Long term ageing effect on fracture toughness of the GTAW welded joints for nuclear power main pipelines

被引:7
|
作者
Wu, Songwei [1 ]
Zhang, Zhe [2 ]
机构
[1] Quzhou Univ, Coll Civil Engn & Architecture, Quzhou 324000, Zhejiang, Peoples R China
[2] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300350, Peoples R China
关键词
Thermal ageing; Gas tungsten arc welding (GTAW) joints; Fracture toughness; Nuclear power main pipelines; Crack initiation; Stretch zone width (SZW); AUSTENITIC STAINLESS-STEEL; STRETCH ZONE; MICROSTRUCTURE EVOLUTION; MECHANICAL-PROPERTIES; CORROSION-RESISTANCE; STRAIN LOCALIZATION; EMBRITTLEMENT; TIG; DEFORMATION; PARAMETERS;
D O I
10.1016/j.ijpvp.2020.104250
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Gas tungsten arc welding (GTAW) joints of nuclear power main pipelines were subjected on accelerated thermal ageing tests until 30000 h to investigate long-term ageing effect on fracture property. The results indicate that fracture toughness values J(IC) and J(SZW) of both base metals and welded metals decreases clearly and fracture mode transits subsequently from typical ductile to brittle fracture with increasing ageing time, but J-resistance (J-R) curves still lie above the recommend low-bound lines given by NUREG/CR after 30000 h thermal ageing. Moreover, base metals have better fracture toughness than welded metals regardless of thermal ageing time, and thus welded metals are still the weakest part for the whole welded joints. In addition, thermal ageing has no significantly influence on the location of crack initiation at the crack tip and crack growth mode because the thermal ageing could enhance the hardness and strength of ferrite phases and thus the austenite phases still have lower strength.
引用
收藏
页数:11
相关论文
共 50 条
  • [41] RESEARCH ACTIVITIES IN THE EUROPEAN UNION ON AGEING MANAGEMENT FOR LONG TERM OPERATION OF NUCLEAR POWER PLANTS
    Martin, Oliver
    Ballesteros, Antonio
    Bruynooghe, Christiane
    Bieth, Michel
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE 2010, VOL 5, 2010, : 193 - 198
  • [42] Effect of long-term water immersion on the fracture toughness of denture base and reline resins
    Finoti, Livia Sertori
    Machado, Ana Lucia
    Lima Chaves, Carolina De Andrade
    Pavarina, Ana Claudia
    Vergani, Carlos Eduardo
    GERODONTOLOGY, 2012, 29 (02) : E858 - E864
  • [43] Effect of composition on the tensile properties and fracture toughness of A7N01S-T5 aluminum alloys welded joints
    Liu, Yali
    Gou, Guoqing
    Chen, Jia
    Chen, Hui
    Wang, Wanjng
    Li, Xiaodong
    Che, Xiaoli
    Wang, Yirong
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2017, 31 (16-19):
  • [44] EVALUATION OF FRACTURE-TOUGHNESS OF THICK PLATES AND WELDED-JOINTS FOR A NUCLEAR-REACTOR PRESSURE-VESSEL BY DC ELECTRICAL POTENTIAL METHOD
    KODAIRA, T
    MATSUMOTO, M
    FUKAYA, K
    OKU, T
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1983, 23 (08) : B302 - B302
  • [45] Experimental study of the effect of pre-bond contamination with de-icing fluid and ageing on the fracture toughness of composite bonded joints
    Moutsompegka, E.
    Tserpes, K. I.
    Polydoropoulou, P.
    Tornow, C.
    Schlag, M.
    Brune, K.
    Mayer, B.
    Pantelakis, S.
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2017, 40 (10) : 1581 - 1591
  • [46] Suppression of Type IV fracture in welded joints of advanced ferritic power plant steels - effect of boron and nitrogen
    Abe, F.
    Tabuchi, M.
    Kondo, M.
    Okada, H.
    MATERIALS AT HIGH TEMPERATURES, 2006, 23 (3-4) : 145 - 154
  • [47] Identification and analysis of a reverse dynamic strain ageing in welded joints of C-Mn steels in the secondary circuit welds of nuclear power plants
    Mottay, W.
    Hoummada, K.
    Brechet, Y.
    Massardier, V.
    Perrin-Pellegrino, C.
    Maugis, P.
    Roch, F.
    Goune, M.
    SCRIPTA MATERIALIA, 2024, 247
  • [48] EFFECT OF THE WELDING PROCESS AND HEAT INPUT ON THE FRACTURE-TOUGHNESS OF WELDED-JOINTS IN HIGH-STRENGTH LOW-ALLOY STEEL
    SUNDARAM, P
    PANDEY, RK
    KUMAR, AN
    MATERIALS SCIENCE AND ENGINEERING, 1987, 91 : 29 - 38
  • [49] Effect of long-term formalin preservation on the bending properties and fracture toughness of bovine compact bone
    Kikugawa, H
    Asaka, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2005, 69 (02) : 267 - 271
  • [50] Effect of long-term stress and temperature exposure on the fracture toughness of Ti-62222 alloy
    Singhal, S
    Tucker, J
    Saxena, A
    ENGINEERING FRACTURE MECHANICS, 1999, 64 (06) : 799 - 803