The influence of aging on the microstructure and creep behaviour of a γ-Ti-48%A1-2%W intermetallic

被引:39
|
作者
Seo, DY
Beddoes, J
Zhao, L [1 ]
Botton, GA
机构
[1] Natl Res Council Canada, Inst Aerosp Res, Struct Mat & Prop Lab, Ottawa, ON, Canada
[2] Carleton Univ, Dept Aerosp & Mech Engn, Ottawa, ON K1S 5B6, Canada
[3] Canada Ctr Mineral & Energy Technol, Mat Technol Labs, Ottawa, ON, Canada
基金
加拿大自然科学与工程研究理事会;
关键词
TiAl plus W alloy; aging; beta o precipitates; creep; W diffusion; alpha(2) decomposition; lamellar;
D O I
10.1016/S0921-5093(01)01630-6
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The results of aging at 950 C for up to 192 h on the microstructure and creep properties of a fully lamellar Ti-48at.% Al-2at.% W is presented. Aging times as short as 5 h result in acicular precipitates of W rich beta(o) along lamellar interfaces, with the beta(o) size increasing with aging time. The beta(o) precipitates nucleate and grow in the alpha(2) lamellar by diffusion of W. Concurrently, the alpha(2) decomposes into discontinuous lamellar. Creep tests at 760 degreesC and 276 MPa indicate that the precipitation of beta(o) along interfaces substantially reduces the primary creep strain, primarily due to the influence of beta(o) on interface dislocation emission and motion. However, aging reduces the extent of tertiary creep and slightly reduces creep life, due to larger and more numerous intergranular beta(o) particles, which serve to initiate intergranular void formation during tertiary creep. The results are discussed in terms of the effect of W solute and beta(o) precipitates on the alpha(2) lamellar stability and are used to infer the influence of microstructural features on the various creep resistance parameters. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:810 / 820
页数:11
相关论文
共 50 条
  • [31] Flow softening behavior during high temperature deformation of Ti-48Al-2W intermetallic compound
    Hee Y. Kim
    Soon H. Hong
    Metals and Materials, 1998, 4 : 765 - 770
  • [32] Flow softening behavior during high temperature deformation of Ti-48Al-2W intermetallic compound
    Kim, HY
    Hong, SH
    METALS AND MATERIALS-KOREA, 1998, 4 (04): : 765 - 770
  • [33] Flow Softening Behavior during High Temperature Deformation of Ti-48Al-2W Intermetallic Compound
    Kim, Hee Y.
    Hong, Soon H.
    Metals and Materials International, 1998, 4 (04): : 765 - 770
  • [34] CREEP DEFORMATION IN NEAR-GAMMA TIAL .2. INFLUENCE OF CARBON ON CREEP DEFORMATION IN TI-48AL-1V-0.3C
    WORTH, BD
    JONES, JW
    ALLISON, JE
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1995, 26 (11): : 2961 - 2972
  • [35] Microstructure and wear resistance of a laser surface alloyed γ-TiAl intermetallic alloy Ti-48Al-2Cr-2Nb
    Yu, Ligen
    Li, Xiaoxuan
    Wang, Huaming
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2000, 29 (05): : 328 - 331
  • [36] Microstructure and wear resistance of a laser surface alloyed γ-TiAl intermetallic alloy Ti-48Al-2Cr-2Nb
    Yu, LG
    Li, XX
    Wang, HM
    RARE METAL MATERIALS AND ENGINEERING, 2000, 29 (05) : 328 - 331
  • [37] High temperature internal friction in a Ti-46Al-1Mo-0.2Si intermetallic, comparison with creep behaviour
    Castillo-Rodriguez, M.
    No, M. L.
    Jimenez, J. A.
    Ruano, O. A.
    Juan, J. San
    ACTA MATERIALIA, 2016, 103 : 46 - 56
  • [38] CREEP DEFORMATION IN NEAR-GAMMA TIAL .1. THE INFLUENCE OF MICROSTRUCTURE ON CREEP DEFORMATION IN TI-49AL-1V
    WORTH, BD
    JONES, JW
    ALLISON, JE
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1995, 26 (11): : 2947 - 2959
  • [39] Phase identification and effect of W on the microstructure and micro-hardness of Ti2AlNb-based intermetallic alloys
    Yang, Seung Jin
    Nam, Soo Woo
    Hagiwara, Masuo
    1600, Elsevier Ltd (350): : 1 - 2
  • [40] Phase identification and effect of W on the microstructure and micro-hardness of Ti2AlNb-based intermetallic alloys
    Yang, SJ
    Nam, SW
    Hagiwara, M
    JOURNAL OF ALLOYS AND COMPOUNDS, 2003, 350 (1-2) : 280 - 287