On highly active partially oxidized platinum in carbon monoxide oxidation over supported platinum catalysts

被引:104
|
作者
Alayon, E. M. C. [1 ]
Singh, J. [1 ]
Nachtegaal, M. [2 ]
Harfouche, M. [2 ]
van Bokhoven, J. A. [1 ]
机构
[1] ETH, Inst Chem & Bioengn, CH-8093 Zurich, Switzerland
[2] Paul Scherrer Inst, Gen Energy Res Dept, Lab Energy & Mat Cycles, CH-5232 Villigen, Switzerland
基金
瑞士国家科学基金会;
关键词
In situ XAS; Carbon monoxide oxidation; Supported platinum catalysts; Active phase; X-RAY-ABSORPTION; CO OXIDATION; IN-SITU; RATE OSCILLATIONS; KINETIC OSCILLATIONS; XAFS SPECTROSCOPY; SURFACE COVERAGE; ISLAND FORMATION; PT/GAMMA-AL2O3; NANOPARTICLES;
D O I
10.1016/j.jcat.2009.02.010
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In situ X-ray absorption spectroscopy identified the role of oxidized platinum species in generating a high-activity state in the oxidation of carbon monoxide over Pt/Al2O3, Pt/TiO2 and Pt/SiO2. Two activity regimes were identified: low-activity at high carbon monoxide concentration and low temperature, and high activity at low carbon monoxide concentration and high temperature. The change between the two regimes occurred suddenly; there was ignition when going from low to high activity, and extinction from high to low activity. Ignition only occurred when the concentration of oxygen was higher than that of carbon monoxide. The catalyst was metallic and covered with carbon monoxide at low activity and partially oxidic at high activity. Carbon monoxide poisoned the catalyst at low activity. The partially oxidized platinum catalysts showed high activity. The partially oxidized catalyst had a lower oxygen coordination number and shorter Pt-O bond length as expected for bulk PtO2, suggesting that a strongly defected platinum oxide was formed with a possibly square planar coordination. The catalyst structure showed a dynamic behavior and the amount of oxide depended on the concentration of reactants in the gas phase. Smaller particles of Pt/Al2O3 reached high activity at lower temperature than the larger particles. Pt/TiO2 reached high activity at the lowest temperature while Pt/SiO2 required the highest temperature. Parallel with the temperature of ignition, Pt/SiO2 was the most oxidized while Pt/TiO2 was the least oxidized. (C) 2009 Elsevier Inc. All rights reserved.
引用
收藏
页码:228 / 238
页数:11
相关论文
共 50 条
  • [21] Carbon monoxide and methanol oxidation at platinum catalysts supported on ordered mesoporous carbon: the influence of functionalization of the support
    Salgado, J. R. C.
    Quintana, J. J.
    Calvillo, L.
    Lazaro, M. J.
    Cabot, P. L.
    Esparbe, I.
    Pastor, E.
    PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2008, 10 (45) : 6796 - 6806
  • [22] The promotion of carbon monoxide oxidation by hydrogen on supported platinum catalyst
    Salomons, S.
    Hayes, R. E.
    Votsmeier, M.
    APPLIED CATALYSIS A-GENERAL, 2009, 352 (1-2) : 27 - 34
  • [23] Platinum catalysts supported on silicas: effect of silica characteristics on their catalytic activity in carbon monoxide oxidation
    Mi-Young Kim
    Se Min Park
    Jung-Hyun Park
    Chae-Ho Shin
    Won-Jin Moon
    Nark-Eon Sung
    Gon Seo
    Reaction Kinetics, Mechanisms and Catalysis, 2011, 103 : 463 - 479
  • [24] Preferential oxidation of carbon monoxide with iron-promoted platinum catalysts supported on metal foams
    Chin, P
    Sun, XL
    Roberts, GW
    Spivey, JJ
    APPLIED CATALYSIS A-GENERAL, 2006, 302 (01) : 22 - 31
  • [25] Platinum catalysts supported on silicas: effect of silica characteristics on their catalytic activity in carbon monoxide oxidation
    Kim, Mi-Young
    Park, Se Min
    Park, Jung-Hyun
    Shin, Chae-Ho
    Moon, Won-Jin
    Sung, Nark-Eon
    Seo, Gon
    REACTION KINETICS MECHANISMS AND CATALYSIS, 2011, 103 (02) : 463 - 479
  • [26] OXIDATION OF CARBON-MONOXIDE ON PLATINUM ANTIMONY OXIDE CATALYSTS
    FUCHS, S
    LINTZ, HG
    DELMON, B
    APPLIED CATALYSIS A-GENERAL, 1993, 94 (01) : 85 - 90
  • [27] Selective Oxidation of Glycerol over Platinum-Based Catalysts Supported on Carbon Nanotubes
    Rodrigues, Elodie G.
    Pereira, Manuel F. R.
    Chen, Xiaowei
    Delgado, Juan J.
    Orfao, Jose J. M.
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2013, 52 (49) : 17390 - 17398
  • [28] Combination of carbon dioxide reforming and partial oxidation of methane over supported platinum catalysts
    Souza, MMVM
    Schmal, M
    APPLIED CATALYSIS A-GENERAL, 2003, 255 (01) : 83 - 92
  • [29] THE STABILITY AND OSCILLATIONS OF CARBON-MONOXIDE OXIDATION OVER PLATINUM SUPPORTED CATALYST - EFFECT OF BUTENE
    ALUKO, M
    CHANG, HC
    CHEMICAL ENGINEERING SCIENCE, 1985, 40 (12) : 2389 - 2391
  • [30] THE STABILITY AND OSCILLATIONS OF CARBON-MONOXIDE OXIDATION OVER PLATINUM SUPPORTED CATALYST - EFFECT OF BUTENE
    MUKESH, D
    CUTLIP, MC
    GOODMAN, M
    KENNEY, CN
    MORTON, W
    CHEMICAL ENGINEERING SCIENCE, 1982, 37 (12) : 1807 - 1810