LaNiO3 nanocube embedded in mesoporous silica for dry reforming of methane with enhanced coking resistance

被引:50
|
作者
Zhang, Li [1 ]
Lian, Jie [1 ]
Li, Le [1 ]
Peng, Cheng [1 ]
Liu, Wenming [1 ]
Xu, Xianglan [1 ]
Fang, Xiuzhong [1 ]
Wang, Zheng [2 ]
Wang, Xiang [1 ]
Peng, Hongen [1 ]
机构
[1] Nanchang Univ, Inst Appl Chem, Coll Chem, 999 Xuefu Rd, Nanchang 330031, Jiangxi, Peoples R China
[2] Ningxia Univ, State Key Lab High Efficiency Utilizat Coal & Gre, Yinchuan 750021, Peoples R China
基金
国家重点研发计划; 中国国家自然科学基金;
关键词
Perovskite; LaNiO3; nanocube; Perpendicular mesoporous silica shell; Core-shell structure; Dry reforming of methane; Coke resistance; NI CATALYSTS; SINTERING-RESISTANCE; SHELL-NANOPARTICLES; MICROPOROUS SILICA; SYNTHESIS GAS; CO2; CH4; PERFORMANCE; STABILITY; DESIGN;
D O I
10.1016/j.micromeso.2018.02.021
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
Methane dry reforming (DRM) is a fascinating reaction which can effectively utilize two abundant and greenhouse gases (CO2 and CH4) to prepare syngas (CO and H-2). The design and synthesis of high coking resistance Ni based catalysts are still a challenge. Herein, a perfect perovskite LaNiO3 nano-cube was encapsulated in perpendicular mesoporous silica shell to form a novel core-shell structured catalyst (LaNiO3-cube@meso-SiO2) for DRM reaction. The morphology of LaNiO3-cube@meso-SiO2 retained well even after reduced at high temperature, and the effect of shell thickness on its catalytic performance was also studied in detail. Its found that the mesoporous silica shell has positively effects to improve the coking resistance of Ni/La2O3 (derived from LaNiO3 nano-cube after reduction). When the shell thickness increased, the formation of coking deposition is decreased. The reasons for this novel core-shell structured catalyst with superior DRM performance should be attributed to the dual confinement effects. One is the strong metal-support interaction (SMSI) between Ni and La2O3 and silica, and the other is derived from the perpendicular mesoporous silica shell. The dual confinement strategy developed in this work can be used to design other high coking resistance catalysts for DRM reaction or other high temperature thermal catalysts.
引用
收藏
页码:189 / 197
页数:9
相关论文
共 50 条
  • [31] Ni and Ni3C catalysts supported on mesoporous silica for dry reforming of methane
    Roblero, J. G.
    Pola-Albores, F.
    Valenzuela, M. A.
    Rojas-Garcia, E.
    Rios-Valdouinos, E.
    Valverde-Aguilar, G.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (21) : 10473 - 10483
  • [32] The effect of the sandblasting method on the performance of LaNiO3/γ-Al2O3 adhesion in a microchannel reactor for dry reforming of methane process
    Ghazi, Atefeh
    Moradi, Gholamreza
    Montazeri, Vahab
    BRAZILIAN JOURNAL OF CHEMICAL ENGINEERING, 2024,
  • [33] Nanocast LaNiO3 Perovskites as Precursors for the Preparation of Coke-Resistant Dry Reforming Catalysts
    Nair, Mahesh Muraleedharan
    Kaliaguine, Serge
    Kleitz, Freddy
    ACS CATALYSIS, 2014, 4 (11): : 3837 - 3846
  • [34] Silica-based micro- and mesoporous catalysts for dry reforming of methane
    Li, Ziwei
    Das, Sonali
    Hongmanorom, Plaifa
    Dewangan, Nikita
    Wai, Ming Hui
    Kawi, Sibudjing
    CATALYSIS SCIENCE & TECHNOLOGY, 2018, 8 (11) : 2763 - 2778
  • [35] Severe Deactivation of a LaNiO3 Perovskite-Type Catalyst Precursor with H2S during Methane Dry Reforming
    Gallego, Jaime
    Batiot-Dupeyrat, Catherine
    Barrault, Joel
    Mondragon, Fanor
    ENERGY & FUELS, 2009, 23 (10) : 4883 - 4886
  • [36] Enhanced coking resistance of alumina-supported cobalt nitride catalyst via doping of phosphorus for dry reforming of methane
    Ai, Bolun
    Wu, Hongda
    Rong, Qingshan
    Shi, Yan
    Yao, Zhiwei
    PHOSPHORUS SULFUR AND SILICON AND THE RELATED ELEMENTS, 2024, 199 (7-9) : 654 - 660
  • [37] Effect of the Calcination Temperature of LaNiO3 on the Structural Properties and Reaction Performance of Catalysts in the Steam Reforming of Methane
    Wang, Yujie
    Qian, Shuairen
    Chen, Yuxin
    Yan, Binhang
    Cheng, Yi
    CATALYSTS, 2023, 13 (02)
  • [38] CO2 reforming of methane over supported LaNiO3 perovskite-type oxides
    Rabelo-Neto, R. C.
    Sales, H. B. E.
    Inocencio, C. V. M.
    Varga, E.
    Oszko, A.
    Erdohelyi, A.
    Noronha, F. B.
    Mattos, L. V.
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2018, 221 : 349 - 361
  • [39] Modifying perovskite-type oxide catalyst LaNiO3 with Ce for carbon dioxide reforming of methane
    Su, Yun-Jie
    Pan, Kuan-Lun
    Chang, Moo-Been
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2014, 39 (10) : 4917 - 4925
  • [40] Synthesis and Application of LaNiO3 Perovskite-type Nanocatalyst with Zr for Carbon Dioxide Reforming of Methane
    Talaie, Nooshin
    Sadr, Moayed Hossaini
    Aghabozorg, Hamidreza
    Zare, Karim
    ORIENTAL JOURNAL OF CHEMISTRY, 2016, 32 (05) : 2723 - 2730