PREPARATION AND UV VISIBLE SPECTRA OF FULLERENES C60 AND C70
    HARE, JP
    KROTO, HW
    TAYLOR, R
    CHEMICAL PHYSICS LETTERS, 1991, 177 (4-5) : 394 - 398
  • [25] Spectrophotometric analysis of C60 and C70 fullerenes in the toluene solutions
    Anikina, NS
    Zaginaichenko, SY
    Maistrenko, MI
    Zolotarenko, AD
    Sivak, GA
    Schur, DV
    Teslenko, LO
    HYDROGEN MATERIALS SCIENCE AND CHEMISTRY OF CARBON NANOMATERIALS, 2004, 172 : 207 - 216
  • [26] Technology for manufacture of pure fullerenes C60, C70 and a concentrate of higher fullerenes
    Yu. S. Grushko
    V. P. Sedov
    V. A. Shilin
    Russian Journal of Applied Chemistry, 2007, 80 : 448 - 455
  • [27] Molecular complexes of fullerenes C60 and C70 with saturated amines
    Konarev, DV
    Kovalevsky, AY
    Litvinov, AL
    Drichko, NV
    Tarasov, BP
    Coppens, P
    Lyubovskaya, RN
    JOURNAL OF SOLID STATE CHEMISTRY, 2002, 168 (02) : 474 - 485
  • [28] Synthesis and structure of allylated derivatives of fullerenes C60 and C70
    V. P. Gubskaya
    L. N. Islamova
    G. M. Fazleeva
    Sh. K. Latypov
    A. F. Saifina
    A. T. Gubaidullin
    D. R. Sharafutdinova
    I. A. Nuretdinov
    O. G. Sinyashin
    Russian Chemical Bulletin, 2016, 65 : 1556 - 1565
  • [29] Stability of C60 and C70 fullerenes toward corpuscular and γ radiation
    Cataldo, Franco
    Strazzulla, Giovanni
    Iglesias-Groth, Susana
    MONTHLY NOTICES OF THE ROYAL ASTRONOMICAL SOCIETY, 2009, 394 (02) : 615 - 623
  • [30] Molecular complexes of fullerenes C60 and C70 with organic donors
    Lyubovskaya, RN
    Konarev, DV
    RECENT ADVANCES IN THE CHEMISTRY AND PHYSICS OF FULLERENES AND RELATED MATERIAL, VOL 7, 1999, 99 (12): : 615 - 627