The effect of calcination temperature on the performance of Co3O4-Bi2O3 as a heterogeneous catalyst of peroxymonosulfate

被引:1
|
作者
Zhang, Guangshan [1 ]
Hu, Limin [1 ]
Wang, Peng [1 ]
Yuan, Yixing [1 ]
机构
[1] Harbin Inst Technol, Sch Environm, State Key Lab Urban Water Resource & Environm, Harbin 150090, Heilongjiang, Peoples R China
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
EFFICIENT DEGRADATION; OXIDATION;
D O I
10.1088/1755-1315/94/1/012029
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
In this work, a time-saving microwave-assisted method for synthesis of Co3O4-Bi2O3 was reported. The synthesized Co3O4-Bi2O3 samples were characterized with different techniques to probe their crystalline structures and morphologies. The catalytic performances of synthesized Co3O4-Bi2O3 as peroxymonosulfate activator were evaluated by the degradation of bisphenol A. The effect of calcination temperature on Co3O4-Bi2O3 products was explored and the result showed that the sample calcined at 400 degrees C possessing superior catalytic activity.
引用
收藏
页数:4
相关论文
共 50 条
  • [21] DeNOx performance of Ag/Al2O3 catalyst by n-dodecane: Effect of calcination temperature
    Yoon, Dal Young
    Park, Joo-Hyoung
    Kang, Ho-Chul
    Kim, Pyung Soon
    Nam, In-Sik
    Yeo, Gwon Koo
    Kil, Jeong Ki
    Cha, Moon-Soon
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2011, 101 (3-4) : 275 - 282
  • [22] Effect of Sintering Temperature on the Photothermal Spectrum of Bi2O3-TiO2-Co3O4-ZnO Ceramics
    Rizwan, Z.
    Zakaria, A.
    Hashim, M.
    Shaari, A. H.
    Yunus, W. M. M.
    INTERNATIONAL CONFERENCE ON ADVANCEMENT OF MATERIALS AND NANOTECHNOLOGY 2007, 2010, 1217 : 530 - 534
  • [23] Effect of Calcination Temperature on the Structure and Performance of Mn/Al2O3-TiO2 Catalyst in the Catalytic Oxidation of NO
    Mou Yi-Meng
    Liang Hong
    Li Shu-Hua
    Wu Shao-Tao
    Chen Yao
    Yu Xin-Wei
    CHINESE JOURNAL OF INORGANIC CHEMISTRY, 2016, 32 (04) : 602 - 608
  • [24] Effects of Calcination Temperature and Calcination Atmosphere on the Performance of Co3O4 Catalysts for the Catalytic Oxidation of Toluene
    Jiang, Sicheng
    You, Zhimin
    Tang, Ning
    PROCESSES, 2023, 11 (07)
  • [25] CuO-Co3O4@CeO2 as a heterogeneous catalyst for efficient degradation of 2,4-dichlorophenoxyacetic acid by peroxymonosulfate
    Li, Wei
    Li, Yuxin
    Zhang, Deyun
    Lan, Yeqing
    Guo, Jing
    JOURNAL OF HAZARDOUS MATERIALS, 2020, 381
  • [26] Effect of calcination and reaction conditions on the catalytic performance of Co-Ni/Al2O3 catalyst for CO hydrogenation
    Zare, Akbar
    Zare, Ahad
    Shiva, Mehdi
    Mirzaei, Ali Akbar
    JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, 2013, 19 (06) : 1858 - 1868
  • [27] Activation of Peroxymonosulfate by a CoAl2O4/Co2O3@γ-Al2O3 Catalyst for Efficient Phenol Degradation in Water
    Wei, Jingcheng
    Zhang, Jing
    Zhu, Bingyan
    Xue, Tingfeng
    Song, Zejia
    Li, Sumin
    Pan, Liwei
    JOURNAL OF ENVIRONMENTAL ENGINEERING, 2024, 150 (08)
  • [28] Effect of preparation method, loading of Co3O4 and calcination temperature on the physicochemical and catalytic properties of Co3O4/ZnO nanomaterials
    El -Mona, Sahar A.
    Ali, Laila I.
    Mahmoud, Hala R.
    Ibrahim, Marwa M.
    Naghmash, Mona A.
    MATERIALS CHEMISTRY AND PHYSICS, 2017, 185 : 44 - 54
  • [29] Effect of Calcination Temperature on Activity of Fe2O3–Al2O3 Nanocomposite Catalysts in CO Oxidation
    Anna M. Kremneva
    Alexander V. Fedorov
    Olga A. Bulavchenko
    Yury V. Knyazev
    Andrey A. Saraev
    Vadim A. Yakovlev
    Vasily V. Kaichev
    Catalysis Letters, 2020, 150 : 3377 - 3385
  • [30] Effect of Calcination Temperature of Support on the Performance of Co-Mo/MgO-Al2O3 Water-Gas Shift Catalyst
    Lian Yixin
    Wang Huifang
    Fang Weiping
    Yang Yiquan
    CHINESE JOURNAL OF CATALYSIS, 2009, 30 (06) : 549 - 554