The Production and Characterization of Near Stoichiometric NdFeB-Type HDDR Powder
被引:0
|
作者:
Shaaban, A.
论文数: 0引用数: 0
h-index: 0
机构:
Univ Tekn Malaysia Melaka, Fac Mfg Engn, Ayer Keroh 75450, Melaka, MalaysiaUniv Tekn Malaysia Melaka, Fac Mfg Engn, Ayer Keroh 75450, Melaka, Malaysia
Shaaban, A.
[1
]
机构:
[1] Univ Tekn Malaysia Melaka, Fac Mfg Engn, Ayer Keroh 75450, Melaka, Malaysia
A study of the processing of HDDR powder with the composition Nd(12.7)Fe(81.3)B(60) and Ne(12.2)Fe(81.2)B(5.9)Zr(0.1) have been undertaken. The homogenized alloys were disproportionated at 850 degrees C for 30 minutes and employing a range of recombination temperatures from 790 degrees C to 920 degrees C. The optimum recombination temperature in the HDDR treatment was found to be 880 degrees C. Zr-addition appears to inhibit grain growth during the treatment process.
机构:
Natl Inst Adv Ind Sci & Technol, Magnet Powder Met Res Ctr, Nagoya, Aichi 4638560, JapanNatl Inst Adv Ind Sci & Technol, Magnet Powder Met Res Ctr, Nagoya, Aichi 4638560, Japan
Takagi, Kenta
Jinno, Miho
论文数: 0引用数: 0
h-index: 0
机构:
Natl Inst Adv Ind Sci & Technol, Magnet Powder Met Res Ctr, Nagoya, Aichi 4638560, JapanNatl Inst Adv Ind Sci & Technol, Magnet Powder Met Res Ctr, Nagoya, Aichi 4638560, Japan