Evaluating corrosion resistances of Fe-based amorphous alloys by YCr/Mo values

被引:25
|
作者
Xia Huaixiao [1 ]
Chen Qingjun [1 ]
Wang Chengjie [1 ]
机构
[1] Nanchang Hangkong Univ, Sch Mat Sci & Engn, Nanchang 330063, Jiangxi, Peoples R China
基金
中国国家自然科学基金;
关键词
the Y-Cr/Mo value; corrosion resistance; amorphous alloys; passivation current density; passive film; rare earths; BULK METALLIC GLASSES; 1 M HCL; HYDROCHLORIC-ACID; FORMING ABILITY; BEHAVIOR; CR; MOLYBDENUM; PASSIVITY; MECHANISM; CHROMIUM;
D O I
10.1016/S1002-0721(17)60926-8
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
In this paper, the synthetic effect of Cr, Mo and Y on corrosion resistance was explored, and the frim value was employed to evaluate the corrosion resistance. The composition of amorphous alloy was designed by mixing the Fe41Co7Cr15Mo14C15B6Y2 (BMG1) with good glass forming ability (GFA) and Fe50Cr22B23Ni5.4 with a high corrosion resistance at 9:1 ratio. At the same time, the contents of Y, Mo and Cr were fine-tuned. The electrochemical tests demonstrated that the passivation current density decreased with the increase of the Yam value. The passivation current density of Fe-based amorphous alloy was reduced by about half an order of magnitude. The fitting result showed that the logarithm of passivation current density (I) and the Yam value (X) were logarithmic relationship, and the fitting equation was J=-5.649+4.904x 10(15)e(-17) (52x). The X-ray photoelectron spectroscopy (XPS) results showed that the Yam value played a key role in stability of passive films. When the Yam value was low, the Cr6+ ion, Mo6+ ion were enriched in the initial stage of passivation process, then leading to the increase. passivation current density. However, when the Yam value was high, the low-valence Fe2+, Cr3+, and Mo4+ ion were enriched more easily, which result in small passivation current densities and more stable passive films.
引用
收藏
页码:406 / 411
页数:6
相关论文
共 50 条
  • [21] Mechanical crystallization of Fe-based amorphous alloys
    Sharma, Satyajeet
    Suryanarayana, C.
    JOURNAL OF APPLIED PHYSICS, 2007, 102 (08)
  • [22] CRYSTALLIZATION OF Fe-BASED BULK AMORPHOUS ALLOYS
    Bloch, K.
    Nabialek, M.
    Dospial, M.
    Garus, S.
    ARCHIVES OF METALLURGY AND MATERIALS, 2015, 60 (01) : 7 - 10
  • [23] Advances in Fe-based amorphous/nanocrystalline alloys
    Zhou, Jifeng
    You, Junhua
    Qiu, Keqiang
    JOURNAL OF APPLIED PHYSICS, 2022, 132 (04)
  • [24] ENHANCED MAGNETISM IN AMORPHOUS FE-BASED ALLOYS
    LIOU, SH
    GE, SH
    TAYLOR, JN
    CHIEN, CL
    JOURNAL OF APPLIED PHYSICS, 1987, 61 (08) : 3243 - 3245
  • [25] Irradiation properties of Fe-based amorphous alloys
    Du C.-X.
    Wang R.-S.
    Lü K.
    Si J.-J.
    Hui X.-D.
    Zhang Y.-W.
    Bai G.-H.
    Hui, Xi-Dong (hui_xidong@yahoo.com), 2017, Science Press (39): : 1372 - 1379
  • [26] Corrosion studies on Fe-based amorphous alloys in simulated PEM fuel cell environment
    Jayaraj, J
    Kim, YC
    Kim, KB
    Seok, HK
    Fleury, E
    SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS, 2005, 6 (3-4) : 282 - 289
  • [27] Effect of Si addition on the corrosion properties of amorphous Fe-based soft magnetic alloys
    Dan, Zhenhua
    Takenaka, Kana
    Zhang, Yan
    Unami, Shigeru
    Takeuchi, Akira
    Hara, Nobuyoshi
    Makino, Akihiro
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2014, 402 : 36 - 43
  • [28] Corrosion and Wear Resistance of Fe-Based Amorphous Coatings
    Li, Guang
    Gan, Youyi
    Liu, Chenheng
    Shi, Yu
    Zhao, Yanchun
    Kou, Shengzhong
    COATINGS, 2020, 10 (01)
  • [29] Crystallization and nanocrystallization kinetics of Fe-based amorphous alloys
    Hsiao, A
    Turgut, Z
    Willard, MA
    Selinger, E
    Laughlin, DE
    McHenry, ME
    Hasegawa, R
    ADVANCED HARD AND SOFT MAGNETIC MATERIALS, 1999, 577 : 551 - 556
  • [30] Evolution and Removal of Inclusions in Fe-Based Amorphous Alloys
    Zhang, Hua
    Mo, Shuai
    Yang, Ling
    Liu, Tao
    Wu, Yi-Nan
    Ni, Hong-Wei
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2022, 53 (10): : 3565 - 3572