共 50 条
Interfacial Compatibility on the Crystal Transformation of Isotactic Poly (1-Butene)/Herb Residue Composite
被引:16
|作者:
Wang, Bo
[1
,2
]
Mao, Shuangdan
[1
]
Lin, Fuhua
[2
,3
,4
]
Zhang, Mi
[4
]
Zhao, Yuying
[1
]
Zheng, Xiuhong
[1
]
Wang, Hui
[1
]
Luo, Jun
[5
]
机构:
[1] Taiyuan Univ Sci & Technol, Sch Chem & Biol Technol, Taiyuan 030021, Peoples R China
[2] Chinese Acad Sci, Guangzhou Inst Energy Convers, Key Lab Renewable Energy, Guangzhou 510640, Peoples R China
[3] Taiyuan Univ Sci & Technol, Sch Mat Sci & Engn, Taiyuan 030021, Peoples R China
[4] Shanxi Chem Res Inst Co Ltd, Taiyuan 030021, Peoples R China
[5] Guangzhou Fibre Prod Testing & Res Inst, Guangzhou 510220, Peoples R China
来源:
关键词:
isotactic polybutylene-1;
herb residue;
crystal transformation;
interfacial compatibility;
SILANE COUPLING AGENT;
CRYSTALLIZATION BEHAVIOR;
SURFACE MODIFICATION;
CELLULOSE;
POLYPROPYLENE;
POLYBUTENE-1;
ACID;
D O I:
10.3390/polym13101654
中图分类号:
O63 [高分子化学(高聚物)];
学科分类号:
070305 ;
080501 ;
081704 ;
摘要:
Isotactic poly (1-butene) (iPB) has excellent properties which are recognized as a green and energy saving product. However, the most stable and valuable crystal form I had a spontaneous transformation that took as long as seven days to complete. As a special solid waste, the herb residue (HR) is rich in cellulose which has great potential to accelerate the crystal transformation of the iPB. However, the polarity of HR results in the interface compatibility with non-polar iPB. In this study, the HR was modified by silane coupling agent (KH570) to obtain KHR and the iPB/HR composite was prepared. The FTIR spectrum was indicated that the organic functional groups of KH570 successfully graft onto the surface of HR and the water contact angle test was indicated that the hydrophilicity of the KHR was greatly decreased. The complete crystal transformation time is 7 days for iPB, 6 days for iPB+5% HR but only 3 days for iPB+5% KHR. The addition of the HR and KHR improve the thermal stability of the composite and this beneficial effect is more obvious for KHR. After annealing for 5 days, the physical properties value include tensile strength, flexural strength, and HDT of iPB+5% HR reach that of pure iPB after annealing for 7 days, but only 3 days for iPB+5% KHR. The TG analysis and SEM photographs give clear evidence that the beneficial effect of KH570 modified HR on improving the interface compatibility with iPB.