Effect of Heat Treatment on Structure and Wear Resistance of High Chromium Cast Steel Containing Boron

被引:16
|
作者
Cen, Qi-hong [1 ]
Zhang, Hai-bin [2 ]
Fu, Han-guang [2 ]
机构
[1] Kunming Univ Sci & Technol, Sch Mat Sci & Engn, Natl Engn Res Ctr Waste Resource Recovery, Kunming 650093, Yunnan, Peoples R China
[2] Beijing Univ Technol, Sch Mat Sci & Engn, Beijing 100124, Peoples R China
基金
中国国家自然科学基金;
关键词
high chromium cast steel; boron alloying; microstructure; mechanical property; wear resistance; MICROSTRUCTURE; TITANIUM; NIOBIUM; IRON;
D O I
10.1016/S1006-706X(14)60083-2
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The microstructure, mechanical properties and wear resistance of high chromium cast steel containing boron after different heat treatments were studied by means of the optical microscopy (OM), the scanning electron microscopy (SEM), X-ray diffraction (XRD), hardness, impact toughness, tensile and pin-on-disc abrasion tests'. The results show that as-cast microstructures of boron-free high chromium steel consist of martensite and a few (Cr, Fe)(7)C-3 carbide, and the macro-hardness of boron-free high chromium steel is 55-57 HRC. After 0.5 mass% B was added into high chromium cast steel, as-cast structure transforms into eutectic (Fe, Cr)(2)B, (Cr, Fe)(7) (C, B)(3) and martensite, and the macro-hardness reaches 58-60 HRC. High temperature quenching leads to the disconnection and isolated distribution of boride, and there are many (Cr, Fe)(23) (C, B)(6) precipitated phases in the quenching structure. Quenching from 1050 degrees C, high chromium steel obtained the highest hardness, and the hardness of high chromium cast steel containing boron is higher than that of boron-free high chromium steel. The change of quenching temperature has no obvious effect on impact toughness of high chromium steel, and the increase of quenching temperature leads to tensile strength having an increasing tendency. At the same quenching temperature, the wear resistance of high chromium cast steel containing boron is more excellent than that of boron-free high chromium steel. High chromium cast steel guide containing boron has good performance while using in steel bar mill.
引用
收藏
页码:532 / 538
页数:7
相关论文
共 50 条
  • [31] RESEARCH AND APPLICATION OF AS-CAST WEAR RESISTANCE HIGH CHROMIUM CAST IRON
    Liu Jinhai Liu Gensheng Li Guolu Hebei University of Technology Wang Kunjun CHINESE JOURNAL OF MECHANICAL ENGINEERINGVolume 11 Number 2 1998 Zhang Jiakou Xuanhau Science and Technology Development Co. Zeng Daben Qinghua University
    Chinese Journal of Mechanical Engineering(English Edition), 1998, (02) : 51 - 56
  • [32] Research and application of as-cast wear resistance high chromium cast iron
    Liu, Jinhai
    Liu, Gensheng
    Li, Guolu
    Wang, Kunjun
    Zeng, Daben
    Chinese Journal of Mechanical Engineering (English Edition), 1998, 11 (02): : 130 - 135
  • [33] Effect of heat treatment on the structure and properties of cast steel shot
    S. V. Grachev
    L. A. Mal’tseva
    O. V. Zhuikov
    V. P. Gvozdovskii
    S. N. Shlyapnikov
    A. F. Emel’yanov
    Metal Science and Heat Treatment, 2006, 48 : 166 - 169
  • [34] Effect of heat treatment on the structure and properties of cast steel shot
    Grachev, S. V.
    Mal'tseva, L. A.
    Zhuikov, O. V.
    Gvozdovskii, V. P.
    Shlyapnikov, S. N.
    Emel'yanov, A. F.
    METAL SCIENCE AND HEAT TREATMENT, 2006, 48 (3-4) : 166 - 169
  • [35] Effect of post-welding heat treatment on wear resistance of cast-steel die with surfacing layer
    Xu, Wujiao
    Ma, Xin
    Tang, Nongjie
    Zhu, Li
    Li, Wuhua
    Ding, Yongfeng
    MANUFACTURING REVIEW, 2015, 2
  • [36] Wear Resistance of High-Chromium Cast Iron.
    Matsui, A.
    Hara, M.
    Aufbereitungs-Technik/Mineral Processing, 1975, 16 (08): : 418 - 424
  • [37] Effect of Si on Microstructure and Wear Resistance of Hypereutectic High-Chromium Cast Iron
    Chen, Zhengyang
    Fu, Hanguang
    Wang, Feng
    Yuan, Naibo
    Lin, Jian
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (12) : 5450 - 5465
  • [38] Effect of Si on Microstructure and Wear Resistance of Hypereutectic High-Chromium Cast Iron
    Zhengyang Chen
    Hanguang Fu
    Feng Wang
    Naibo Yuan
    Jian Lin
    Journal of Materials Engineering and Performance, 2023, 32 : 5450 - 5465
  • [39] Influence of Heat Treatment on Erosive Wear Resistance of High Cr Cast Irons
    Ngo, Huynh Kinh Luan
    Yamamoto, Kaoru
    Okuyama, Tetsuya
    Nakayama, Masaru
    Mizuno, Kuniaki
    Koizumi, Koreaki
    INTERNATIONAL JOURNAL OF METALCASTING, 2024,
  • [40] High wear resistance cast high-speed steel
    Kononov, AA
    Salmanov, NS
    Salmanov, MN
    MODERN TECHNIQUES AND TECHNOLOGY: MTT' 2000, 2000, : 159 - 160