Adhesion to Y-TZP ceramic: Study of silica nanofilm coating on the surface of Y-TZP

被引:60
|
作者
Druck, Carolina Ceolin [1 ]
Pozzobon, Joao Luiz [1 ]
Callegari, Gustavo Luiz [2 ]
Dorneles, Lucio Strazzabosco [2 ]
Valandro, Luiz Felipe [1 ]
机构
[1] Univ Fed Santa Maria, Fac Odontol, BR-97119900 Santa Maria, RS, Brazil
[2] Univ Fed Santa Maria, Dept Phys, BR-97119900 Santa Maria, RS, Brazil
关键词
adhesion; zirconia; nanofilm; silica deposition; RESIN BOND STRENGTH; STABILIZED TETRAGONAL ZIRCONIA; BIAXIAL FLEXURAL STRENGTH; FIXED PARTIAL DENTURES; AIR-PARTICLE ABRASION; PHASE-TRANSFORMATION; CONDITIONING METHODS; COMPOSITE RESIN; LUTING AGENTS; SELF-ADHESIVE;
D O I
10.1002/jbm.b.33184
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
This study evaluated the influence of silica-based film coatings on the surface of yttrium-stabilized tetragonal zirconia polycrystal (Y-TZP), in particular on the durability of the bond strength between the ceramic and resin cement. Eighty Y-TZP (In-Ceram YZ, Vita) blocks (4 x 4 x 3 mm) were obtained and divided into four groups according to the surface treatments (n=20): tribochemical silica coating (TBS; Cojet, 3M/ESPE), 5 nm SiO2 nanofilm and silanization (F-5), 500 nm SiO2 nanofilm and silanization (F-500), and 500 nm SiO2 nanofilm+hydrofluoric-acid-etching+silanization (F-500HF). Specimens of composite resin (3.25 mm in diameter and 3 mm in height) were cemented to Y-TZP blocks using resin cement (Relyx ARC). Half of the specimens from each group were tested 24 h after adhesion (B: baseline condition), and the other half were subjected to aging (A: storage for 90 days and 10,000 thermal cycles). The specimens were subjected to shear testing (SBS) (1 mm/min). After testing, the surfaces were analyzed with a stereomicroscope and scanning electron microscope. Micromorphologic and elemental chemical analyses of the treated Y-TZP surface were made by X-ray energy dispersive spectroscopy. Bond strength data were statistically analyzed by Kruskal-Wallis/Mann-Whitney tests (=0.05). The surface treatment showed significant differences for B (p=0.0001) and A (p=0.0000) conditions. In both storage conditions, TBS and F-5 groups promoted the significantly highest bond strength. Most of the specimens presented adhesive failure. The X-ray energy dispersive spectroscopy analysis depicted the highest peak of silica in the TBS, F-5, and F-500 groups. The adhesion to zirconia can be improved if the surface receives a 5 nm layer of SiO2 nanofilm or is subjected to sandblasting with silica particles, followed by silanization. (c) 2014 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 103B: 143-150, 2015.
引用
收藏
页码:143 / 150
页数:8
相关论文
共 50 条
  • [41] Low-temperature degradation of a Y-TZP ceramic after surface treatments
    Amaral, Marina
    Valandro, Luiz Felipe
    Bottino, Marco A.
    Souza, Rodrigo O. A.
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2013, 101 (08) : 1387 - 1392
  • [42] Y-TZP/Ce-TZP functionally graded composite
    Zhao, C
    Vleugels, J
    Vandeperre, L
    Basu, B
    Van der Biest, O
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1998, 17 (17) : 1453 - 1455
  • [43] Effect of surface topography and wettability on shear bond strength of Y-TZP ceramic
    Suriyakul Wongsue
    Ornnicha Thanatvarakorn
    Taweesak Prasansuttiporn
    Piyarat Nimmanpipug
    Thanapat Sastraruji
    Keiichi Hosaka
    Richard M. Foxton
    Masatoshi Nakajima
    Scientific Reports, 13
  • [44] Low Temperature Degradation of Y-TZP Ceramic for Dental Applications
    Wu, Zhi-kai
    Li, Ning
    Zhao, Wan-qian
    Yan, Jia-zhen
    EIGHTH CHINA NATIONAL CONFERENCE ON FUNCTIONAL MATERIALS AND APPLICATIONS, 2014, 873 : 241 - 249
  • [45] Surface characterization of dental Y-TZP ceramic after air abrasion treatment
    Hallmann, Lubica
    Ulmer, Peter
    Reusser, Eric
    Haemmerle, Christoph H. F.
    JOURNAL OF DENTISTRY, 2012, 40 (09) : 723 - 735
  • [46] Influence of surface and heat treatments on the flexural strength of Y-TZP dental ceramic
    Guazzato, M
    Quach, L
    Albakry, M
    Swain, MV
    JOURNAL OF DENTISTRY, 2005, 33 (01) : 9 - 18
  • [47] Surface characterization of different surface treatments associations with plasma and bonding of Y-TZP and the ceramic
    Bitencourt, Sandro Basso
    dos Santos, Daniela Micheline
    Bastos-Bitencourt, Natalia Almeida
    Rangel, Elidiane Cipriano
    da Cruz, Nilson Cristino
    Bonfante, Estevam Augusto
    De Souza, Grace Mendonca
    Pesqueira, Aldieris Alves
    DENTAL MATERIALS, 2021, 37 (12) : 1873 - 1883
  • [48] Effect of surface topography and wettability on shear bond strength of Y-TZP ceramic
    Wongsue, Suriyakul
    Thanatvarakorn, Ornnicha
    Prasansuttiporn, Taweesak
    Nimmanpipug, Piyarat
    Sastraruji, Thanapat
    Hosaka, Keiichi
    Foxton, Richard M.
    Nakajima, Masatoshi
    SCIENTIFIC REPORTS, 2023, 13 (01)
  • [49] Y-TZP纳米陶瓷的制备
    孟国文,陈大明,康沫狂,杨峥,韩栋
    西北工业大学学报, 1995, (04) : 563 - 566
  • [50] Deflocculation study of aqueous nanosized Y-TZP suspensions
    Liu, YQ
    Gao, L
    MATERIALS CHEMISTRY AND PHYSICS, 2003, 78 (02) : 480 - 485