RESEARCH ON HR6W MANUFACTURED REHEATER OUTLET HEADER OF THE ADVANCED USC BOILER

被引:0
|
作者
Tian Zhihao [1 ]
Zhu Yufeng [1 ]
Lu Xiaoli [1 ]
Wang Yu [1 ]
Yang Kaiyin [1 ]
Wang Chongbin [1 ]
机构
[1] Shanghai Boiler Works Co, Shanghai, Peoples R China
关键词
653 degrees C reheat steam; HR6W; 617B; material performance;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper reports the performance of HR6W iron-nickel based alloy and 617B nickel based alloy which are the candidate material for high temperature reheater outlet header of advanced secondary reheat ultra-supercritical unit boiler with reheat steam 653 degrees C, and analysis the applicable temperature range of the material. As a result, HR6W is the appropriate material to manufacture high temperature reheater outlet header of A-USC boiler with parameters 620 degrees C /653 degrees C/653 degrees C.
引用
收藏
页码:326 / 335
页数:10
相关论文
共 34 条
  • [31] 超超临界HR6W钢平板钨极氩弧焊接焊缝的微观组织和性能
    陈勇
    湖北理工学院学报, 2021, 37 (05) : 40 - 43
  • [32] 高温CO环境下耐热合金HR6W和740H的腐蚀行为
    李玉峰
    梁志远
    邓世丰
    桂雍
    邵怀爽
    赵钦新
    西安交通大学学报, 2020, (05) : 179 - 188
  • [33] High-temperature corrosion of Fe-Ni-based alloy HR6W, Ni-based alloys Haynes 282 and Inconel 740 in supercritical water at 450 °C and 25 MPa
    Guo, Shuwei
    Xu, Donghai
    Jiang, Guanyu
    Jing, Zefeng
    Wang, Shuzhong
    Lv, Heng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 878
  • [34] High-temperature corrosion of an Fe-Ni-based alloy HR6W under various conditions at 750 °C and 810 °C: Effect of the temperature, water vapor, simulated ash and SO2
    Liang, Zhiyuan
    Guo, Tingshan
    Deng, Shifeng
    Zhao, Qinxin
    MATERIALS CHEMISTRY AND PHYSICS, 2020, 256