Effect of immediate and delayed dentin sealing on the fracture strength, failure type and Weilbull characteristics of lithiumdisilicate laminate veneers

被引:46
|
作者
Gresnigt, Marco M. M. [1 ]
Cune, Marco S. [1 ]
de Roos, Joanne G. [1 ]
Ozcan, Mutlu [2 ]
机构
[1] Univ Groningen, Univ Med Ctr Groningen, Ctr Dent & Oral Hyg, Dept Fixed & Removable Prosthodont, Antonius Deusinglaan 1, NL-9713 AV Groningen, Netherlands
[2] Univ Zurich, Dent Mat Unit, Ctr Dent & Oral Med, Clin Fixed & Removable Prosthodont & Dent Mat Sci, Zurich, Switzerland
关键词
Adhesion; Bonding; Cementation; Ceramic; Dentin; Immediate dentin sealing; Laminate; Veneer; MICROTENSILE BOND STRENGTH; PORCELAIN VENEERS; CLINICAL-PERFORMANCE; RESIN COMPOSITE; RESTORATIONS; ADAPTATION; ADHESIVES; CROWN; ETCH;
D O I
10.1016/j.dental.2016.01.001
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. Adhesion on dentin is less reliable than on enamel, which could affect the durability of laminate veneers (LV). Immediate dentin sealing (IDS) is suggested instead of delayed dentin sealing (DDS) to overcome hypersensitivity and prevent debonding from dentin. This study evaluated the effect of IDS and DDS on the durability of Li2Si2O5 laminate veneers in vitro. Methods. Window preparations were made on the labial surfaces of sound maxillary central incisors (N=50). They were randomly divided into five groups: Group 1: Enamel only + H3PO4 Adhesive (control); Group 2: <1/4 dentin + H3PO4 DDS (2 weeks later); Group 3: Complete dentin + H3PO4 DDS (2 weeks later); Group 4: <1/4 dentin + H3PO4 IDS; Group 5: Complete dentin + H3PO4 + IDS. Li2Si2O5 laminate veneers (e.max Press) were bonded to the labial surfaces of the teeth with adhesive resin cement (Variolink Veneer). IDS layers were silicacoated (CoJet System) and silanized (ESPE-Sil). The teeth with their bonded laminates were thermocycled (10.000x cycles) and then subjected to static loading (1 mm/min). Failure type and location after debonding were classified. Data were analyzed using ANOVA and Tukey's post hoc test (alpha = 0.05). Two-parameter Weibull distribution values including the Weibull modulus, scale (m) and shape (o), values were calculated. Results. Mean fracture strength (N) per group in descending order was as follows: Group 5 (576 +/- 254), Group 4 (478 +/- 216), Group 1 (473 +/- 159), Group 2 (465 +/- 186), and Group 3 (314 +/- 137). The presence of complete dentin exposure sealed with DDS after 2 weeks on the bonded surface (Group 3) resulted in significantly lower fracture strength results than those in group 5 with IDS (p = 0.034). Weibull distribution presented higher shape (o) for Group 1 (3.67), than those of other groups (2.51-2.89). Failure types were predominantly adhesive failure between the cement and the laminate veneer in Groups 1, 2, 4 whereas Group 3 presented more often complete adhesive failures between the cement and dentin. In Group 5, failures showed some IDS and cement with or without ceramic fracture attached on the tooth. Significance. When laminate veneers are bonded to a large dentin substrate, application of immediate dentin sealing improves adhesion and thereby, the fracture strength of Li2Si2O5 laminate veneers. (C) 2016 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:E73 / E81
页数:9
相关论文
共 27 条
  • [21] Effect of radiotherapy, immediate dentin sealing and irrigation simulating single- or two-visits endodontic treatment on the bond strength to pulp chamber dentin: an in vitro study
    Pauletto, Guilherme
    Machry, Renan Vaz
    Baumhardt, Tadeu
    Daudt, Natalia de Freitas
    Pereira, Gabriel Kalil Rocha
    Bier, Carlos Alexandre Souza
    ODONTOLOGY, 2025, 113 (01) : 261 - 273
  • [22] Experimental study of effects of fracture type on strength characteristics and failure modes of fractured rockmass
    Liu Xue-wei, m
    Liu Quan-sheng
    Chen Yuan
    Li Qiang
    ROCK AND SOIL MECHANICS, 2015, 36 : 208 - 214
  • [23] Effect of immediate dentin sealing on load-bearing capacity under accelerated fatigue of thin occlusal veneers made of CAD-CAM glass-ceramic and resin composite material
    Mueller, Bruna
    Pilecco, Rafaela Oliveira
    Valandro, Luiz Felipe
    Ruschel, Vanessa Carla
    Pereira, Gabriel Kalil Rocha
    Bernardon, Jussara Karina
    DENTAL MATERIALS, 2023, 39 (04) : 372 - 382
  • [24] Biaxial flexural strength and Weilbull characteristics of adhesively luted hybrid and reinforced CAD/CAM materials to dentin: effect of self-etching ceramic primer versus hydrofluoric acid etching
    Mendes Tribst, Joao Paulo
    de Oliveira Dal Piva, Amanda Maria
    Lopes, Gabriel Cirone
    Souto Borges, Alexandre Luiz
    Bottino, Marco Antonio
    Ozcan, Mutlu
    de Melo, Renata Marques
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2020, 34 (12) : 1253 - 1268
  • [25] Computer-Aided-Design/Computer-Assisted-Manufactured Adhesive Restoration of Molars with a Compromised Cusp: Effect of Fiber-Reinforced Immediate Dentin Sealing and Cusp Overlap on Fatigue Strength
    Ritter, Andre V.
    JOURNAL OF ESTHETIC AND RESTORATIVE DENTISTRY, 2012, 24 (02) : 147 - 147
  • [26] Experimental study of the effect of silica fume and coarse aggregate type on the fracture characteristics of high-strength concrete
    Mousavi, Seyed Mohammad
    Ranjbar, Malek Mohammad
    ENGINEERING FRACTURE MECHANICS, 2021, 258
  • [27] Fracture strength, failure type and Weibull characteristics of lithium disilicate and multiphase resin composite endocrowns under axial and lateral forces
    Gresnigt, Marco M. M.
    Ozcan, Mutlu
    van den Houten, Mieke L. A.
    Schipper, Laura
    Cune, Marco S.
    DENTAL MATERIALS, 2016, 32 (05) : 607 - 614