Microstructural characterization and layer stability of low-temperature carburized AISI 304L and AISI 904L austenitic stainless steel

被引:0
|
作者
Maistro, G. [1 ]
Nyborg, L. [1 ]
Vezzu, S. [2 ]
Cao, Y. [1 ]
机构
[1] Chalmers, S-41296 Gothenburg, Sweden
[2] Veneto Nanotech, Venice, Italy
来源
METALLURGIA ITALIANA | 2015年 / 11-12期
关键词
AUSTENITIC STAINLESS STEEL; LOW-TEMPERATURE CARBURIZING; S-PHASE; EXPANDED AUSTENITE; STABILITY; MICROSTRUCTURE; KOLSTERISING; THERMO-CHEMICAL TREATMENT; S-PHASE; PARAEQUILIBRIUM CARBURIZATION; CARBON SUPERSATURATION; MECHANICAL-PROPERTIES; FATIGUE BEHAVIOR; 316-STAINLESS-STEEL;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Carbon stabilized expanded austenite (S-phase) is prepared by commercial low-temperature carburizing process (LTC) on austenitic stainless steels AISI 304L and AISI 904L. The current paper deals with the material response to LTC and thermal stability of the formed metastable structure. The aim is to investigate the influence of the alloy composition and surface finishing as well as thermal annealing on the microstructure, phase constituents and hardness of the modified layer by means of combined analysis techniques. It has been found that the formation of expanded austenite is accompanied by Hagg carbides on as-carburized 304L. However the highly alloyed 904L exhibits mainly S-phase with larger degree of lattice expansion after carburizing. S-phase has proven to be more stable in 9041, whereas residual and/or induced ferrite/martensite in 3041 makes the formation of S-phase less favourable. LTC induces significant enhancement of surface hardness, more effectively on 904L. The hardening mechanism is discussed. In order to evaluate the phase evolution and stability of the expanded austenite at elevated temperatures, annealing has been performed in vacuum at temperature of 600 degrees C for 150 hours. The decomposition of S-phase and the related microstructure evolution give rise to reduced hardening effect and declined corrosion resistance in both S-phase layer and the region below.
引用
收藏
页码:19 / 28
页数:10
相关论文
共 50 条
  • [11] Development and Characterization of Cladding AISI 304L Stainless Steel on Aluminum
    Gabsi, Yasmine
    Zouari, Sahar
    Abdennadher, Mariem
    Dieng, Lamine
    Elleuch, Riadh
    JOURNAL OF MANUFACTURING AND MATERIALS PROCESSING, 2025, 9 (02):
  • [12] Role of Nitrogen Uptake During the Oxidation of 304L and 904L Austenitic Stainless Steels
    Yu Cao
    Mats Norell
    Oxidation of Metals, 2013, 80 : 479 - 491
  • [13] Investigation of AISI 904L austenitic stainless steel by carbonitriding process under dry sliding conditions
    Koppula, Shivani
    Jagarlamudi, Venkata Gautam
    Prudhvi, Reddi Sai
    Rajkumar, Aakula
    Prashanth, S.
    Saranya, J.
    Sateesh, N.
    Subbiah, Ram
    MATERIALS TODAY-PROCEEDINGS, 2021, 44 : 1418 - 1422
  • [14] Acoustic wave propagation in austenitic stainless steel AISI 304L: Application examples
    Dahmene, F.
    Laksimi, A.
    Hariri, S.
    Herve, C.
    Jaubert, L.
    Cherfaoui, M.
    Mouftiez, A.
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2012, 92 : 77 - 83
  • [15] Role of Nitrogen Uptake During the Oxidation of 304L and 904L Austenitic Stainless Steels
    Cao, Yu
    Norell, Mats
    OXIDATION OF METALS, 2013, 80 (5-6): : 479 - 491
  • [16] Nitrogen interstitial diffusion induced decomposition in AISI 304L austenitic stainless steel
    Martinavicius, A.
    Abrasonis, G.
    Scheinost, A. C.
    Danoix, R.
    Danoix, F.
    Stinville, J. C.
    Talut, G.
    Templier, C.
    Liedke, O.
    Gemming, S.
    Moeller, W.
    ACTA MATERIALIA, 2012, 60 (10) : 4065 - 4076
  • [17] Analysis of Fatigue Life and Crack Growth in Austenitic Stainless Steel AISI 304l
    Chelbi, Lotfi
    Hentati, Fatma
    Znaidi, Amna
    JORDAN JOURNAL OF MECHANICAL AND INDUSTRIAL ENGINEERING, 2023, 17 (04): : 501 - 508
  • [18] Low-pressure hollow cathode plasma source carburizing of AISI 304L austenitic stainless steel at low temperature
    Liu, H. Y.
    Che, H. L.
    Gao, J. Y.
    Li, G. B.
    Lei, M. K.
    SURFACE & COATINGS TECHNOLOGY, 2022, 442
  • [19] Sensitization evaluation of the austenitic stainless steel AISI 304L, 316L, 321 and 347
    A. S. Lima
    A. M. Nascimento
    H. F. G. Abreu
    P. de Lima-Neto
    Journal of Materials Science, 2005, 40 : 139 - 144
  • [20] Sensitization evaluation of the austenitic stainless steel AISI 304L, 316L, 321 and 347
    Lima, AS
    Nascimento, AM
    Abreu, HFG
    De Lima-Neto, P
    JOURNAL OF MATERIALS SCIENCE, 2005, 40 (01) : 139 - 144