Deposition and characterization of CrN/Si3N4 and CrAIN/Si3N4 nanocomposite coatings prepared using reactive DC unbalanced magnetron sputtering

被引:43
|
作者
Barshilia, Harish C. [1 ]
Deepthi, B. [1 ]
Rajam, K. S. [1 ]
机构
[1] Surface Engn Div, Natl Aerosp Lab, Bangalore 560017, Karnataka, India
来源
SURFACE & COATINGS TECHNOLOGY | 2007年 / 201卷 / 24期
关键词
CrN-/Si3N4 and CrAlN/Si3N4 nanocomposite coatings; unbalanced magnetron sputtering; structural and mechanical properties; thermal stability;
D O I
10.1016/j.surfcoat.2007.04.002
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Nanocomposite coatings of CrN/Si3N4 and CrAlN/Si3N4 with varying silicon contents were synthesized using a reactive direct current (DC) unbalanced magnetron sputtering system. The Cr and CrAl targets were sputtered using a DC power supply and the Si target was sputtered using an asymmetric bipolar-pulsed DC power supply, in Ar+N-2, plasma. The coatings were approximately 1.5 mu m thick and were characterized using X-ray diffraction (XRD), nanoindentation, X-ray photoelectron spectroscopy and atomic force microscopy. Both the CrN/Si3N4 and CrAlN/Si3N4 nanocomposite coatings exhibited cubic B1 NaCl structure in the XRD data, at low silicon contents (< 9 at.%). A maximum hardness and elastic modulus of 29 and 305 GPa, respectively were obtained from the nanoindentation data for CrN/Si3N4 nanocomposite coatings, at a silicon content of 7.5 at.%. (cf,. 24 and 285 GPa, respectively for CrN). The hardness and elastic modulus decreased significantly with further increase in silicon content. CrAlN/Si3N4 nanocomposite coatings exhibited a hardness and elastic modulus of 32 and 305 GPa, respectively at a silicon content of 7.5 at.% (cf., 31 and 298 GPa, respectively for CrAlN). The thermal stability of the coatings was studied by heating the coatings in air for 30 min in the temperature range of 400-900 degrees C. The microstructural changes as a result of heating were studied using micro-Raman spectroscopy. The Raman data of the heat-treated coatings in air indicated that CrN/Si3N4 and CrAlN/Si3N4 nanocomposite coatings, with a silicon content of approximately 7.5 at.% were thermally stable up to 700 and 900 degrees C, respectively. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:9468 / 9475
页数:8
相关论文
共 50 条
  • [21] Deposition of Ni-Fe/Si3N4 nanocomposite prepared by electroplating
    Marita, Yusrini
    Yaacob, Iskandar Idris
    WORLD CONGRESS ON ENGINEERING 2008, VOLS I-II, 2008, : 1372 - 1374
  • [22] Densification and mechanical properties of Si3N4/SiC nanocomposite using Si-nitrided Si3N4 powder
    Yang, JF
    Choa, YH
    Sekino, T
    Niihara, K
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1999, 18 (07) : 505 - 507
  • [23] A crystalline Si3N4 amorphous Si3N4 composite
    Reimanis, IE
    Petrovic, JJ
    Suematsu, H
    Mitchell, TE
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1996, 79 (02) : 395 - 400
  • [24] Crystalline Si3N4/amorphous Si3N4 composite
    Los Alamos Natl Lab, Los Alamos, United States
    J Am Ceram Soc, 2 (395-400):
  • [25] Low temperature heat capacity measurements of β-Si3N4 and γ-Si3N4: Determination of the equilibrium phase boundary between β-Si3N4 and γ-Si3N4
    Nishiyama, Norimasa
    Kitani, Suguru
    Ohta, Yuki
    Kulik, Eleonora
    Netriova, Zuzana
    Holzheid, Astrid
    Lences, Zoltan
    Kawaji, Hitoshi
    Wakai, Fumihiro
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (16) : 6309 - 6315
  • [26] The relationship between substrate temperature and mechanical properties of CrN/Si3N4 nanolayered coatings deposited by magnetron sputtering
    Bai, Xiaoming
    Lin, Wanfeng
    Wang, Mingxiao
    Zhang, Xinying
    INTEGRATED FERROELECTRICS, 2017, 180 (01) : 61 - 68
  • [27] Structural and mechanical studies of W2N embedded Si3N4 nanocomposite hard coating prepared by reactive magnetron sputtering
    Anwar, Sharmistha
    Islam, Aminul
    Bajpai, Shubhra
    Anwar, Shahid
    SURFACE & COATINGS TECHNOLOGY, 2017, 311 : 268 - 273
  • [28] Laser surface nanostructuring for reliable Si3N4/Si3N4 and Si3N4/Invar joined components
    Salvo, Milena
    Casalegno, Valentina
    Suess, Manuela
    Gozzelino, Laura
    Wilhelmi, Christian
    CERAMICS INTERNATIONAL, 2018, 44 (16) : 20596 - 20597
  • [29] Wettability of PdNi(Co)-Cr alloys on Si3N4 ceramic and joining of Si3N4 to Si3N4
    Xiong, Hua-Ping
    Chen, Bo
    Guo, Wan-Lin
    Ye, Lei
    WELDING IN THE WORLD, 2015, 59 (01) : 33 - 44
  • [30] β-Si3N4及添加β-Si3N4的α-Si3N4的气氛加压烧结
    张宝林
    庄汉锐
    罗新宇
    李文兰
    硅酸盐通报, 1999, (02) : 37 - 41+47