Sulfide stress cracking susceptibility of welded X-60 and X-65 pipeline steels

被引:9
|
作者
Natividad, C.
Salazar, M.
Contreras, A.
Albiter, A.
Perez, R.
Gonzalez-Rodriguez, J. G.
机构
[1] UAEM, CIICAP, Cuernavaca 6225, Morelos, Mexico
[2] Univ Nacl Autonoma Mexico, Fac Quim Circuito Interior, CU, Mexico City 04510, DF, Mexico
[3] Inst Mexicano Petr, Programa Invest & Desarrollo Ductos, Mexico City 07730, DF, Mexico
关键词
hydrogen embrittlement; sulfide stress corrosion cracking; X-60 and X-65 steel weldments;
D O I
10.5006/1.3278275
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The susceptibility of API X-60 and X-65 longitudinal weld beads to sulfide stress cracking (SSC) has been evaluated using slow strain rate tests (SSRT) in the NACE solution saturated with hydrogen sulfide (H2S). The tests were supplemented by potentiodynamic polarization curves and hydrogen permeation measurements. The weld beads were produced using the submerged arc welding (SAM) process. Three different temperatures were used: room temperature (25 degrees C), 37 degrees C, and 50 degrees C. The corrosion rate, taken as the corrosion current density, I-corr, the amount of hydrogen uptake for the weldments, C-0, and the SSC susceptibility increased with an increase in the temperature from 25 degrees C to 50 degrees C. Although anodic dissolution seems to play an important role in the cracking mechanism, the most likely mechanism for the cracking susceptibility of X-60 and X-65 weldments in H2S solutions seems to be hydrogen embrittlement.
引用
收藏
页码:375 / 382
页数:8
相关论文
共 50 条
  • [41] Effect of passivity of the oxide film on low-pH stress corrosion cracking of API 5L X-65 pipeline steel in bicarbonate solution
    Park, JJ
    Pyun, SI
    Na, KH
    Lee, SM
    Kho, YT
    CORROSION, 2002, 58 (04) : 329 - 336
  • [42] Investigation of Hydrogen-induced Cracking Susceptibility of X90 Pipeline Steel Welded Joints
    Yan C.
    Zhou Q.
    Zhang H.
    Jiang X.
    Yi S.
    Zhang K.
    Jixie Gongcheng Xuebao/Journal of Mechanical Engineering, 2023, 59 (24): : 83 - 94
  • [43] Cyclic crack growth rates of X-60 pipeline steel in a neutral dilute solution
    Ahmed, TM
    Lambert, SB
    Sutherby, R
    Plumtree, A
    CORROSION, 1997, 53 (07) : 581 - 590
  • [44] Non-destructive evaluation of aging in welded pipeline X60 and X65 by thermoelectric power means
    Conejo, V.
    Hernandez, L.
    Carreon, H.
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2024, 207
  • [45] Corrosion of X-65 Pipeline Steel Under a Simulated Cathodic Protection Shielding Coating Disbondment
    Eslami, A.
    Kania, R.
    Worthingham, B.
    Boven, G. V.
    Eadie, R.
    Chen, W.
    CORROSION, 2013, 69 (11) : 1103 - 1110
  • [46] Cold cracking susceptibility of X100 pipeline steel
    严春妍
    姜心怡
    元媛
    纪秀林
    张可召
    China Welding, 2019, 28 (03) : 25 - 33
  • [47] Effect of Zr-Ti deoxidisation on the hydrogen-induced cracking of X65 pipeline steels
    Du, Y.
    Wu, K. M.
    Cheng, L.
    Li, Y.
    Isayev, O.
    Hress, O.
    MATERIALS SCIENCE AND TECHNOLOGY, 2016, 32 (07) : 728 - 735
  • [48] Stress Corrosion Cracking of Welded API X70 Pipeline Steel in Simulated Underground Water
    Liu, Z. Y.
    Du, C. W.
    Li, C.
    Wang, F. M.
    Li, X. G.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2013, 22 (09) : 2550 - 2556
  • [49] Stress Corrosion Cracking of Welded API X70 Pipeline Steel in Simulated Underground Water
    Z. Y. Liu
    C. W. Du
    C. Li
    F. M. Wang
    X. G. Li
    Journal of Materials Engineering and Performance, 2013, 22 : 2550 - 2556
  • [50] Mechanical and microstructural effects on the stress corrosion cracking of weld beads of X-52 and X-70 pipeline steels
    Contreras, A
    Albiter, A
    Angeles-Chavez, C
    Pérez, R
    REVISTA MEXICANA DE FISICA, 2004, 50 : 49 - 53