RESEARCH ON HR6W MANUFACTURED REHEATER OUTLET HEADER OF THE ADVANCED USC BOILER

被引:0
|
作者
Tian Zhihao [1 ]
Zhu Yufeng [1 ]
Lu Xiaoli [1 ]
Wang Yu [1 ]
Yang Kaiyin [1 ]
Wang Chongbin [1 ]
机构
[1] Shanghai Boiler Works Co, Shanghai, Peoples R China
关键词
653 degrees C reheat steam; HR6W; 617B; material performance;
D O I
暂无
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper reports the performance of HR6W iron-nickel based alloy and 617B nickel based alloy which are the candidate material for high temperature reheater outlet header of advanced secondary reheat ultra-supercritical unit boiler with reheat steam 653 degrees C, and analysis the applicable temperature range of the material. As a result, HR6W is the appropriate material to manufacture high temperature reheater outlet header of A-USC boiler with parameters 620 degrees C /653 degrees C/653 degrees C.
引用
收藏
页码:326 / 335
页数:10
相关论文
共 34 条
  • [1] Creep Rupture Properties of HR6W for Advanced-USC Boilers
    Saito, Nobuhiko
    Komai, Nobuyoshi
    ADVANCES IN MATERIALS TECHNOLOGY FOR FOSSIL POWER PLANTS: PROCEEDINGS FROM THE SIXTH INTERNATIONAL CONFERENCE, 2010, 2011, : 962 - 971
  • [2] Research on the superheater header material for 700°C USC boiler
    Shanghai Boiler Works Co., Ltd, Shanghai Boiler Works Co., Ltd, No, 250 Huaning Road, Minhang, Shanghai
    200245, China
    Int, Conf. Power Eng.,
  • [3] LONG-TERM CREEP RUPTURE PROPERTIES AND MICROSTRUCTURES IN HR6W (44Ni-23Cr-7W) FOR A-USC BOILERS
    Saito, Nobuhiko
    Komai, Nobuyoshi
    Hashimoto, Keita
    Kitamura, Masaki
    ADVANCES IN MATERIALS TECHNOLOGY FOR FOSSIL POWER PLANTS: PROCEEDINGS FROM THE EIGHTH INTERNATIONAL CONFERENCE, 2016, 2016, : 418 - 428
  • [4] Isothermal, Thermo-Mechanical and Bithermal Fatigue Life of Ni Base Alloy HR6W for Piping in 700°C USC Power Plants
    Noguchi, Yasutaka
    Okada, Hirokazu
    Semba, Hiroyuki
    Yoshizawa, Mitsuru
    11TH INTERNATIONAL CONFERENCE ON THE MECHANICAL BEHAVIOR OF MATERIALS (ICM11), 2011, 10 : 1127 - 1132
  • [5] Creep-fatigue properties of Fe-Ni base alloy HR6W for piping in 700C USC power plants
    Noguchi, Yasutaka
    Miyahara, Mitsuo
    Okada, Hirokazu
    Igarashi, Masaaki
    Ogawa, Kazuhiro
    Zairyo/Journal of the Society of Materials Science, Japan, 2008, 57 (06) : 569 - 575
  • [6] Failure analysis of 12Cr1MoVG outlet header for the reheater of the boiler under high temperature and high-pressure environment
    Yu, Ting
    Ying, Chenkai
    Wang, Zimeng
    Gao, Zhen
    Zhong, Fengping
    CANADIAN METALLURGICAL QUARTERLY, 2024,
  • [7] CREEP PROPERTIES AND STRENGTHENING MECHANISMS IN 23Cr-45Ni-7W (HR6W) ALLOY AND Ni-BASE SUPERALLOYS FOR 700°C A-USC BOILERS
    Semba, H.
    Okada, H.
    Igarashi, M.
    ADVANCES IN MATERIALS TECHNOLOGY FOR FOSSIL POWER PLANTS, 2008, : 168 - 184
  • [8] Impact of Temperature on Low-Cycle Fatigue Characteristics of the HR6W Alloy
    Junak, Grzegorz
    Marek, Anzelina
    Paduchowicz, Michal
    MATERIALS, 2021, 14 (22)
  • [9] Precipitation Behavior of Wrought Fe-Ni-Based Alloy HR6W
    Iwamaru, Arata
    Hisazawa, Hiromu
    Terada, Yoshihiro
    JOURNAL OF THE JAPAN INSTITUTE OF METALS AND MATERIALS, 2019, 83 (01) : 30 - 35
  • [10] Use of the Wilshire Equations to Correlate and Extrapolate Creep Data of HR6W and Sanicro 25
    Cedro, Vito, III
    Garcia, Christian
    Render, Mark
    MATERIALS, 2018, 11 (09)