Correlation between microstructural characteristics and cavitation resistance of Stellite-6 coatings on 17-4 PH stainless steel prepared with supersonic laser deposition and laser cladding

被引:33
|
作者
Zhang, Qunli [1 ,2 ,3 ]
Wu, Lijuan [1 ,2 ,3 ]
Zou, Hongsen [4 ]
Li, Bo [1 ,2 ,3 ]
Zhang, Gang [1 ,2 ,3 ]
Sun, Jingyong [1 ,2 ,3 ]
Wang, Jianjun [1 ,2 ,3 ]
Yao, Jianhua [1 ,2 ,3 ]
机构
[1] Zhejiang Univ Technol, Inst Laser Adv Mfg, Hangzhou 310023, Peoples R China
[2] Zhejiang Univ Technol, Coll Mech Engn, Hangzhou 310023, Peoples R China
[3] Zhejiang Univ Technol, Collaborat Innovat Ctr High End Laser Mfg Equipme, Natl 2011 Plan, Hangzhou 310023, Peoples R China
[4] State Grid Ningxia Maintenance Co, Yinchuan 750011, Ningxia, Peoples R China
基金
国家重点研发计划; 中国国家自然科学基金; 中国博士后科学基金;
关键词
Cavitation erosion; Stellite-6; coatings; Supersonic laser deposition; Microstructure; Failure mechanism;
D O I
10.1016/j.jallcom.2020.158417
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Stellite-6 coatings were deposited on 17-4 PH stainless steel substrate by supersonic laser deposition (SLD) and laser cladding (LC) to improve cavitation resistance of the substrate. The microstructural characteristics of the as-deposited coatings were analyzed on the basis of OM, SEM, EBSD, XRD, Vicker's hardness and nano-indentation results. The cavitation erosion performances in 3.5 wt% NaCl solution were comparatively investigated by a vibratory apparatus for the coatings prepared by SLD and LC technologies. The underlying mechanisms for differences of cavitation behavior between these two samples were elucidated in terms of grain size, dilution level, phase composition, hardness, elastic modulus and topographical features of the worn surfaces. Results show that SLD coating has finer grain, lower dilution and higher ratio of hardness to modulus. By analyzing the eroded surfaces, it is found that the pores formed due to mechanical bonding between particles in SLD coating are the priority position of cavitation where bubbles nucleate, grow and collapse. Repeated impact force from bubble collapse produces cracks and makes cracks propagation, leading to particle detachment and finally material removal. Although the porosity of SLD coating is higher than that of LC coating, its content is only less than 0.4%. Therefore, the negative effect of porosity is weaker than the positive effect of grain refinement, low dilution ratio and high hardness on cavitation performance. Consequently, SLD coating has better cavitation resistance than LC coating. (C) 2020 Elsevier B.V. All rights reserved.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Microstructure, microhardness and corrosion resistance of Stellite-6 coatings reinforced with WC particles using laser cladding
    Bartkowski, Dariusz
    Mlynarczak, Andrzej
    Piasecki, Adam
    Dudziak, Bartlomiej
    Goscianski, Marek
    Bartkowska, Aneta
    OPTICS AND LASER TECHNOLOGY, 2015, 68 : 191 - 201
  • [22] 17-4 PH stainless-steel as a material for high resolution laser metal deposition
    Steponavicute, Ada
    Selskiene, Ausra
    Stravinskas, Karolis
    Borodinas, Sergejus
    Mordas, Genrik
    MATERIALS TODAY-PROCEEDINGS, 2022, 52 : 2268 - 2272
  • [23] Microstructure and wear behaviors of 17-4 PH stainless steel fabricated by laser cladding with post laser shock peening treatment
    Li, Nan
    Wang, Qiang
    Niu, Wenjuan
    Han, Peng
    Guo, Nan
    Li, Shenao
    WEAR, 2024, 538
  • [24] Solid-state fabrication of WCp-reinforced Stellite-6 composite coatings with supersonic laser deposition
    Li, Bo
    Jin, Yan
    Yao, Jianhua
    Li, Zhihong
    Zhang, Qunli
    SURFACE & COATINGS TECHNOLOGY, 2017, 321 : 386 - 396
  • [25] Microstructure and wear resistance of Stellite-6/WC MMC coatings produced by laser cladding using Yb:YAG disk laser
    Bartkowski, Dariusz
    Kinal, Grzegorz
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2016, 58 : 157 - 164
  • [26] Influence of laser power on microstructure of laser metal deposited 17-4 ph stainless steel
    Adeyemi, A. A.
    Akinlabi, E. T.
    Mahamood, R. M.
    Sanusi, K. O.
    Pityana, S.
    Tlotleng, M.
    INTERNATIONAL CONFERENCE ON MATERIALS, ALLOYS AND EXPERIMENTAL MECHANICS (ICMAEM-2017), 2017, 225
  • [27] Embrittlement of laser surface-annealed 17-4 PH stainless steel
    Tsay, LW
    Yang, TY
    Young, MC
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 311 (1-2): : 64 - 73
  • [28] STUDY ON 17-4 PH STAINLESS STEEL PRODUCED BY SELECTIVE LASER MELTING
    Auguste, Pierre
    Mauduit, Arnold
    Fouquet, Lionel
    Pillot, Sebastien
    UNIVERSITY POLITEHNICA OF BUCHAREST SCIENTIFIC BULLETIN SERIES B-CHEMISTRY AND MATERIALS SCIENCE, 2018, 80 (04): : 197 - 210
  • [29] Electrochemical stability of laser shock peened 17-4 PH stainless steel
    Karthik, D.
    Swaroop, S.
    OPTICS AND LASER TECHNOLOGY, 2019, 120
  • [30] Additive manufacturing of functionally graded stellite6/17-4 PH fabricated via direct laser deposition
    Ilanlou, Morteza
    Razavi, Reza Shoja
    Pirali, Pouya
    Borhani, Mohammadreza
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 32 : 985 - 999