Compressive Properties and Energy Absorption Characteristics of Extruded Mg-Al-Ca-Mn Alloy at Various High Strain Rates

被引:11
|
作者
Xiang, Chongchen [1 ]
Xiao, Zhendong [1 ]
Ding, Hanlin [1 ]
Wang, Zijian [1 ]
机构
[1] Soochow Univ, Shagang Sch Iron & Steel, 8 Jixue Rd, Suzhou 215137, Peoples R China
关键词
Mg-Al-Ca-Mn alloy; rapid hot extrusion; high strain rate; specific energy absorption;
D O I
10.3390/ma14010087
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This paper is focused on the mechanical properties and the energy absorption characteristics of the extruded Mg-Al-Ca-Mn alloy in different compression directions under high strain rate compression. Compressive characterization of the alloy was conducted from the high strain rate (HSR) test by using a Split Hopkinson Pressure Bar (SHPB). Results show that the investigated alloy exhibits a strong strain rate sensitivity. With the rise of strain rate, the compressive strength is increased significantly, and the deformation ability also improves. When compressed along the extrusion direction, as the strain rate increases, the total absorbed energy E, the crush force efficiency (CFE), and the specific energy absorption SEA of Mg-Al-Ca-Mn alloy are all greatly improved as compared with those obtained along other compression directions.
引用
收藏
页码:1 / 19
页数:19
相关论文
共 50 条
  • [21] Development of a magnesium alloy with good casting characteristics on the basis of Mg-Al-Ca-Mn system, having Mg-Al2Ca structure
    Koltygin, A. V.
    Bazhenov, V. E.
    Belova, E. A.
    Nikitina, A. A.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2013, 1 (03) : 224 - 229
  • [22] Investigation of the crystallographic structure and orientations of the Al2Ca phase in a Mg-Al-Ca-Mn alloy
    Liu, Yu
    Wang, Nana
    Wang, Jinwei
    Ma, Baichang
    Zhao, Dongqing
    MATERIALS CHARACTERIZATION, 2018, 142 : 377 - 382
  • [23] Elucidating dynamic precipitation and yield strength of rolled Mg-Al-Ca-Mn alloy
    Li, Jiehua
    Zhou, Xuyang
    Su, Jing
    Breitbach, Benjamin
    Chwalek, Marta Lipinska
    Wang, Huiyuan
    Dehm, Gerhard
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 856
  • [24] Accelerated solid solution and aging induced by electropulsing in Mg-Al-Ca-Mn alloy
    Hou, Qingyu
    Xu, Xiaofeng
    Zhao, Yang
    Yan, Xudong
    Zhou, Yachong
    Wang, Jinguo
    Wei, Lai
    Yu, Yongqiang
    MATERIALS LETTERS, 2022, 318
  • [25] Dynamic microstructure evolution and mechanical properties of dilute Mg-Al-Ca-Mn alloy during hot rolling
    Xu, Shiwei
    Zhu, Congcong
    Lin, Zhanhong
    Jin, Chen
    Kamado, S.
    Oh-ishi, K.
    Qin, Yun
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 129 : 1 - 14
  • [26] Ultrahigh strength Mg-Al-Ca-Mn extrusion alloys with various aluminum contents
    Li, Z. T.
    Qiao, X. G.
    Xu, C.
    Kamado, S.
    Zheng, M. Y.
    Luo, A. A.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 792 : 130 - 141
  • [27] Potential of multi-pass ECAP on improving the mechanical properties of a high-calcium-content Mg-Al-Ca-Mn alloy
    Huang, He
    Liu, Huan
    Wang, Ce
    Sun, Jiapeng
    Bai, Jing
    Xue, Feng
    Jiang, Jinghua
    Ma, Aibin
    JOURNAL OF MAGNESIUM AND ALLOYS, 2019, 7 (04) : 617 - 627
  • [28] Dynamic microstructure evolution and mechanical properties of dilute Mg-Al-Ca-Mn alloy during hot rolling
    Shiwei Xu
    Congcong Zhu
    Zhanhong Lin
    Chen Jin
    S.Kamado
    K.Oh-ishi
    Yun Qin
    Journal of Materials Science & Technology, 2022, 129 (34) : 1 - 14
  • [29] Effect of Ca/Al Ratio on Microstructure and Mechanical Properties of Slow Extrusion High-Strength Mg-Al-Ca-Mn Alloys
    Shilei Wang
    Kaibo Nie
    An Yang
    Kunkun Deng
    Journal of Materials Engineering and Performance, 2023, 32 : 3129 - 3141
  • [30] Effect of Ca/Al Ratio on Microstructure and Mechanical Properties of Slow Extrusion High-Strength Mg-Al-Ca-Mn Alloys
    Wang, Shilei
    Nie, Kaibo
    Yang, An
    Deng, Kunkun
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (07) : 3129 - 3141