Fracture behaviour of WC-Co hardmetals with WC partially substituted by titanium carbide

被引:10
|
作者
Szutkowska, M. [1 ]
Boniecki, M. [2 ]
Cygan, S. [1 ]
Kalinka, A. [1 ]
Grilli, M. L. [3 ]
Balos, S. [4 ]
机构
[1] Inst Adv Mfg Technol, Krakow, Poland
[2] Inst Elect Mat Technol, Warsaw, Poland
[3] ENEA Energy Technol Dept, Rome, Italy
[4] Fac Tech Sci, Novi Sad, Serbia
关键词
Hardmetals; sintering HIP; fracture toughness; Palmqvist cracks; titanium carbide;
D O I
10.1088/1757-899X/329/1/012015
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The addition of various amounts of TiC0.9 phase in the range from 5wt.% to 20wt.% substituting WC phase was applied in WC-Co hardmetals with 9.5 wt.% bonding cobalt phase. The hardmetals were consolidated using Hot Isostatic Pressing (HIP) method at temperature of 1573K and pressure of 1500 atm. The plain strain fracture toughness has been determined from 3PB test on a pre-cracking single edge notched beam (SENB) specimen. The indentation fracture toughness with Vickers cracks for comparison was also measured, which changed from 12 to 9.0 MPa.m(1/2). The amount of the TiC0.9 phase affected the mechanical and physical properties: Vickers hardness from 12.5 to 14.0 GPa, Young's modulus from 550 to 460 GPa, density from 13.1 to 9.6 g/cm(3), friction coefficient from 0.24 to 0.45, fracture toughness from 16.8 to 11.0 MPa.m(1/2). Scanning electron microscopy (SEM), X-ray and electron diffraction phase analysis were used to examine the WC-Co hardmetal with addition of the TiC0.9 phase. For comparison, physical and mechanical properties of the WC-Co hardmetals before modification were tested.
引用
收藏
页数:10
相关论文
共 50 条
  • [41] In situ study of fracture behavior of ultrafine WC-Co cemented carbide
    Liu, Xingwei
    Wang, Haibin
    Wang, Lihua
    Hou, Chao
    Song, Xiaoyan
    Liu, Xuemei
    Han, Xiaodong
    MATERIALS RESEARCH LETTERS, 2017, 5 (01): : 55 - 60
  • [42] Fracture and fatigue behavior of a γ-phase containing WC-Co cemented carbide
    Serra, M.
    Garcia-Marro, F.
    Cinca, N.
    Tarres, E.
    Jimenez-Pique, E.
    Llanes, L.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (11)
  • [43] Wear behaviour of graphene platelets reinforced WC-Co cemented carbide
    Li, Meng
    Cheng, Zanlin
    Dusza, Jan
    Song, Zhuolin
    Xiao, Fangkun
    Gong, Manfeng
    Sun, Shangyue
    Zhang, Chengyu
    ADVANCES IN APPLIED CERAMICS, 2022, 121 (04) : 143 - 149
  • [44] Preparation and sintering of WC-Co composite powders for coarse grained WC-8Co hardmetals
    Su, Wei
    Sun, Yexi
    Wang, Huifeng
    Zhang, Xianqi
    Ruan, Jianming
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2014, 45 : 80 - 85
  • [45] Effect of Heat Treatment on Structure and Properties of WC-Co Hardmetals
    Yang Jinhui Lai Hoyi (Institute of Mining and Mineral Engineering)(Department of Materials Science and Engineering
    北京科技大学学报, 1991, (S2) : 29 - 34
  • [46] FRACTURE TOUGHNESS AND FRACTURE OF WC-CO COMPOSITES
    CHERMANT, JL
    OSTERSTOCK, F
    JOURNAL OF MATERIALS SCIENCE, 1976, 11 (10) : 1939 - 1951
  • [47] Surface finishing: Impact on tribological characteristics of WC-Co hardmetals
    Bonny, K.
    De Baets, P.
    Quintelier, J.
    Vleugels, J.
    Jiang, D.
    Van der Biest, O.
    Lauwers, B.
    Liu, W.
    TRIBOLOGY INTERNATIONAL, 2010, 43 (1-2) : 40 - 54
  • [48] CORROSION, EROSION CORROSION, AND THE FLEXURAL STRENGTH OF WC-CO HARDMETALS
    TOMLINSON, WJ
    MOLYNEUX, ID
    JOURNAL OF MATERIALS SCIENCE, 1991, 26 (06) : 1605 - 1608
  • [49] On the abrasion of ultrafine WC-Co hardmetals by small SiC abrasive
    Krakhmalev, P. V.
    TRIBOLOGY LETTERS, 2008, 30 (01) : 35 - 39
  • [50] Influence of microstructure on the abrasive edge wear of WC-Co hardmetals
    Krakhmalev, P. V.
    Rodil, T. Adeva
    Bergstrom, J.
    WEAR, 2007, 263 : 240 - 245