Long term ageing effect on fracture toughness of the GTAW welded joints for nuclear power main pipelines

被引:7
|
作者
Wu, Songwei [1 ]
Zhang, Zhe [2 ]
机构
[1] Quzhou Univ, Coll Civil Engn & Architecture, Quzhou 324000, Zhejiang, Peoples R China
[2] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300350, Peoples R China
关键词
Thermal ageing; Gas tungsten arc welding (GTAW) joints; Fracture toughness; Nuclear power main pipelines; Crack initiation; Stretch zone width (SZW); AUSTENITIC STAINLESS-STEEL; STRETCH ZONE; MICROSTRUCTURE EVOLUTION; MECHANICAL-PROPERTIES; CORROSION-RESISTANCE; STRAIN LOCALIZATION; EMBRITTLEMENT; TIG; DEFORMATION; PARAMETERS;
D O I
10.1016/j.ijpvp.2020.104250
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Gas tungsten arc welding (GTAW) joints of nuclear power main pipelines were subjected on accelerated thermal ageing tests until 30000 h to investigate long-term ageing effect on fracture property. The results indicate that fracture toughness values J(IC) and J(SZW) of both base metals and welded metals decreases clearly and fracture mode transits subsequently from typical ductile to brittle fracture with increasing ageing time, but J-resistance (J-R) curves still lie above the recommend low-bound lines given by NUREG/CR after 30000 h thermal ageing. Moreover, base metals have better fracture toughness than welded metals regardless of thermal ageing time, and thus welded metals are still the weakest part for the whole welded joints. In addition, thermal ageing has no significantly influence on the location of crack initiation at the crack tip and crack growth mode because the thermal ageing could enhance the hardness and strength of ferrite phases and thus the austenite phases still have lower strength.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Fracture toughness of welded joints materials for main pipelines at Ignalina NPP
    Daunys, M
    Krasauskas, P
    Dundulis, R
    NUCLEAR ENGINEERING AND DESIGN, 2005, 235 (07) : 747 - 760
  • [2] A comparison between fracture toughness at different locations of SMAW and GTAW welded joints of primary coolant piping
    Yu, Weiwei
    Fan, Minyu
    Shi, Jinhua
    Xue, Fei
    Chen, Xu
    Liu, Hui
    ENGINEERING FRACTURE MECHANICS, 2018, 202 : 135 - 146
  • [3] Reasons for crack nucleation in welded joints of main gas-pipelines after a long-term operation
    Maruschak, P. O.
    Bishchak, R. T.
    Shlapak, L. S.
    Panin, S. V.
    INTERNATIONAL CONFERENCE ON MECHANICAL ENGINEERING, AUTOMATION AND CONTROL SYSTEMS 2016, 2017, 177
  • [4] Intercrystalline Corrosion Cracking of Welded Joints of the Austenitic Pipelines of Nuclear Power Plants
    B. T. Timofeev
    V. A. Fedorova
    A. A. Buchatskii
    Materials Science, 2004, 40 : 676 - 683
  • [5] Intercrystalline corrosion cracking of welded joints of the austenitic pipelines of nuclear power plants
    Timofeev, BT
    Fedorova, VA
    Buchatskii, AA
    MATERIALS SCIENCE, 2004, 40 (05) : 676 - 683
  • [6] The effect of mechanical inhomogeneity in microzones of welded joints on CTOD fracture toughness of nuclear thick-walled steel
    Tan, Long
    Li, Songyang
    Zhao, Liangyin
    Wang, Lulu
    Zhao, Xiuxiu
    NUCLEAR ENGINEERING AND TECHNOLOGY, 2023, 55 (11) : 4112 - 4119
  • [7] Effect of crack length on fracture toughness of welded joints with pronounced strength heterogeneity
    Stefane, Primoz
    Naib, Sameera
    Hertele, Stijn
    De Waele, Wim
    Gubeljak, Nenad
    ECF22 - LOADING AND ENVIRONMENTAL EFFECTS ON STRUCTURAL INTEGRITY, 2018, 13 : 1895 - 1900
  • [8] Evaluation of the fracture toughness of butt-welded joints using the boundary effect model
    Li, Yao
    Lu, Pengmin
    Wang, Binhua
    Hu, Xiaozhi
    Li, Datao
    Xiang, Qingyi
    ENGINEERING FRACTURE MECHANICS, 2022, 274
  • [9] Main deficiencies and corrective measures of nuclear power plants in ageing management for safe long term operation
    Krivanek, Robert
    Fiedler, Jan
    NUCLEAR ENGINEERING AND DESIGN, 2017, 323 : 78 - 83
  • [10] Effect of long-term operation on steels of main gas pipeline Reduction of static fracture toughness
    Maruschak, P. O.
    Panin, S. V.
    Chausov, M. G.
    Bishchak, R. T.
    Polyvana, U. V.
    JOURNAL OF NATURAL GAS SCIENCE AND ENGINEERING, 2017, 38 : 182 - 186