摘要
A hot dip aluminizing process to simulate the continuous galvanizing line (CGL) was carried out in three successive steps by a hot dip simulator: the pre-treatment for removing scales on the 200 x 250 mm(2) and 1mm in thickness cold rolled steel sheet, the dipping in 660 degrees C Al-Si melt for 3s and the cooling. In a pre-treatment, the steel specimen was partly coated by Au to confirm the mechanism of intermetallic compound (IMC) formation. Scanning electron microscopy (SEM), energy dispersive X-ray spectroscopy (EDX), and transmission electron microscopy (TEM) analyses were followed to observe the cross-section and the distribution of the elements. The specimen was analyzed in the boundary of the dipped-undipped part to see the formation mechanism of the aluminized steel. An intermetallic compound (IMC) is rapidly developed and grown in the steel-liquid interface. It has been usually reported that the IMC was formed by the dissolution of iron in the steel substrate toward the melt and the diffusion of aluminum in an opposite direction. The specimen is covered with aluminum-10 wt.% silicon, forms the IMC in the part that was not Au coated. However, IMC is not formed in the Au-coated part. The interface of the dipped-undipped is also analyzed by EDX. At the interface of the steel-IMC, it is clearly shown that the IMC is only formed in the dipped part and exists in the steel substrate as well, and contributes by iron, aluminum and silicon. The result clearly shows that only aluminum diffuses into the steel substrate without the dissolution of iron and forms the IMC between the steel substrate and the melt. Au coating and the short dipping time prevent the iron from dissolving into the aluminum melt. By TEM combined with focused ion beam (FIB) sample preparation, the IMC is confirmed as Fe2SiAl8, a hexagonal structure with space group P6(3)/mmc.
引用
收藏
页码:1871 / 1875
页数:5
相关论文
共 50 条
  • [41] Atmospheric corrosion resistance of hot-dip aluminized SUH409L steel sheet
    Yoshizaki, F
    Hattori, Y
    Miyoshi, Y
    Andoh, A
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2003, 89 (01): : 180 - 187
  • [42] Hot-dip aluminized steel sheet. A material for automobile components subjected to high stresses
    Warnecke, W.
    Heidtmann, U.
    Neba, G.
    Stahl und Eisen, 1990, (Spec Is):
  • [43] Dry Sliding Wear Behavior and Mechanism of a Hot-Dip Aluminized Steel as a Function of Sliding Velocity
    Yubiao Yang
    Benguo Zhang
    Wei Jiang
    Shuqi Wang
    Journal of Materials Engineering and Performance, 2019, 28 : 1685 - 1697
  • [44] Research on Corrosion Inhibitors for Coatings on Hot-Dip Aluminized-Galvanized Steel in Marine Environment
    Xu, Zhenkai
    Chen, Lian
    Han, Jingliang
    Zhu, Chengfei
    RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY A, 2023, 97 (09) : 2044 - 2051
  • [45] Heat Treatment Effect on Corrosion Resistance of Mg Coating Film on Hot-Dip Aluminized Steel
    Kim, Soon-Ho
    Lee, Seung-Hyo
    Lee, Myeong-Hoon
    SCIENCE OF ADVANCED MATERIALS, 2022, 14 (07) : 1220 - 1230
  • [46] Crystallographic features of Al4C3 phase in hot-dip aluminized steel
    School of Materials Science and Engineering, Henan University of Science and Technology, Luoyang 471003, China
    不详
    不详
    Cailiao Rechuli Xuebao, 2006, 2 (75-78):
  • [47] Fine structures in Fe3Al alloy layer of a new hot dip aluminized steel
    Yajiang L.
    Juan W.
    Yonglan Z.
    Holly X.
    Bulletin of Materials Science, 2002, 25 (7) : 635 - 639
  • [48] Fine structures in Fe3Al alloy layer of a new hot dip aluminized steel
    Li, YJ
    Wang, J
    Zhang, YL
    Holly, X
    BULLETIN OF MATERIALS SCIENCE, 2002, 25 (07) : 635 - 639
  • [49] Microstructural investigations on the hot-dip aluminized AISI 321 stainless steel after diffusion treatment
    Huilgol, Prashant
    Udupa, K. Rajendra
    Bhat, K. Udaya
    SURFACE & COATINGS TECHNOLOGY, 2019, 375 : 544 - 553
  • [50] Research on Corrosion Inhibitors for Coatings on Hot-Dip Aluminized-Galvanized Steel in Marine Environment
    Zhenkai Xu
    Lian Chen
    Jingliang Han
    Chengfei Zhu
    Russian Journal of Physical Chemistry A, 2023, 97 (9) : 2044 - 2051