Failure Mechanism and Interface Engineering for NASICON-Structured All-Solid-State Lithium Metal Batteries

被引:88
|
作者
He, Linchun [1 ]
Sun, Qiaomei [1 ]
Chen, Chao [1 ,2 ]
Oh, Jin An Sam [1 ,4 ,5 ]
Sun, Jianguo [1 ]
Li, Minchan [1 ]
Tu, Wenqiang [1 ]
Zhou, Henghui [3 ]
Zeng, Kaiyang [1 ]
Lu, Li [1 ,2 ]
机构
[1] Natl Univ Singapore, Dept Mech Engn, Singapore 117575, Singapore
[2] Natl Univ Singapore Suzhou Res Inst, Suzhou 215123, Peoples R China
[3] Peking Univ, Coll Chem & Mol Engn, Beijing 100871, Peoples R China
[4] Natl Univ Singapore, Grad Sch Integrat Sci & Engn, Singapore 138632, Singapore
[5] ASTAR, Singapore Inst Mfg Technol, 2 Fusionopolis Way, Singapore 138634, Singapore
关键词
all-solid-state lithium metal battery; NASICON structure; solid-state electrolyte; failure mechanism; interface; IONIC-CONDUCTIVITY; ELECTROLYTE; TEMPERATURE; STABILITY; ORIGIN; BULK;
D O I
10.1021/acsami.9b05516
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
All-solid-state lithium metal batteries (ASSLiMB) have been considered as one of the most promising next-generation high-energy storage systems that replace liquid organic electrolytes by solid-state electrolytes (SSE). Among many different types of SSE, NASICON-structured Li1+xAlxGe2-x(PO3)(4) (LAGP) shows high a ionic conductivity, high stability against moisture, and wide working electrochemical windows. However, it is unstable when it is in contact with molten Li, hence largely limiting its applications in ASSLiMB. To solve this issue, we have studied reaction processes and mechanisms between LAGP and molten Li, based on which a failure mechanism is hence proposed. With better understanding the failure mechanism, a thin thermosetting Li salt polymer, P(AAco-MA)Li, layer is coated on the bare LAGP pellet before contacting with molten Li. To further increase the ionic conductivity of P(AA-co-MA)Li, LiCl is added in P(AA-co-MA)Li. A symmetric cell of Li/interface/LAGP/interface/Li is prepared using molten Li-Sn alloy and galvanically cycled at current densities of 15, 30, and 70 mu A cm(-2) for 100 cycles, showing stable low overpotentials of 0.036, 0.105, and 0.257 V, respectively. These electrochemical results demonstrate that the interface coating of P(AA-co-MA)Li can be an effective method to avoid an interfacial reaction between the LAGP electrolyte and molten Li.
引用
收藏
页码:20895 / 20904
页数:10
相关论文
共 50 条
  • [41] PEO kaolinite intercalation interface accelerates lithium-ion transfer for all-solid-state lithium metal batteries
    Li, Huiyao
    Ao, Zhuoran
    Wan, Yu
    Liang, Yaru
    Li, Peiguang
    Zou, Youlan
    ELECTROCHIMICA ACTA, 2024, 507
  • [42] Engineering a High-Voltage Durable Cathode/Electrolyte Interface for All-Solid-State Lithium Metal Batteries via In Situ Electropolymerization
    Li, Qi
    Zhang, Xiaoyu
    Peng, Jian
    Wang, Zhihao
    Rao, Zhixiang
    Li, Yuyu
    Li, Zhen
    Fang, Chun
    Han, Jiantao
    Huang, Yunhui
    ACS APPLIED MATERIALS & INTERFACES, 2022, 14 (18) : 21018 - 21027
  • [43] Integrated interface configuration by in-situ interface chemistry enabling uniform lithium deposition in all-solid-state lithium metal batteries
    Yu-Long Liao
    Jiang-Kui Hu
    Zhong-Heng Fu
    Chen-Zi Zhao
    Yang Lu
    Shuai Li
    Shi-Jie Yang
    Shuo Sun
    Xi-Long Wang
    Jia Liu
    Jia-Qi Huang
    Hong Yuan
    Journal of Energy Chemistry, 2023, 80 (05) : 458 - 465
  • [44] Unlocking the Failure Mechanism of Solid State Lithium Metal Batteries
    Liu, Jia
    Yuan, Hong
    Liu, He
    Zhao, Chen-Zi
    Lu, Yang
    Cheng, Xin-Bing
    Huang, Jia-Qi
    Zhang, Qiang
    ADVANCED ENERGY MATERIALS, 2022, 12 (04)
  • [45] Integrated interface configuration by in-situ interface chemistry enabling uniform lithium deposition in all-solid-state lithium metal batteries
    Liao, Yu-Long
    Hu, Jiang-Kui
    Fu, Zhong-Heng
    Zhao, Chen-Zi
    Lu, Yang
    Li, Shuai
    Yang, Shi-Jie
    Sun, Shuo
    Liu, Jia
    Huang, Jia-Qi
    Yuan, Hong
    JOURNAL OF ENERGY CHEMISTRY, 2023, 80 : 458 - 465
  • [46] Unveiling the role of ring-structured organosulfur additives in solid-state electrolytes for all-solid-state lithium metal batteries
    Lee, Jung Seok
    Hong, Tae Hwa
    Kim, Dong Jun
    Jung, Hyun Wook
    Jung, Han Young
    Moon, Sunhwa
    You, Jungmok
    Lee, Jung Tae
    CHEMICAL ENGINEERING JOURNAL, 2025, 509
  • [47] Reaction and degradation mechanism in all-solid-state lithium-air batteries
    Kitaura, Hirokazu
    Zhou, Haoshen
    CHEMICAL COMMUNICATIONS, 2015, 51 (99) : 17560 - 17563
  • [48] Cell failures of all-solid-state lithium metal batteries with inorganic solid electrolytes: Lithium dendrites
    Ke, Xinyou
    Wang, Yan
    Dai, Liming
    Yuan, Chris
    ENERGY STORAGE MATERIALS, 2020, 33 : 309 - 328
  • [49] Recent Strategies for Stabilizing Interfaces in All-solid-state Lithium Metal Batteries
    Seol, Yoon-Jeong
    Kim, Namhyung
    KOREAN JOURNAL OF CHEMICAL ENGINEERING, 2025,
  • [50] Composite solid electrolytes for all-solid-state lithium batteries
    Dirican, Mahmut
    Yan, Chaoyi
    Zhu, Pei
    Zhang, Xiangwu
    MATERIALS SCIENCE & ENGINEERING R-REPORTS, 2019, 136 (27-46): : 27 - 46