摘要
In situ Ti-6Al-4V/TiB discontinuously reinforced composites, containing 20 and 40% of TiB whiskers by volume, were produced by blending Ti, Al/V, and TiB2 Powders. The consolidated powder blends were annealed to transform the TiB2 particles to TiB. The microstructural evolution of the composite was studied as a function of heat treatment duration at 1100, 1200, 1300 and 1400 degreesC. The mechanical properties of Ti-6Al-4V/TiB composites were established in tension and compression at room temperature and 300 degreesC, and by resonant ultrasound spectroscopy (RUS), for the two volume fractions of TiB, and for randomly oriented and aligned arrays of TiB whiskers. The average Young's modulus of the composite with 20% of randomly oriented TiB whiskers was 153 GPa, compared to 109 GPa for unreinforced Ti-6Al-4V. The average Young's modulus of composites with 20 and 40% of aligned TiB whiskers was measured along the extrusion axis as 169 and 205 GPa, respectively. The stiffness of TiB whiskers was determined from bulk measurements with the Halpin-Tsai equation to be 482 GPa. Yield and ultimate strengths near 1200 MPa were measured. The strength and ductility of the materials were limited in the present study by non-optimal matrix microstructure and inadequate particulate distribution, and approaches for properties improvements are provided. (C) 2003 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2427 / 2442
页数:16
相关论文
共 50 条
  • [21] Mechanical behaviour of flashless hot forged and heat treated TiB-reinforced Ti-6Al-4V composites
    Jia, M.
    Alshammari, Y.
    Yang, F.
    Bolzoni, L.
    MATERIALS CHEMISTRY AND PHYSICS, 2022, 290
  • [22] Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted Ti-6Al-4V and TiB/Ti-6Al-4V composite: A comparative study
    Li, Hailiang
    Jia, Dechang
    Yang, Zhihua
    Liao, Xingqi
    Jin, Haize
    Cai, Delong
    Zhou, Yu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 801
  • [23] Structure of TiB precipitates in laser deposited in situ, Ti-6Al-4V-TiB composites
    Genç, A
    Banerjee, R
    Hill, D
    Fraser, HL
    MATERIALS LETTERS, 2006, 60 (07) : 859 - 863
  • [24] Effect of TiB2 Content on Microstructure and Properties of in-situ TiB/Ti6Al4V Composites
    Huang Weidong
    Zhu Yitao
    Huang Xu
    Wang Lu
    Cheng Xuheng
    LASER & OPTOELECTRONICS PROGRESS, 2023, 60 (23)
  • [25] Effect of reinforcements on rolling contact fatigue behaviors of titanium matrix composite (TiB + TiC)/Ti-6Al-4V
    Xie, Lechun
    Zhou, Qinghua
    Jin, Xiaoqing
    Wang, Zhanjiang
    Jiang, Chuanhai
    Lu, Weijie
    Wang, Jiaxu
    Wang, Q. Jane
    INTERNATIONAL JOURNAL OF FATIGUE, 2014, 66 : 127 - 137
  • [26] Hydrogen induced softening and hardening for hot workability of (TiB + TiC)/Ti-6Al-4V composites
    Wang, Xuan
    Wang, Liang
    Luo, LiangShun
    Xu, YanJin
    Li, XinZhong
    Chen, RuiRun
    Su, YanQing
    Guo, JingJie
    Fu, HengZhi
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (05) : 3380 - 3388
  • [27] Superplasticity of fine TiB dispersed Ti-6Al-4V alloy composites obtained by reaction sintering
    Funami, K
    Kobayashi, M
    Suzuki, S
    Ouchi, C
    SUPERPLASTICITY IN ADVANCED MATERIALS - ICSAM-97, 1997, 243-2 : 515 - 520
  • [28] Nanoindentation Characterization on Microhardness of Micron-Level TiC and TiB Reinforcements in in-situ Synthesized (TiC+TiB)/Ti-6Al-4V Composite
    Wen, Yan
    Guo, Tingting
    Zhou, Yuangui
    Bai, Huiping
    Wang, Zhou
    FRONTIERS IN MATERIALS, 2019, 6
  • [29] Fabrication of TiB-TiC, TiB-TiN and TiB2-TiC composites and their bonding to Ti-6Al-4V alloy by spark and resistance sintering
    Ding, LX
    Nakasa, K
    Kato, M
    Tachiyama, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2002, 66 (06) : 597 - 605
  • [30] Nearly dense Ti-6Al-4V/TiB composites manufactured via hydrogen assisted BEPM
    Song, Yuchao
    Ma, Guangyu
    Qiu, Fucheng
    Stasiuk, Oleksandr
    Savvakin, Dmytro
    Ivasishin, Orest
    Xu, Xiaofeng
    Cheng, Tuo
    CERAMICS INTERNATIONAL, 2022, 48 (08) : 10902 - 10910