Degradation of outdoor exposed poly(1-trimethylsilyl)-1-propyne

被引:7
|
作者
Gallo, R
Pegoraro, M
Severini, F
Ipsale, S
Nisoli, E
机构
[1] Politecn Milan, Dipartimento Chim Ind & Ingn Chim G Natta, I-20133 Milan, Italy
[2] Univ Messina, Dipartimento Chim Ind, I-98100 Messina, Italy
[3] Assessorato Ambiente, I-98100 Messina, Italy
关键词
D O I
10.1016/S0141-3910(97)00046-3
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The outdoor ageing of poly(1-trimethylsilyl)-1-propyne (PTMSP) membranes has been studied mainly by means of differential scanning calorimetry (DSC), thermogravimetry, viscosimetry and infra-red spectroscopy. Membranes lose their integrity within 288 h of exposure. After exposure for 192 h the oxidation time at 523 K decreases from 25 to 0.5 min, while the starting temperature of degradation, as measured by DSC, changes from 543 K to 393 K and the viscosimetric molecular weight decreases five times. The high speed of the photodegradation process can be accounted for by the high oxygen solubility of this polymer. (C) 1997 Elsevier Science Limited.
引用
收藏
页码:247 / 250
页数:4
相关论文
共 50 条
  • [21] Control of permselectivity with surface modifications of poly[1-(trimethylsilyl)-1-propyne] membranes
    Uragami, T
    Doi, T
    Miyata, T
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 1999, 19 (05) : 405 - 409
  • [22] Separation of benzene using the poly[1-(trimethylsilyl)-1-propyne] blend membranes
    Takahashi, S
    Yoshida, Y
    Kamada, T
    Nakagawa, T
    KOBUNSHI RONBUNSHU, 2001, 58 (05) : 213 - 220
  • [23] Accelerated physical aging of thin poly[1-(trimethylsilyl)-1-propyne] films
    Dorkenoo, KD
    Pfromm, PH
    MACROMOLECULES, 2000, 33 (10) : 3747 - 3751
  • [24] Poly[1-(trimethylsilyl)-1-propyne] as a solvent resistance nanofiltration membrane material
    Volkov, A. V.
    Stamatialis, D. F.
    Khotimsky, V. S.
    Volkov, V. V.
    Wessling, M.
    Plate, N. A.
    JOURNAL OF MEMBRANE SCIENCE, 2006, 281 (1-2) : 351 - 357
  • [25] Crosslinking poly[ 1-(trimethylsilyl)-1-propyne] and its effect on physical stability
    Kelman, Scott D.
    Rowe, Brandon W.
    Bielawski, Christopher W.
    Pas, Steven J.
    Hill, Anita J.
    Paul, D. R.
    Freeman, B. D.
    JOURNAL OF MEMBRANE SCIENCE, 2008, 320 (1-2) : 123 - 134
  • [26] Hydrodynamic properties and conformation of poly[1-(trimethylsilyl)-1-propyne] molecules in solution
    Shtennikova, IN
    Kolbina, GF
    Khotimskii, VS
    Litvinova, EG
    Plate, NA
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA A & SERIYA B, 1998, 40 (10): : 1569 - 1576
  • [27] Poly[1-(trimethylsilyl)-1-propyne] and related polymers: synthesis, properties and functions
    Nagai, K
    Masuda, T
    Nakagawa, T
    Freeman, BD
    Pinnau, I
    PROGRESS IN POLYMER SCIENCE, 2001, 26 (05) : 721 - 798
  • [28] STUDIES ON APPLICATION OF SUBSTITUTED POLY(ACETYLENE) TO UV PHOTORESIST .1. UV DEGRADATION OF POLY[1-(TRIMETHYLSILYL)-1-PROPYNE] AND EFFECTS OF SENSITIZERS ON THE DEGRADATION
    TAKADA, K
    MATSUYA, H
    KISHIKI, H
    KOBUNSHI RONBUNSHU, 1987, 44 (12) : 905 - 910
  • [29] Comparison of gas diffusion in poly[1-(trimethylsilyl)-1-propyne] and poly(dimethylsiloxane) by atomistic modeling
    Yang, JS
    Choi, K
    Jo, WH
    MACROMOLECULAR THEORY AND SIMULATIONS, 2000, 9 (05) : 287 - 291
  • [30] CROSS-LINKED POLY[1-(TRIMETHYLSILYL)-1-PROPYNE] GAS SEPARATION MEMBRANES
    JIA, JP
    BAKER, GL
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1995, 210 : 86 - POLY