ELEMENT PARTITIONING IN LOW-CARBON Si2Mn2CrMoVNb TRIP-ASSISTED STEEL IN INTERCRITICAL TEMPERATURE RANGE

被引:5
|
作者
Efremenko, Vasily [1 ]
Kussa, Roman [1 ]
Petryshynets, Ivan [2 ]
Shimizu, Kazumichi [3 ]
Kromka, Frantisek [2 ]
Zurnadzhy, Vadim [1 ]
Gavrilova, Victoria [1 ]
机构
[1] Pryazovskyi State Tech Univ PSTU, Vul Univ Ska 7, UA-87555 Mariupol, Ukraine
[2] Slovak Acad Sci, Inst Mat Res, Watsonova 1935-47, Kosice 04001, Slovakia
[3] Muroran Inst Technol, 27-1 Mizumotocho, Muroran, Hokkaido 0508585, Japan
来源
ACTA METALLURGICA SLOVACA | 2020年 / 26卷 / 03期
关键词
TRIP-assisted steel; annealing; SEM/EDX; element partitioning; ferrite; martensite; MECHANICAL-PROPERTIES; RETAINED AUSTENITE; GRINDING MEDIA; BEHAVIOR; TRANSFORMATION; MICROSTRUCTURE; SI; DECARBURIZATION; PRINCIPLES; DIFFUSION;
D O I
10.36547/ams.26.3.554
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The present paper is aimed at the study of the kinetics of Mn, Si, Cr partitioning in 0.2wt%C-Si2Mn2CrMoVNb TRIP-assisted steel under the annealing at 770 oC and 830 oC to be within the intercritical temperature range. The work was fulfilled using SEM, EDX, dilatometry, and hardness measurements. It was found that under heating a redistribution of the alloying elements between ferrite and austenite took place. Specifically, silicon partitioned to ferrite while chromium diffused to austenite with distribution coefficient values of 1.12-1.21 (K-Si) and 0.75-0.86 (K-Cr). Manganese was found to partition to a much greater extent resulting in a distribution coefficient of K-Mn=0.38-0.50 and 2.6 times higher concentration in austenite as compared to ferrite. As annealing temperature raised from 770 degrees C to 830 degrees C the elemental partitioning was accelerated, followed by the decrease in manganese content in austenite (by 1.44 time) and ferrite (by 1.34 time) caused by an increase in austenite volume fraction. Silicon featured uneven distribution within ferrite to be accumulated at the "martensite/ferrite" interface and near ferrite grain boundaries, while manganese was concentrated in MC carbides. The recommendation for annealing holding was formulated based on elemental partitioning kinetics.
引用
收藏
页码:116 / 121
页数:6
相关论文
共 48 条
  • [31] Acoustic properties of low-carbon 2% Mn-doped steel manufactured by laser powder bed fusion technology
    Murav'eva, Olga
    Murav'ev, Vitaly
    Volkova, Ludmila
    Kazantseva, Nataliya
    Nichipuruk, Alexander
    Stashkov, Alexey
    ADDITIVE MANUFACTURING, 2022, 51
  • [32] SUBSTRUCTURAL EVOLUTION OF FERRITE IN A LOW-CARBON STEEL DURING HOT DEFORMATION IN (F+A) 2-PHASE RANGE
    WANG, RH
    LEI, TC
    SCRIPTA METALLURGICA ET MATERIALIA, 1993, 28 (05): : 629 - 632
  • [33] DYNAMIC RECRYSTALLIZATION OF FERRITE IN A LOW-CARBON STEEL DURING HOT-ROLLING IN THE (F+A) 2-PHASE RANGE
    WANG, RZ
    LEI, TC
    SCRIPTA METALLURGICA ET MATERIALIA, 1994, 31 (09): : 1193 - 1196
  • [34] High-temperature nitriding of low-carbon martensitic steel 12Kh2G2NMFB in nontoxic salt melts
    D. M. Larinin
    L. M. Kleiner
    A. A. Shatsov
    Metal Science and Heat Treatment, 2008, 50 : 502 - 507
  • [35] High-temperature nitriding of low-carbon martensitic steel 12Kh2G2NMFB in nontoxic salt melts
    Larinin, D. M.
    Kleiner, L. M.
    Shatsov, A. A.
    METAL SCIENCE AND HEAT TREATMENT, 2008, 50 (9-10) : 502 - 507
  • [36] Effect of bainite isothermal temperature on microstructure and properties of 0.2C-1.5Si-2Mn-0.43Cu-0.26Ni TRIP steel
    Engineering Research Institute, University of Science and Technology Beijing, Beijing, China
    Cailiao Rechuli Xuebao, 10 (128-133):
  • [37] Low-temperature and low-carbon thermal decomposition of phosphogypsum by steel slag and H2S: Thermodynamic, kinetic and DFT studies
    Du, Wang
    Ma, Liping
    Yin, Xia
    Liu, Hongpan
    Xie, Longgui
    Luo, Yuetao
    Zhang, Wei
    Yang, Jie
    Dai, Quxiu
    CHEMICAL ENGINEERING JOURNAL, 2025, 504
  • [38] Optimization of CaO-SiO2-Al2O3-MgO-CaF2 refining slag in low-carbon and aluminum-containing 20Mn2 steel
    Guo, Bao-Qi
    Bao, Yan-Ping
    Wang, Min
    Lin, Lu
    Gongcheng Kexue Xuebao/Chinese Journal of Engineering, 2015, 37 (11): : 1415 - 1421
  • [39] Increasing Low-Temperature Toughness of 09Mn2Si Steel through Lamellar Structuring by Helical Rolling
    Panin, Sergey
    Vlasov, Ilya
    Moiseenko, Dmitry
    Maksimov, Pavel
    Maruschak, Pavlo
    Yakovlev, Alexander
    Gomorova, Julia
    Mishin, Ivan
    Schmauder, Siegfried
    METALS, 2021, 11 (02) : 1 - 29
  • [40] Effect of final cooling temperature on mechanical properties of a water cooled Mn-series low carbon bainitic steel as 8Mn2SiNb
    Feng Chun
    Pan Zhi Yong
    Li Guang Shan
    Bai Bing Zhe
    ADVANCES IN CHEMICAL ENGINEERING, PTS 1-3, 2012, 396-398 : 468 - +