Effect of thermal residual stress on matrix cracking strain and fracture behavior of the sintered SiC fiber reinforced SiO2-mullite composites

被引:2
|
作者
Nagahisa, K [1 ]
Iwamoto, K
Shinozaki, K
Sasaki, G
Enoki, M
Yoshida, M
机构
[1] Hiroshima Univ, Grad Sch Engn, Dept Mech Syst, Higashihiroshima 7398527, Japan
[2] Univ Tokyo, Sch Engn, Dept Mat Engn, Tokyo 1138656, Japan
关键词
ceramic matrix composite (CMC); thermal residual stress; matrix cracking; fracture behavior; acoustic emission (AE);
D O I
10.2320/jinstmet.68.172
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The sintered SiC fiber reinforced SiO2-mullite composites with matrix compositions, i.e., SiO2-3.7, 30, and 50 mol%Al2O3, had already been developed. In these composites, the thermal residual stress field changed with an increase in the coefficient of thermal expansion of the matrix accompanied by an increasing Al2O3 content (mullite volume fraction) in the matrices. A three-point flexural test was conducted for the composites at room temperature. The strain gauge method and AE monitoring were used to detect the matrix cracking strain during the test. The effect of the thermal residual stress on the matrix cracking strain and fracture behavior were investigated. The results are as follows. The matrix cracking strain observed in the composites with a higher tensile thermal residual stress in the matrix region parallel to the fiber axis was well predicted by the BHE theory. For the SiC fiber/SiO2-50 mol%Al2O3 composite, the first acoustic emission signal was detected just after the initial proportional limit of the stress-strain curve. For the other composites, the signals were detected below this limit. When the residual stress in the matrix region parallel to the fiber axis was compressive, the linear fracture behavior was found. On the contrary, the bi-linear fracture behavior was enhanced by the tensile residual stress in the matrix. This tendency agreed with the prediction method by Luh and Evans. The magnitude of the fracture energy obtained in each composite was qualitatively explained by the conventional theoretical formula.
引用
收藏
页码:172 / 180
页数:9
相关论文
共 50 条
  • [21] Stress-dependent matrix cracking in 2D woven SiC-fiber reinforced melt-infiltrated SiC matrix composites
    Morscher, GN
    COMPOSITES SCIENCE AND TECHNOLOGY, 2004, 64 (09) : 1311 - 1319
  • [22] EFFECT OF MATRIX CRACKING ON THE OVERALL THERMAL-CONDUCTIVITY OF FIBER-REINFORCED COMPOSITES
    LU, TJ
    HUTCHINSON, JW
    PHILOSOPHICAL TRANSACTIONS OF THE ROYAL SOCIETY A-MATHEMATICAL PHYSICAL AND ENGINEERING SCIENCES, 1995, 351 (1697): : 595 - 610
  • [23] An analytical model for the high temperature fracture strength of SiC fiber reinforced ceramic matrix composites considering oxidation and residual thermal stresses
    Jia, Tingya
    Deng, Yong
    Hao, Yi
    Gao, Xinran
    Zhang, Chao
    Cheng, Tianbao
    Li, Weiguo
    Yun, Gunjin
    COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2023, 173
  • [24] Effect of BN interfacial layer on the mechanical behavior of SiC fiber reinforced SiC ceramic matrix composites
    Chen, Mingwei
    Qiu, Haipeng
    Zhao, Yuliang
    Zhang, Bingyu
    Liu, Shanhua
    Luo, Wendong
    Ma, Xin
    Xie, Weijie
    Chen, Yi
    Zhang, Qiyue
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2024, 21 (03) : 1892 - 1904
  • [25] The thermal expansion behavior of unidirectional SiC fiber-reinforced Cu-matrix composites
    Luo, Xian
    Yang, Yanqing
    Liu, Cuixia
    Xu, Ting
    Yuan, Meini
    Huang, Bin
    SCRIPTA MATERIALIA, 2008, 58 (05) : 401 - 404
  • [26] Effect of matrix properties on thermal residual stress of fiber reinforced Ti-matrix composities
    Lou J.
    Yang Y.
    Cailiao Yanjiu Xuebao/Chinese Journal of Materials Research, 2016, 30 (07): : 503 - 508
  • [27] Modeling of thermal residual stress in environmental barrier coated fiber reinforced ceramic matrix composites
    Abdul-Aziz, Ali
    Bhatt, Ramakrishna T.
    JOURNAL OF COMPOSITE MATERIALS, 2012, 46 (10) : 1211 - 1218
  • [28] Modeling the effect of temperature on first matrix cracking stress and fracture strength of cross-ply fiber reinforced ceramic-matrix composites
    Deng, Yong
    Li, Weiguo
    Zheng, Shifeng
    Zhang, Xu
    Zhang, Xin
    Li, Ying
    Zhang, Xuyao
    Fang, Zhouyu
    Ma, Jianzuo
    Qu, Zhaoliang
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2019, 39 (16) : 5204 - 5212
  • [29] EFFECT OF MATRIX CRACKING AND INTERFACE SLIDING ON THE THERMAL-EXPANSION OF FIBER-REINFORCED COMPOSITES
    LU, TJ
    HUTCHINSON, JW
    COMPOSITES, 1995, 26 (06): : 403 - 414
  • [30] The effect of interface modification on fracture behavior of tungsten fiber reinforced copper matrix composites
    Wu, Z.
    Kang, P. C.
    Wu, G. H.
    Guo, Q.
    Chen, G. Q.
    Jiang, L. T.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 536 : 45 - 48