Fabrication of 2D C/ZrC-SiC composite and its structural evolution under high-temperature treatment up to 1800 °C

被引:79
|
作者
Li, Houbu [1 ]
Zhang, Litong [1 ]
Cheng, Laifei [1 ]
Wang, Yiguang [1 ]
机构
[1] Northwestern Polytech Univ, Natl Key Lab Thermostruct Composite Mat, Xian 710072, Peoples R China
关键词
Precursors: organic; Composites; Whiskers; Structural evolution; SILICON-CARBIDE WHISKERS; MATRIX COMPOSITES; SLURRY INFILTRATION; THERMAL-STABILITY; C/SIC COMPOSITES; GROWTH-MECHANISM; FIBER; POLYCARBOSILANE;
D O I
10.1016/j.ceramint.2009.03.030
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Two-dimensional C/ZrC-SiC composites were fabricated by chemical vapor infiltration (CVI) process combined with a modified polymer infiltration and pyrolysis (PIP) method. Two kinds of ZrC slurries (ZrC aqueous slurry and ZrC/polycarbosilane slurry) were employed to densify composites before the PIP process. The as-produced C/ZrC-SiC composites exhibited better mechanical properties than the C/SiC composites densified only by CVI and PIP process. Structural evolution for C/ZrC-SiC composites treated in the range 1200-1800 degrees C mainly consisted of the change of SiC whiskers and the decomposition of polymer derived ceramic. (C) 2009 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:2831 / 2836
页数:6
相关论文
共 50 条
  • [1] Ablation behavior of a SiC/ZrC-SiC coating on C/CA composite for high-temperature thermal protection
    Yang, Lingkun
    Sun, Wei
    Xu, Junjie
    Xiong, Xiang
    Wang, Lidong
    Zuo, Jinlv
    Yang, Bo
    CERAMICS INTERNATIONAL, 2024, 50 (11) : 20447 - 20459
  • [2] Mechanism of ablation of 3D C/ZrC-SiC composite under an oxyacetylene flame
    Chen, Si'an
    Zhang, Changrui
    Zhang, Yudi
    Zhao, Dan
    Hu, Haifeng
    Zhang, Zhibin
    CORROSION SCIENCE, 2013, 68 : 168 - 175
  • [3] Reactive hot pressing of ZrB2-SiC-ZrC ultra high-temperature ceramics at 1800°C
    Wu, Wen-Wen
    Zhang, Guo-Jun
    Kan, Yan-Mei
    Wang, Pei-Ling
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2006, 89 (09) : 2967 - 2969
  • [4] Fabrication and mechanical behaviors of 2D C/SiC-BCx composite at room temperature
    Liu, Yongsheng
    Cheng, Laifei
    Zhang, Litong
    Yang, Wenbin
    Zhou, Shengtian
    Zhang, Weihua
    JOURNAL OF COMPOSITE MATERIALS, 2012, 46 (10) : 1251 - 1260
  • [5] High-temperature properties and microstructure evolution of C/C-ZrC-SiC composites fabricated by reactive melt infiltration
    Xu, Chongqing
    Jia, Chenglan
    Peng, Zheng
    Chen, Sian
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (10)
  • [6] Enhanced high-temperature strength of HfB2-SiC composite up to 1600 °C
    Guo, Shuqi
    Liu, Tianwei
    Ping, De-Hai
    Nishimura, Toshiyuki
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (04) : 1152 - 1157
  • [7] Fabrication and properties of 2D C/C-ZrB2-ZrC-SiC composites by hybrid precursor infiltration and pyrolysis
    Wu, Haitang
    Xie, Changming
    Zhang, Weigang
    Zhang, Junhua
    ADVANCES IN APPLIED CERAMICS, 2013, 112 (06) : 366 - 373
  • [8] Effect of reaction melt infiltration temperature on the ablation properties of 2D C/C-SiC-ZrC composites
    Li, Zhaoqian
    Li, Hejun
    Zhang, Shouyang
    Wang, Jie
    Li, Wei
    Sun, Fengjiao
    CORROSION SCIENCE, 2012, 58 : 12 - 19
  • [9] Oxidation analysis of 2D C/ZrC-SiC composites with different coating structures in CH4 combustion gas environment
    Li, Houbu
    Zhang, Litong
    Cheng, Laifei
    Wang, Yiguang
    CERAMICS INTERNATIONAL, 2009, 35 (06) : 2277 - 2282
  • [10] Damage Characteristics of 2D C/SiC-ZrC Composites under Low Velocity Impact
    Pi Huilong
    Zhang Baopeng
    Yu Xinmin
    Liu Wei
    Jin Xin
    JOURNAL OF INORGANIC MATERIALS, 2020, 35 (12) : 1327 - 1332