共 50 条
- [41] Hot corrosion resistance of NiCr based Cermet coatings for the protection of boiler heat exchanger tubes CONTRIBUTIONS OF SURFACE ENGINEERING TO MODERN MANUFACTURING AND REMANUFACTURING, 2002, : 188 - 192
- [42] Porosity and Wear Resistance of Flame Sprayed Tungsten Carbide Coatings GREEN PROCESS, MATERIAL, AND ENERGY: A SUSTAINABLE SOLUTION FOR CLIMATE CHANGE, 2017, 1855
- [45] Corrosion resistance improvement of mechanical seals with tungsten carbide coating 15TH INTERNATIONAL CONFERENCE ON FLUID SEALING: MEETING USERS' NEEDS, 1997, (26): : 271 - 283
- [48] Effects of process parameters on the deposition rate, hardness, and corrosion resistance of tungsten carbide coatings deposited by reactive sputtering Japanese Journal of Applied Physics, Part 1: Regular Papers and Short Notes and Review Papers, 2005, 44 (5 A): : 3196 - 3199
- [49] Effects of process parameters on the deposition rate, hardness, and corrosion resistance of tungsten carbide coatings deposited by reactive sputtering JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2005, 44 (5A): : 3196 - 3199