Microstructure evolution and mechanical properties of γ-TiAl honeycomb structure fabricated by isothermal forging and pulse current assisted diffusion bonding

被引:17
|
作者
Shi, Chengcheng [1 ,2 ]
Lu, Zhen [2 ]
Zhang, Kaifeng [1 ,2 ]
Deng, Linwei [3 ]
Wang, Cheng [3 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Heilongjiang, Peoples R China
[2] Harbin Inst Technol, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Heilongjiang, Peoples R China
[3] Beijing Spacecrafts, Beijing 100000, Peoples R China
关键词
gamma-TiAl based alloy; Honeycomb structure; Isothermal forging; Pulse current assisted diffusion bonding; Microstructure evolution; HIGH-TEMPERATURE DEFORMATION; TITANIUM ALUMINIDE ALLOYS; HOT DEFORMATION; HIGH NB; BEHAVIOR; PHASE; MOLD;
D O I
10.1016/j.intermet.2018.05.008
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The hot deformation behavior and pulse current assisted diffusion bonding (PCDB) behavior of sintered gamma-TiAl based alloy with near gamma microstructure were investigated for fabricating honeycomb structure via isothermal forging - PCDB route. Honeycomb core structures were fabricated via isothermal forging at 1150-1250 degrees C with a nominal strain rate of 10(-3) s(-1) based on the hot deformation behavior of the sintered alloy. Additionally, the mechanical property and structural morphology demonstrated that the best forging parameter was forging at 1200 degrees C with a nominal strain rate of 10(-3) s(-1). Subsequently, the effects of bonding temperature, holding time, and bonding pressure on the microstructure evolution, plastic strain, and shear strength of the PCDB joints were investigated. The plastic strain and shear strength of the PCDB joints increased with increasing bonding temperature, time and stress, additionally, the fracture mode transformed from interfacial sliding fracture into substrate fracture with the optimization of bonding parameters. Furthermore, a sound metallurgical bonding joint with smaller plastic strain and shear strength as high as 92% of the base material was achieved at 1100 degrees C with a holding time of 20 min and a pressure of 25 MPa, showing priority compared to traditional hot pressing diffusion bonding process.
引用
收藏
页码:59 / 68
页数:10
相关论文
共 50 条
  • [41] Evolution of microstructure and mechanical properties in TiBw/Ti65 composites during vacuum solid-phase diffusion bonding
    Wang, Chunxu
    Zhou, Tongxu
    Xu, Xunhu
    Wu, Tao
    Zhang, Mangong
    Wu, Jiafeng
    Zhan, Liqiang
    Wang, Guofeng
    MATERIALS TODAY COMMUNICATIONS, 2024, 41
  • [42] Insight into microstructure evolution and mechanical properties of 5 wt% SiC/Al composites by high frequency pulse current treatment
    Xiang, Jin
    Liu, Ruifeng
    VACUUM, 2023, 215
  • [43] Effect of oxygen content in WC-FeAl powders on microstructure and mechanical properties of sintered composites fabricated by pulse current sintering technique
    Furushima, Ryoichi
    Katou, Kiyotaka
    Nakao, Setsuo
    Sun, Zheng Ming
    Shimojima, Koji
    Hosokawa, Hiroyuki
    Matsumoto, Akihiro
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2014, 61 (06): : 281 - 289
  • [44] Effect of Oxygen Content in WC-FeAl Powders on Microstructure and Mechanical Properties of Sintered Composites Fabricated by Pulse Current Sintering Technique
    Furushima, Ryoichi
    Katou, Kiyotaka
    Nakao, Setsuo
    Sun, Zheng Ming
    Shimojima, Koji
    Hosokawa, Hiroyuki
    Matsumoto, Akihiro
    MATERIALS TRANSACTIONS, 2014, 55 (12) : 1792 - 1799
  • [45] Microstructure, Texture and Mechanical Properties of Al-SiC Composite with Bimodal Structure Fabricated by Multi-Layer Accumulative Roll Bonding
    Zhang, Shengcheng
    Wei, Liqun
    Fu, Bin
    Guo, Yanhui
    COATINGS, 2023, 13 (03)
  • [46] Microstructure evolution and mechanical properties of the cladding layer of Ti-6Al-4V alloy depending on ultrasonic-assisted forging
    Gao, Guo-Fu
    Su, Ting-Ting
    Li, Zhang-Dong
    Wang, Yi
    Guo, Zi-Long
    Yuan, Zhao-Jie
    JOURNAL OF INDUSTRIAL AND PRODUCTION ENGINEERING, 2020, 37 (2-3) : 158 - 164
  • [47] Microstructure Evolution and Mechanical Properties of Nano-structured Al–0.2 wt%Zr Alloy Fabricated by Accumulative Roll Bonding (ARB) Process
    Bahram Azad
    Hamidreza Mohammadian Semnani
    Ehsan Borhani
    Transactions of the Indian Institute of Metals, 2017, 70 : 2725 - 2732
  • [48] Microstructure evolution and mechanical properties of bioinspired interpenetrating Ti2AlNb/TiAl matrix composite with a crossed-lamellar structure
    Zou, Hang
    Hu, Rui
    Zhou, Mi
    Gao, Zitong
    Liu, Xinxin
    Luo, Xian
    COMPOSITES PART B-ENGINEERING, 2024, 287
  • [49] A Study on the Microstructural Evolution, Interfacial Diffusion and Mechanical Properties of Ultra-thin Stainless Steel-Copper Composites Fabricated by Roll Bonding
    Qi, Yanyang
    Ma, Xiaoguang
    Ma, Linan
    Zhou, Cunlong
    Jiang, Zhengyi
    Zhao, Jingwei
    METALS AND MATERIALS INTERNATIONAL, 2024, 30 (10) : 2925 - 2941
  • [50] Evolution of microstructure and mechanical properties during hot forging and heat treatments of Cu-15Ni-8Sn alloy fabricated by hot isostatic pressing
    Hu, Meichen
    Zhang, Xianwei
    Liu, Chaoqiang
    Gan, Xueping
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010