A comparative study on the dissolution and stability of beudantite and hidalgoite at pH 2-12 and 25-45 °C for the possible long-term simultaneous immobilization of arsenic and lead
被引:5
|作者:
Zhu, Yinian
[1
]
Wei, Wanying
[1
]
Tang, Shen
[2
]
Zhu, Zongqiang
[1
]
Yan, Qiming
[1
]
Zhang, Lihao
[2
]
Deng, Huan
[1
]
机构:
[1] Guilin Univ Technol, Coll Environm Sci & Engn, Guilin 541004, Peoples R China
[2] Guilin Univ Technol, Guangxi Key Lab Environm Pollut Control Theory &, Guilin 541004, Peoples R China
来源:
基金:
中国国家自然科学基金;
关键词:
Arsenate;
Lead;
Beudantite;
Hidalgoite;
Dissolution;
Stability;
THERMODYNAMIC PROPERTIES;
MOLECULAR-STRUCTURE;
CRYSTAL-STRUCTURE;
SEGNITITE SERIES;
AQUEOUS-SOLUTION;
ALUNITE FAMILY;
GOLD MINE;
JAROSITE;
NATROALUNITE;
BEHAVIOR;
D O I:
10.1016/j.chemosphere.2020.128386
中图分类号:
X [环境科学、安全科学];
学科分类号:
08 ;
0830 ;
摘要:
Beudantite and hidalgoite were synthesized and characterized to investigate their possible immobilization for arsenic and lead in acidic and oxidizing environments by a long-term dissolution. The synthetic beudantite [Pb-0.35(H3O)(0.40)Fe-3.09(AsO4)(0.37)(SO4)(1.63)(OH)(6.00)] was spherulitic pseudo-cubic crystals with nearly smooth surface. The synthetic hidalgoite [Pb-0.72(H3O)(2.71)Al-2.26(AsO4)(0.93)(SO4)(1.07)(OH)(6.00)] was well-formed pseudo-cubic, pseudo-cuboctahedral or pseudo-octahedral crystals. During the beudantite dissolution, the constituents were dissolved preferentially in the order of SO42- > AsO43- > Pb2+ > Fe3+ in the early 24 h and SO42- > AsO43- > Fe3+ > Pb2+ after 24 h; the dissolved concentrations exhibited a minimum of 0.0027 e0.0030 mg/L Pb and 0.0248-0.0250 mg/L As. During the hidalgoite dissolution, the constituents were dissolved preferentially in the order of Pb2+ > SO42- > AsO43- > Al3+ at initial pH < 4 or AsO43-,SO42- > Al3+ > Pb2+ at initial pH > 4; the dissolved concentrations showed a minimum of 0.0055 -0.0061 mg/L Pb and 0.0750-0.0810 mg/L As. From the data of the dissolution at initial pH 2 and 25 degrees C for 270-330 d, the ion-activity products [log_IAP] were estimated to be -94.18 +/- 0.04 for the beudantite and -73.82 +/- 0.11 for the hidalgoite, respectively. The concentrations of Pb and As released in the beudantite dissolution were always lower than in the hidalgoite dissolution and arsenate appeared to be much more soluble than Pb. Beudantite was more effective for the immobilization of As and Pb than hidalgoite. (C) 2020 Elsevier Ltd. All rights reserved.