Study on the microstructure, mechanical properties, tarnish and corrosion resistance of sterling silver alloyed with manganese

被引:28
|
作者
Nisaratanaporn, E.
Wongsriruksa, S.
Pongsukitwat, S.
Lothongkum, G.
机构
[1] Chulalongkorn Univ, Dept Engn Met, Fac Engn, Bangkok 10330, Thailand
[2] Srinakharinwirot Univ, Fac Sci, Dept Mat Sci, Bangkok 10110, Thailand
关键词
sterling silver; microstructure; mechanical properties; tarnish and corrosion resistance;
D O I
10.1016/j.msea.2006.09.106
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The objective of this research was to investigate the effect of manganese in as-cast sterling silver alloys used in jewellery industry on microstructure, mechanical properties. and tarnish and corrosion resistance. In order to determine the suitable manganese content, manganese in the specimens varied from 0, 0.38, 0.76, 1.3, 1.7, 2.1, 2.6 and 3.0 wt%. The microstructure consisted of both silver-rich solid solution, as a matrix, and eutectic structure. The amount of manganese examined in the eutectic region was higher than those in the matrix. By increasing manganese content, the amount of eutectic structure decreased, and therefore, tensile and yield strengths and hardness of the alloys also decreased. It was obvious that the hardness of 3.0% Mn alloys (52.1 HV) was lower than that of manganese-free alloys (66.8 HV). The tarnish resistance improved when the amount of manganese increased. The tarnish films were studied quantitatively using a spectrophotometer. For 3-h tarnishing test time, the colour difference, DE*, of the manganese-free alloy was 24.98 and higher than that of the 3.0% Mn alloy, which was 5.19. The anodic polarization curves, from which the corrosion potentials (E-corr), the primary passive potentials (E-pp), the pitting potentials (E-p) and passive current density (I-p) were evaluated, of the test alloys were measured in 1% NaCl and H2S-saturated 1% NaCl solutions. In 1% NaCl solution, increasing of manganese content not only promoted the noble shift in corrosion potentials but also reduced the average passive current density. In H2S-saturated 1% NaCl solution, the passive region was not observed and the effect of manganese in sterling silver on corrosion potential was not clear, but the corrosion current decreased with the increase of the manganese content. The tarnish and corrosion resistance of sterling silver were improved with manganese. This may be due to the decrease of eutectic structure, of which the presence of copper content was higher than that of matrix. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:663 / 668
页数:6
相关论文
共 50 条
  • [41] Microstructure and Mechanical Properties of a Low Alloyed MnB Cast Steel
    Kaishuang Luo
    Bingzhe Bai
    Journal of Materials Engineering and Performance, 2010, 19 : 829 - 833
  • [42] Corrosion properties of lead anodes. II. Lead alloys alloyed with silver, titanium, tin, cobalt, manganese, and silicon
    Kozin, L.F.
    Kozin, V.F.
    Zashchita Metallov, 1997, 33 (06): : 609 - 615
  • [43] Microstructure, mechanical properties, and corrosion resistance of an explosively welded Mg-Al composite
    Acarer, Mustafa
    Demir, Bilge
    Dikici, Burak
    Salur, Emin
    JOURNAL OF MAGNESIUM AND ALLOYS, 2022, 10 (04) : 1086 - 1095
  • [44] EFFECT OF CHROMIUM ADDITION ON MICROSTRUCTURE AND MECHANICAL PROPERTIES AND CORROSION RESISTANCE OF TiAlN BASED COATING
    Nojit, Teerapat
    Taweesup, Kattareeya
    Visuttipitukul, Patama
    SURANAREE JOURNAL OF SCIENCE AND TECHNOLOGY, 2021, 28 (06):
  • [45] Selective laser melting dental CoCr alloy: microstructure, mechanical properties and corrosion resistance
    Chen, Jie
    Yang, Yongqiang
    Wu, Shibiao
    Zhang, Mingkang
    Mai, Shuzhen
    Song, Changhui
    Wang, Di
    RAPID PROTOTYPING JOURNAL, 2021, 27 (08) : 1457 - 1466
  • [46] Effects of Sc addition on microstructure, mechanical and corrosion resistance properties of 7055 Al alloy
    Huang, Kai
    Feng, Qin
    Zhou, Wenbiao
    Huang, Liang
    Xiang, Jing
    Luo, Nengneng
    Han, Kai
    Zhu, Yutao
    Wei, Yuezhou
    MATERIALS RESEARCH EXPRESS, 2021, 8 (04)
  • [47] Microstructure, mechanical properties, and corrosion resistance of continuous heating aging 6013 aluminum alloy
    Lei, Guopeng
    Wang, Bo
    Lu, Jing
    Wang, Chen
    Li, Yimin
    Luo, Fenghua
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 18 : 370 - 383
  • [48] Effect of aging temperature on the microstructure and properties of alloyed high-manganese steel
    Sun, J.
    Jiang, M.
    Dong, L.
    Ding, Z.
    Bao, Y.
    Luo, S.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2024, 55 (07) : 1045 - 1051
  • [49] Microstructure, Corrosion and Mechanical Properties of Magnesium Alloys
    Zengin, Hueseyin
    METALS, 2023, 13 (09)
  • [50] Effect of inoculation on microstructure, mechanical and corrosion properties of high manganese ductile Ni-resist alloy
    Rashidi, M. Mohd
    Idris, Mohd Hasbullah
    MATERIALS & DESIGN, 2013, 51 : 861 - 869