Behaviour of hydrogen impurity in aluminium alloys during anodizing

被引:14
|
作者
Iglesias-Rubianes, L
Skeldon, P
Thompson, GE
Kreissig, U
Grambole, D
Habazaki, H
Shimizu, K
机构
[1] UMIST, Corros & Protect Ctr, Manchester M60 1QD, Lancs, England
[2] Forschungszentrum Rossendorf EV, Inst Ion Beam Phys & Mat Res, D-01314 Dresden, Germany
[3] Hokkaido Univ, Grad Sch Engn, Kita Ku, Sapporo, Hokkaido 0608628, Japan
[4] Keio Univ, Chem Lab, Yokohama, Kanagawa 223, Japan
关键词
anodic oxidation; aluminium; hydrogen; nuclear reaction analysis;
D O I
10.1016/S0040-6090(02)01100-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present study examines the behaviour of hydrogen impurity in an Al-6.5 at.% W alloy during anodizing, using elastic recoil detection and nuclear reaction analyses. Increased concentrations of hydrogen are found near the alloy/anodic film interface, amounting to similar to 2 X 10(15) H atoms cm(-2) for the particular alloy, containing 0.1-0.3 at.% hydrogen in the bulk regions, and conditions of anodizing. The enrichment arises from hydrogen in the alloy (i) diffusing to the interface, which acts as a trap, or (ii) accumulating at the interface, due to the growth of the anodic film, or a combination of both processes. Diffusion is consistent with the known mobility of hydrogen in aluminium near ambient temperature. Further, accumulation, and subsequent oxidation, of hydrogen are expected based on the general behaviour of alloying elements in anodized aluminium. The anodic films contained similar to0.1-0.3 at.% hydrogen, originating from either the electrolyte or the alloy. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:201 / 207
页数:7
相关论文
共 50 条
  • [31] HYDROGEN EMBRITTLEMENT RESISTANCE OF AUSTENITIC ALLOYS AND ALUMINIUM ALLOYS
    Li Yiyi
    Fan Cungan
    Rong Lijian
    Yan Desheng
    Li Xiuyan
    ACTA METALLURGICA SINICA, 2010, 46 (11) : 1335 - 1346
  • [32] Spark anodizing behaviour of titanium and its alloys in alkaline aluminate electrolyte
    Nakajima, M.
    Miura, Y.
    Fushimi, K.
    Habazaki, H.
    CORROSION SCIENCE, 2009, 51 (07) : 1534 - 1539
  • [33] ANODIZING OF ALUMINIUM IN SULPHATE SOLUTIONS
    WOOD, GC
    OSULLIVA.JP
    ELECTROCHIMICA ACTA, 1970, 15 (12) : 1865 - &
  • [34] Anodizing of aluminium in Borax solution
    Pokes, A.
    Thompson, G.E.
    Skeldon, P.
    Morgan, P.C.
    Shimizu, K.
    Transactions of the Institute of Metal Finishing, 1999, 77 (pt 5): : 171 - 177
  • [35] Measuring the nucleation of hydrogen porosity during the solidification of aluminium-copper alloys
    Lee, PD
    Hunt, JD
    SCRIPTA MATERIALIA, 1997, 36 (04) : 399 - 404
  • [36] Anodizing of aluminium in borax solution
    Pakes, A
    Thompson, GE
    Skeldon, F
    Morgan, PC
    Shimizu, K
    TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 1999, 77 : 171 - 177
  • [37] Mechanical behaviour of aluminium-lithium alloys
    N. Eswara Prasad
    A. A. Gokhale
    P. Rama Rao
    Sadhana, 2003, 28 : 209 - 246
  • [38] Corrosion behaviour of aluminium alloys in ethanol fuels
    L. Krüger
    F. Tuchscheerer
    M. Mandel
    S. Müller
    S. Liebsch
    Journal of Materials Science, 2012, 47 : 2798 - 2806
  • [39] Characterisation and modelling of the plastic behaviour of aluminium alloys
    Lukac, P
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 1996, 217 : 71 - 81
  • [40] Corrosion behaviour of aluminium alloys in ethanol fuels
    Krueger, L.
    Tuchscheerer, F.
    Mandel, M.
    Mueller, S.
    Liebsch, S.
    JOURNAL OF MATERIALS SCIENCE, 2012, 47 (06) : 2798 - 2806