Improved thermal shock resistance of magnesia-graphite refractories by the addition of MgO-C pellets

被引:51
|
作者
Zhu, Tianbin [1 ,2 ]
Li, Yawei [1 ]
Sang, Shaobai [1 ]
Xie, Zhipeng [2 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Peoples R China
[2] Tsinghua Univ, State Key Lab New Ceram & Fine Proc, Sch Mat Sci & Engn, Beijing 100084, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
Thermal shock resistance; Microstructure; MgO-C pellets; MgO-C refractories; IN-SITU FORMATION; LOW-CARBON; MECHANICAL-PROPERTIES; NANO CARBON; MICROSTRUCTURAL EVOLUTION; CHEMICAL-REACTIONS; AL; NANOCARBON; FRACTURE; ANTIOXIDANTS;
D O I
10.1016/j.matdes.2017.03.054
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Magnesia-graphite (MgO-C) refractories with 12-20 wt% carbon contents are extensively used for the taphole sleeve bricks, bottom blowing elements, slag line bricks, etc. in steelmaking operations. To reduce the carbon content but to have the same or even superior thermal shock resistance with commercial available material compositions (14 wt% flaky graphite), we report here a new approach based on the granulating treatment of flaky graphite to improve the thermal shock resistance of MgO-C refractories (10 wt% flaky graphite). MgO-C pellets are firstly prepared by the crushing granulation method, and then introduced into such refractories. Addition of MgO-C pellets has no apparent influence on their flexural strength, but enhances their flexural strength after thermal shocks and residual strength ratio. Particularly, when 10 wt% flaky graphite of the specimens is replaced totally by MgO-C pellets, their thermal shock resistance is superior to that of the specimens containing 14 wt% flaky graphite. This new method opens up possibilities to obtain MgO-C refractories with improved thermal shock resistance. (C) 2017 Elsevier Ltd. All rights reserved.
引用
收藏
页码:16 / 23
页数:8
相关论文
共 50 条
  • [31] THE ROLE OF GRAPHITE IN THE THERMAL-SHOCK RESISTANCE OF REFRACTORIES
    COOPER, CF
    ALEXANDER, IC
    HAMPSON, CJ
    TRANSACTIONS AND JOURNAL OF THE BRITISH CERAMIC SOCIETY, 1985, 84 (02): : 57 - 62
  • [32] Influence of flake graphite coated MgO particles on thermal shock resistance and fracture behaviour of MgO-C refractories based on Brazilian splitting test with digital image correlation method and acoustic emission technique
    Xu, Xiaofeng
    Li, Yawei
    Zhu, Tianbin
    Dai, Yajie
    Xue, Zhengliang
    Yan, Wen
    Jin, Shengli
    CERAMICS INTERNATIONAL, 2025, 51 (05) : 6458 - 6467
  • [33] Thermal shock behaviour of carbon bonded MgO-C refractories with inorganic micro- and nano-additions
    Aneziris, Christos G.
    Klippel, Uwe
    CFI-CERAMIC FORUM INTERNATIONAL, 2006, 83 (10): : E50 - E52
  • [34] Phenolic resins with carbo-resin additions for improved MgO-C refractories
    Aneziris, CG
    Borzov, D
    Ulbricht, J
    Suren, J
    Dern, H
    EURO CERAMICS VIII, PTS 1-3, 2004, 264-268 : 1767 - 1770
  • [36] Oxidation Resistance and Wetting Behavior of MgO-C Refractories: Effect of Carbon Content
    Liu, Zhaoyang
    Yu, Jingkun
    Yang, Xin
    Jin, Endong
    Yuan, Lei
    MATERIALS, 2018, 11 (06):
  • [37] INFLUENCE OF Zn ADDITION ON PROPERTIES OF METAL COMPOSITE LOW CARBON MgO-C REFRACTORIES
    Ma, Chengliang
    Ren, Zhen
    Ma, Hua
    Meng, Dongdong
    PROCEEDINGS OF THE UNIFIED INTERNATIONAL TECHNICAL CONFERENCE ON REFRACTORIES (UNITECR 2013), 2014, : 727 - 731
  • [38] HOT STRENGTH AND THERMAL-SHOCK RESISTANCE OF MAGNESIA-CARBON REFRACTORIES
    FRANKLIN, SA
    TUCKER, BJS
    BRITISH CERAMIC TRANSACTIONS, 1995, 94 (04): : 151 - 156
  • [39] Study on microstructures and mechanical strength of MgO-C refractories with cobalt-loaded expanded graphite
    Wang, Yilong
    Zhang, Wenli
    Zeng, Xiongfeng
    Huang, Jiankun
    Chen, Yuejun
    Wei, Hengyong
    Tu, Junbo
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2024, 21 (03) : 2312 - 2320
  • [40] Thermal shock resistance of magnesia chrome refractories-experimental and criterial evaluation
    Wojsa, J.
    Podworny, J.
    Suwak, R.
    CERAMICS INTERNATIONAL, 2013, 39 (01) : 1 - 12