Hydrogen assisted crack initiation in metals under monotonic loading: A new experimental approach

被引:10
|
作者
Arora, Aman [1 ]
Kumar, Rakesh [1 ]
Singh, Harpreet [1 ]
Mahajan, Dhiraj K. [1 ]
机构
[1] Indian Inst Technol Ropar, Dept Mech Engn, Ropar Mech Mat Lab, Rupnagar 140001, Punjab, India
关键词
Hydrogen embrittlement; Digital image correlation; Electron backscattered diffraction; Crack initiation; Stress maps; ENHANCED LOCALIZED PLASTICITY; GRAIN-BOUNDARY FRACTURE; FATIGUE; DIFFUSION; CRITERION; NICKEL; NUCLEATION; STEELS; DAMAGE;
D O I
10.1016/j.tafmec.2021.102917
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Hydrogen is foreseen as a promising energy carrier that can control global warming by reducing CO2 emissions. However, hydrogen is associated with an embrittlement phenomenon that imparts substantial damage to the infrastructure by reducing the ductility, fracture strength, strength bearing capacity, etc., of metallic components. Therefore, understanding hydrogen-induced crack initiation mechanisms in metals are of prime importance. Greater insights into this critical phenomenon are expected if the hydrogen-induced crack initiation can be correlated with the local microstructure and corresponding stress-strain state towards their propensity for hydrogen accumulation. With this motivation, in this work, crack initiation is studied for the uncharged and hydrogen charged nickel specimens during in-situ tensile loading under the scanning electron microscope. By assuming the material to be elastic at low strains, a novel approach is implemented for generating the micro structural stress maps through strain and stiffness tensor extracted at each point in the region of interest on the specimen surface using high-resolution digital image correlation (HR-DIC) and Euler angles (given by electron backscattered diffraction data), respectively. Based on this analysis at low strain, the crack initiation sites for uncharged and hydrogen charged nickel specimens are correlated with microstructural maps of maximum Schmid factor, elastic modulus in the loading direction, hydrostatic stress, von Mises stress, and triaxiality factor. The analysis highlighted two independent factors responsible for hydrogen enhanced decohesion (HEDE) based intergranular failure observed only at the random grain boundaries, (i) strain localization due to hydrogen enhanced localized plasticity (HELP) mechanism of hydrogen embrittlement, and (ii) hydrostatic stress-based hydrogen diffusion to the crack initiation sites. These critical insights thus can help to design hydrogen embrittlement resistant metals. In addition, the novel experimental approach can be used to calibrate advance micromechanical models while providing quantitative estimate of the hydrogen distribution in realistic metallic microstructure responsible for hydrogen-assisted crack initiation with deformation.
引用
收藏
页数:10
相关论文
共 50 条
  • [41] Creep crack growth by grain boundary cavitation under monotonic and cyclic loading
    Wen, Jian-Feng
    Srivastava, Ankit
    Benzerga, Amine
    Tu, Shan-Tung
    Needleman, Alan
    JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 2017, 108 : 68 - 84
  • [42] Frictional crack initiation and propagation in rocks under compressive loading
    Alneasan, Mahmoud
    Behnia, Mahmoud
    Bagherpour, Raheb
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2018, 97 : 189 - 203
  • [43] Dynamic Crack Initiation Toughness of Shale under Impact Loading
    Yang, Guoliang
    Li, Xuguang
    Bi, Jingjiu
    Cheng, Shuaijie
    ENERGIES, 2019, 12 (09)
  • [44] A stochastic analysis of glass crack initiation under thermal loading
    Wang, Qingsong
    Wang, Yu
    Zhang, Yi
    Chen, Haodong
    Sun, Jinhua
    He, Linghui
    APPLIED THERMAL ENGINEERING, 2014, 67 (1-2) : 447 - 457
  • [46] Fatigue crack initiation and propagation under cyclic contact loading
    Fajdiga, G.
    Sraml, M.
    ENGINEERING FRACTURE MECHANICS, 2009, 76 (09) : 1320 - 1335
  • [47] Crack and blister initiation and growth in purified iron due to hydrogen loading
    Tiegel, Marie C.
    Martin, May L.
    Lehmberg, Annegret K.
    Deutges, Martin
    Borchers, Christine
    Kirchheim, Reiner
    ACTA MATERIALIA, 2016, 115 : 24 - 34
  • [48] Crack resistance of austenitic stainless steel pipe and pipe welds with a circumferential crack under monotonic loading
    Singh, P. K.
    Vaze, K. K.
    Ghosh, A. K.
    Kushwaha, H. S.
    Pukazhendi, D. M.
    Murthy, D. S. R.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2006, 29 (11) : 901 - 915
  • [49] Experimental investigations of fracture toughness and crack initiation in marble under different freezing and thermal cyclic loading
    Dehghani, Bijan
    Faramarzi, Lohrasb
    CONSTRUCTION AND BUILDING MATERIALS, 2019, 220 : 340 - 352
  • [50] Towards the prediction of intergranular fatigue crack initiation in metals due to hydrogen
    Arora, Aman
    Singh, Harpreet
    Mahajan, Dhiraj K.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 787