Fatigue strength of crack-healed Si3N4/SiC composite ceramics

被引:65
|
作者
Ando, K
Chu, MC
Yao, F
Sato, S
机构
[1] Yokohama Natl Univ, Dept Energy & Safety Engn, Yokohama, Kanagawa 240, Japan
[2] NHK Spring, Kanazawa Ku, Yokohama, Kanagawa, Japan
关键词
Si3N4/SiC ceramics; crack healing; crack-healed zone; bending strength; recovery of strength; cyclic fatigue strength; static fatigue strength; crack initiation site;
D O I
10.1046/j.1460-2695.1999.00210.x
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Si3N4/SiC composite ceramics were sintered and subjected to three-point bending on specimens made according to the appropriate JIS standard. A semi-circular surface crack of 110 mu m in diameter was made on each specimen. By using three kinds of specimen (smooth, cracked and crack healed), crack-healing behaviour, cyclic and static fatigue strengths were determined systematically at room temperature and 1000 degrees C. The main conclusions are as follows: (i) Si3N4/SiC composite ceramics have the ability to heal after cracking; (ii) crack-healed specimens showed similar cyclic and static fatigue strengths as smooth specimens, this being caused by crack healing; (iii) crack-healed zones had a sufficient fatigue strength and most fractures occurred outside the pre-cracked zone in those crack-healed specimens.
引用
收藏
页码:897 / 903
页数:7
相关论文
共 50 条
  • [21] High temperature fatigue strength of crack-healed Al2O3 toughened by SiC whiskers
    Ando, K
    Lee, SK
    Takahashi, K
    Yokouchi, M
    SMART MATERIALS III, 2005, 5648 : 29 - 36
  • [22] Crack-healing behavior and bending strength of Si3N4/SiC composite ceramics by SiO2 colloidal
    Nam, Ki Woo
    Kim, Mi Kyung
    Park, Sung Won
    Ahn, Seok Hwan
    Kim, Jong Soon
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 471 (1-2): : 102 - 105
  • [23] STRENGTH DEGRADATION BY SUBCRITICAL CRACK GROWTH IN SI3N4 AND SIC
    LARSEN, DC
    WALTHER, GC
    BORTZ, SA
    RUH, R
    AMERICAN CERAMIC SOCIETY BULLETIN, 1979, 58 (03): : 350 - 350
  • [24] High tememperature fatigue strength of crack-healed Al2O3/SiC-whiskers
    Lee, SK
    Nakao, W
    Takahashi, K
    Ando, K
    Yokouchi, M
    Suenaga, H
    HIGH TEMPERATURE CERAMIC MATRIX COMPOSITES 5, 2005, : 335 - 340
  • [25] Crack-healing behavior of Si3N4/SiC ceramics under cyclic stress and resultant fatigue strength at the healing temperature
    Ando, K
    Takahashi, K
    Nakayama, S
    Saito, S
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (09) : 2268 - 2272
  • [26] Crack-healing behavior of Si3N4/SiC ceramics under stress and fatigue strength at the temperature of healing (1000°C)
    Ando, K
    Houjyou, K
    Chu, MC
    Takeshita, S
    Takahashi, K
    Sakamoto, S
    Sato, S
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (08) : 1339 - 1346
  • [27] Crack surface interaction in Si3N4 ceramics reinforced by SiC whisker
    Kanayama, M
    Kamata, I
    Shiono, T
    Nishida, T
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 2002, 110 (01) : 32 - 37
  • [28] Fatigue crack propagation behavior of Si3N4 ceramics in corrosive environments
    Okabe, T
    Katayama, G
    Kido, M
    Udaka, N
    MATERIALS SCIENCE RESEARCH INTERNATIONAL, 1996, 2 (03): : 187 - 192
  • [29] Effect of the specimen size on strength of Si3N4 + SiC composite
    Hegedusova, Lucia
    Kasiarova, Monika
    Csehova, Erika
    Dusza, Jan
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2010, 30 (04) : 1059 - 1065
  • [30] THERMAL FATIGUE OF SIC AND SI3N4
    DOHERTY, JE
    AMMANN, CL
    AMERICAN CERAMIC SOCIETY BULLETIN, 1974, 53 (08): : 621 - 621