Antireflective coatings with high damage threshold prepared by laser ablation

被引:5
|
作者
Filipescu, M. [1 ]
Palla-Papavlu, A. [1 ]
Bercea, A. [1 ]
Rusen, L. [1 ]
Cernaianu, M. O. [2 ]
Ion, V [1 ]
Calugar, A. [1 ,3 ]
Nistor, L. C. [4 ]
Dinescu, M. [1 ]
机构
[1] Natl Inst Lasers Plasma & Radiat Phys, 409 Atomistilor St, Magurele 077125, Romania
[2] Horia Hulubei Natl Inst Phys & Nucl Engn, Extreme Light Infrastruct Nucl Phys ELI NP, 30 Reactorului St, Bucharest 077125, Romania
[3] Univ Bucharest, Fac Phys, 405 Atomistilor,POB MG 11, Magurele 077125, Romania
[4] Natl Inst Mat Phys, Magurele 077125, Ilfov, Romania
来源
关键词
OXIDES; FILMS; PLD;
D O I
10.1007/s00339-019-3110-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Latest developments in the field of high power ultra-short pulse lasers have led to intensive studies dedicated to the fabrication possibility of new antireflective coatings which exhibit high damage threshold. Therefore, this study is focused on the deposition and characterization of metal oxide heterostructures followed by laser-induced damage threshold tests which evidence their application in high power laser optics. Al2O3, SiO2, and HfO2 layers are combined to obtain different heterostructures, i.e. HfO2/Al2O3/HfO2/Al2O3/HfO2 and HfO2/SiO2/HfO2/SiO2/HfO2. The metal oxide heterostructures are deposited in a controllable oxygen atmosphere, either at room temperature or high temperatures (600 degrees C) by pulsed laser deposition (PLD). The morphological, structural and optical properties of the as-deposited heterostructures are first investigated. Atomic force microscopy and spectroscopic ellipsometry investigations reveal a lower roughness of the heterostructures based on HfO2/Al2O3 layers grown at 600 degrees C as compared to those grown at room temperature. Furthermore, following the laser-induced damage threshold (LIDT) tests carried out with a Ti-Sapphire laser, higher LIDT values are obtained for the HfO2/Al2O3-based heterostructures than for the HfO2/SiO2-based heterostructures. The ability to control the morphological and structural properties of the antireflective coatings by modifying the deposition parameters of the metal oxide heterostructures demonstrates that PLD is a suitable technique for the manufacturing of antireflective coatings for high power ultra-short laser systems.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Antireflective coatings for high impedance jumps
    Mateus, J. D.
    Posada, H. Vinck
    Baena, J. D.
    2019 THIRTEENTH INTERNATIONAL CONGRESS ON ARTIFICIAL MATERIALS FOR NOVEL WAVE PHENOMENA (METAMATERIALS)), 2019, : 56 - 58
  • [32] Dielectric nanostructures with high laser damage threshold
    Ngo, C. Y.
    Hong, L. Y.
    Deng, J.
    Khoo, E. H.
    Liu, Z.
    Wu, R. F.
    Teng, J. H.
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2017, 123 (02):
  • [33] Dielectric nanostructures with high laser damage threshold
    C. Y. Ngo
    L. Y. Hong
    J. Deng
    E. H. Khoo
    Z. Liu
    R. F. Wu
    J. H. Teng
    Applied Physics A, 2017, 123
  • [34] Multiscale analysis of the laser-induced damage threshold in optical coatings
    Capoulade, Jeremie
    Gallais, Laurent
    Natoli, Jean-Yves
    Commandre, Mireille
    APPLIED OPTICS, 2008, 47 (29) : 5272 - 5280
  • [35] KDP crystal antireflective coatings prepared by spin coating method
    Research Center of Laser Fusion, CAEP, P. O. Box 919-986, Mianyang 621900, China
    Qiangjiguang Yu Lizishu, 2013, 12 (3348-3352):
  • [36] Generation of defects with diamond and silica particles inside High Reflection Coatings: influence on the laser damage threshold
    Poulingue, M
    Dijon, J
    Rafin, B
    Leplan, H
    Ignat, M
    ADVANCES IN OPTICAL INTERFERENCE COATINGS, 1999, 3738 : 325 - 336
  • [37] Influence of electric field distribution on laser induced damage threshold and morphology of high reflectance optical coatings
    Abroinavicius, G.
    Buzelis, R.
    Drazdys, R.
    Melninkaitis, A.
    Sirutkaitis, V.
    LASER-INDUCED DAMAGE IN OPTICAL MATERIALS: 2007, 2008, 6720
  • [38] Silicon nanowires prepared by laser ablation at high temperature
    Zhang, YF
    Tang, YH
    Wang, N
    Yu, DP
    Lee, CS
    Bello, I
    Lee, ST
    APPLIED PHYSICS LETTERS, 1998, 72 (15) : 1835 - 1837
  • [39] Link between mechanical strength and laser damage threshold for antireflective coating made by sol-gel
    Avice, J.
    Piombini, H.
    Boscher, C.
    Belleville, P.
    Vaudel, G.
    Brotons, G.
    Ruello, P.
    Gusev, V.
    LASER-INDUCED DAMAGE IN OPTICAL MATERIALS 2017, 2017, 10447
  • [40] A design with high spectral efficiency and high laser induced damage threshold for 1064nm partially reflective coatings
    Liu, Houkun
    Jiao, Hongfei
    Zhang, Jinlong
    Cheng, Xinbin
    Wang, Zhanshan
    INTERNATIONAL CONFERENCE ON OPTOELECTRONIC AND MICROELECTRONIC TECHNOLOGY AND APPLICATION, 2020, 11617