Stabilization of martensitic microstructure in advanced 9Cr steel during creep at high temperature

被引:208
|
作者
Abe, F
Horiuchi, T
Taneike, M
Sawada, K
机构
[1] NIMS, Steel Res Ctr, Tsukuba, Ibaraki 3050047, Japan
[2] Hitachi Res Lab, Hitachi, Ibaraki 3191292, Japan
[3] NIMS, Mat Informat Technol Stn, Tsukuba, Ibaraki 3050047, Japan
关键词
9Cr steel; tempered martensite; creep rate; boron; M23C6; carbide; MX carbonitride;
D O I
10.1016/j.msea.2003.11.073
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In order to improve the long-term creep strength of 9%Cr steel, the stabilization of martensitic microstructure in the vicinity of prior austenite grain boundaries during creep has been investigated by the addition of boron and by a dispersion of nano-size MX nitrides. Creep tests were carried out at 923 K for up to about 3 x 10(4) h. Boron is enriched in the M23C6 carbides during aging and creep, especially in the vicinity of prior austenite grain boundaries. This reduces the coarsening rate of M23C6 carbides, which effectively stabilizes the martensitic microstructure in the vicinity of prior austenite grain boundaries. A dispersion of nano-sized MX nitrides but no M23C6 along boundaries also gives rise to excellent pinning force for migrating boundaries during creep, as shown by approximately two orders of magnitude longer time to rupture than ASME-P92. The stabilization of martensitic microstructure retards the onset of tertiary or acceleration creep, which results in lower minimum creep rate and longer time to rupture. (C) 2003 Published by Elsevier B.V.
引用
收藏
页码:299 / 303
页数:5
相关论文
共 50 条
  • [41] Creep behavior and microstructure of a 9Cr-3Co-3W martensitic steel
    Fedoseeva, A.
    Dudova, N.
    Kaibyshev, R.
    JOURNAL OF MATERIALS SCIENCE, 2017, 52 (05) : 2974 - 2988
  • [42] Mechanical characteristics and microstructure of weld joint of high-temperature martensitic steel containing 9% Cr
    Ya. E. Shakhova
    A. N. Belyakov
    R. O. Kaibyshev
    The Physics of Metals and Metallography, 2016, 117 : 378 - 389
  • [43] Mechanical characteristics and microstructure of weld joint of high-temperature martensitic steel containing 9% Cr
    Shakhova, Ya. E.
    Belyakov, A. N.
    Kaibyshev, R. O.
    PHYSICS OF METALS AND METALLOGRAPHY, 2016, 117 (04): : 378 - 389
  • [44] Microstructure characteristics and properties of yttrium-bearing 9Cr ferritic-martensitic steel cladding tubes
    Chen, Yingxue
    Yan, Qingzhi
    Zhang, Xiaoxin
    Yang, Jiabao
    Hong, Zhiyuan
    MATERIALS RESEARCH EXPRESS, 2019, 6 (09)
  • [45] Electrochemical Characterization Method of Laves Phase in 9Cr Martensitic Heat-Resistant Steel and Creep Life Prediction
    Yuan, Sui
    Li, Ji
    Guo, Qi
    Tang, Liying
    Xu, Jian
    Zhou, Rongcan
    Zhang, Hongjun
    CRYSTALS, 2023, 13 (11)
  • [46] Roles of Mn in the High-Temperature Air Oxidation of 9Cr Ferritic–Martensitic Steel After Severe Plastic Deformation
    Shenghu Chen
    Lijian Rong
    Oxidation of Metals, 2018, 89 : 415 - 428
  • [47] MICROSTRUCTURAL CHARACTERISATION OF CREEP TESTED 9CR WELDS FOR MARBN STEEL
    Guo, J.
    Jepson, M. A. E.
    Thomson, R. C.
    ADVANCES IN MATERIALS TECHNOLOGY FOR FOSSIL POWER PLANTS: PROCEEDINGS FROM THE EIGHTH INTERNATIONAL CONFERENCE, 2016, 2016, : 962 - 973
  • [48] Enhanced creep resistance of Y-bearing 9Cr ferritic/martensitic steel via vacuum casting technique
    Chen, Yingxue
    Hong, Zhiyuan
    Zhang, Xiaoxin
    Xia, Min
    Yan, Qingzhi
    Ge, Changchun
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (05): : 4588 - 4597
  • [49] Diffusion bonding of 9Cr ODS ferritic/martensitic steel with a phase transformation
    Noh, Sanghoon
    Kimura, Akihiko
    Kim, Tae Kyu
    FUSION ENGINEERING AND DESIGN, 2014, 89 (7-8) : 1746 - 1750
  • [50] Behavior of boron in 9Cr heat resistant steel during heat treatment and creep deformation
    Abe, Fujio
    Mechanical Behavior of Materials X, Pts 1and 2, 2007, 345-346 : 569 - 572