Effect of Mn addition on the precipitation and corrosion behaviour of 22% Cr economical duplex stainless steel after isothermal aging at 800 °C

被引:10
|
作者
Feng, Zaiqiang [1 ]
Yang, Yinhui [2 ]
Wang, Jia [3 ]
机构
[1] North China Univ Water Resources & Elect Power, Sch Mech Engn, Zhengzhou 450045, Peoples R China
[2] Kunming Univ Sci & Technol, Sch Mat Sci & Engn, Kunming 650093, Peoples R China
[3] Tongji Univ, Sch Mat Sci & Engn, Shanghai 200092, Peoples R China
基金
中国国家自然科学基金;
关键词
Metals and alloys; Intermetallics; Microstructure; Precipitation; Corrosion; SIGMA-PHASE PRECIPITATION; MECHANICAL-PROPERTIES; MICROSTRUCTURAL STABILITY; PITTING CORROSION; RESISTANCE; 800-DEGREES-C; CHLORIDE; CAST; ENVIRONMENTS; PARAMETERS;
D O I
10.1016/j.jallcom.2017.01.031
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The microstructural and corrosion behaviour of Fe-22Cr-1.9Ni-2.3Mo-0.2N-xMn low nickel type duplex stainless steel (DSS) with Mn contents ranging from 4.3 to 9.7 wt% were studied after aging treatment at 800 degrees C lasting from 30 to 930 min. The corrosion behaviour was investigated in 3.5 wt% NaCI solution by measurements of potentiodynamic polarisation and electrochemical impedance spectroscopy. The microstructural analysis shows that the sigma precipitates mainly nucleated along gamma/delta phase boundaries and grew into the adjacent delta-ferrite by prolonging the aging time, having the same eutectoid structures as commercial high-Ni DSS. At high Mn contents, the growth rate of a precipitates was initially high with aging times from 30 to 150 min, but decreased gradually up to 930 min with more Mn participation. A Mn content of 4.3 wt% brought only about a 150 mV pitting potential (E-b) drop for the aged specimens, while further addition of Mn significantly lowered E-b at the early stage of aging with more aging-induced a precipitates. The metastable pit nucleation resistance decreased with Mn content from 4.3 to 6.9 wt% and was suppressed by a higher Mn addition of 9.7 wt% for aging treatments from 150 to 930 min. The pits mainly initiated along gamma/delta boundaries and within delta ferrite, then propagated around a precipitates with increasing aging time, and more Mn gives rise to both the number and size of pits in the early stage of aging treatment. The charge transfer resistance (Rt) depends strongly on the existence of defects caused by the a precipitates, while increasing Mn content slightly decreases the passive film resistance (Rfilm) in specimens aged from 60 to 930 min. (C) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:334 / 344
页数:11
相关论文
共 50 条
  • [31] The effect of copper addition on the corrosion resistance of cast duplex stainless steel
    Lopes Ferreira de Lima, Hillane Mirelle
    Maior Tavares, Sergio Souto
    Martins, Marcelo
    Araujo, Walney Silva
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (02): : 2107 - 2119
  • [32] Effect of Aging on the Corrosion Resistance of 2209 Duplex Stainless Steel Weldments
    Donghoon Kang
    Nohoon Kim
    Haewoo Lee
    Metals and Materials International, 2019, 25 : 740 - 750
  • [33] Effect of aging on the corrosion resistance of 2101 lean duplex stainless steel
    Zhang, Lihua
    Jiang, Yiming
    Deng, Bo
    Zhang, Wei
    Xu, Juliang
    Li, Jin
    MATERIALS CHARACTERIZATION, 2009, 60 (12) : 1522 - 1528
  • [34] Effect of Aging on the Corrosion Resistance of 2209 Duplex Stainless Steel Weldments
    Kang, Donghoon
    Kim, Nohoon
    Lee, Haewoo
    METALS AND MATERIALS INTERNATIONAL, 2019, 25 (03) : 740 - 750
  • [35] Influence of isothermal aging on secondary phases precipitation and toughness of a duplex stainless steel SAF 2205
    Calliari, I.
    Zanesco, M.
    Ramous, E.
    JOURNAL OF MATERIALS SCIENCE, 2006, 41 (22) : 7643 - 7649
  • [36] Influence of isothermal aging on secondary phases precipitation and toughness of a duplex stainless steel SAF 2205
    I. Calliari
    M. Zanesco
    E. Ramous
    Journal of Materials Science, 2006, 41 : 7643 - 7649
  • [37] Effect of isothermal treatment of aging on the microstructure and the mechanical properties of a duplex stainless steel
    Arruti, Javier
    Saenz, Laura
    Mejias, Alberto
    Cepeda, Javier
    INGENIERIA UC, 2012, 19 (03): : 23 - 33
  • [38] Investigation on the solution treated behavior of economical 19Cr duplex stainless steels by Mn addition
    Yang, Yinhui
    Cao, Jianchun
    Gu, Yang
    MATERIALS & DESIGN, 2015, 83 : 820 - 828
  • [39] Effect of Aging on Precipitation Behavior and Pitting Corrosion Resistance of SAF2906 Super Duplex Stainless Steel
    Li, Jianchun
    Li, Guoping
    Liang, Wei
    Han, Peide
    Wang, Hongxia
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (09) : 4533 - 4543
  • [40] Study of the effect of sigma phase precipitation on the sliding wear and corrosion behaviour of duplex stainless steel AISI 2205
    del Abra-Arzola, J. L.
    Garcia-Renteria, M. A.
    Cruz-Hernandez, V. L.
    Garcia-Guerra, J.
    Martinez-Landeros, V. H.
    Falcon-Franco, L. A.
    Curiel-Lopez, F. F.
    WEAR, 2018, 400 : 43 - 51