Fracture analysis of monolithic CAD-CAM crowns

被引:23
|
作者
Kashkari, Afnan [1 ]
Yilmaz, Burak [2 ]
Brantley, William A. [2 ]
Schricker, Scott R. [2 ]
Johnston, William M. [2 ]
机构
[1] Johns Hopkins Aramco Healthcare, Restorat & Esthet Dent, Dhahran, Saudi Arabia
[2] Ohio State Univ, Coll Dent, Div Restorat & Prosthet Dent, Columbus, OH 43210 USA
关键词
CAD-CAM; ceramic; fracture; lithium disilicate; lithium silicate; zirconia; ALL-CERAMIC CROWNS; LITHIUM-DISILICATE; MECHANICAL-PROPERTIES; CURING MODE; BITE FORCE; FATIGUE; CONVERSION; POLYMERIZATION; SHRINKAGE; STRENGTH;
D O I
10.1111/jerd.12462
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose The aim of this study was to compare the integrity of zirconia, lithium disilicate, and zirconia-reinforced lithium silicate CAD-CAM crowns after being subjected to cyclic loading and then subjected to static loading until fracture. Material and Methods Zirconia (Zirkonzahn), lithium disilicate (LDS, Ivoclar Vivadent AG), and zirconia-reinforced lithium silicate glass ceramic (ZLS) (Vita Suprinity, Vita Zahnfabrik) monolithic crowns were milled (n = 6). The crowns were bonded using composite resin cements and subjected to cyclic loading under wet conditions. Three specimens from each group were loaded for 10 000 cycles, and the other three specimens were loaded for 50 000 cycles with 250 N. Specimens were subjected to loading until fracture. Load-to-fracture values were analyzed with 2-way (ANOVA) and Tukey-Kramer post hoc test (alpha = 0.05). Specimens from each group were examined using an SEM. Results Mean load-to-fracture values among materials were significantly different from each other (P < 0.05). No significant effect of the number of cycles was found on the load-to-fracture values of crowns (P > 0.05). Conclusion Load-to-fracture values of zirconia were higher than those of LDS, which were higher than those of ZLS. The number of fatigue loading cycles did not affect the load-to-fracture of the tested crowns for a given material. Clinical Significance More research needs to be conducted before considering the routine use of ZLS for molars in patients with high risk of parafunctional habits.
引用
收藏
页码:346 / 352
页数:7
相关论文
共 50 条
  • [41] Design concept for preventing aspiration or ingestion of CAD-CAM crowns: A dental technique
    Lee, Ju-Hyoung
    JOURNAL OF PROSTHETIC DENTISTRY, 2020, 123 (02): : 220 - 222
  • [42] THE BASIS FOR CAD-CAM
    CHASEN, SH
    PROCEEDINGS ANNUAL RELIABILITY AND MAINTAINABILITY SYMPOSIUM, 1981, (NSYM): : 63 - 68
  • [43] Clinical performance of CAD-CAM crowns provided by predoctoral students at the University of Toronto
    Aziz, Ahmed M.
    El-Mowafy, Omar
    Tenenbaum, Howard C.
    Lawrence, Herenia P.
    JOURNAL OF PROSTHETIC DENTISTRY, 2022, 127 (05): : 729 - 736
  • [44] CAD-CAM IN DENTISTRY
    DURET, F
    BLOUIN, JL
    DURET, B
    JOURNAL OF THE AMERICAN DENTAL ASSOCIATION, 1988, 117 (06): : 715 - 720
  • [45] Fatigue resistance of monolithic CAD/CAM ceramic crowns on human premolars
    Homaei, Ehsan
    Farhangdoost, Khalil
    Pow, Edmond Ho Nang
    Matinlinna, Jukka Pekka
    Akbari, Majid
    Tsoi, James Kit-Hon
    CERAMICS INTERNATIONAL, 2016, 42 (14) : 15709 - 15717
  • [46] The aesthetics of all-ceramic veneered and monolithic CAD/CAM crowns
    Herrguth, M
    Wichmann, M
    Reich, S
    JOURNAL OF ORAL REHABILITATION, 2005, 32 (10) : 747 - 752
  • [47] CAD-CAM FOR PUMPS
    NELIK, LA
    DSOUZA, P
    OZSOY, T
    MECHANICAL ENGINEERING, 1987, 109 (08) : 46 - 49
  • [48] A VIEW OF CAD-CAM
    BEZIER, PE
    COMPUTER-AIDED DESIGN, 1981, 13 (04) : 207 - 209
  • [49] CAD-CAM SERVICES
    不详
    COMPUTER-AIDED ENGINEERING, 1995, 14 (12): : 61 - &
  • [50] REINVENTING CAD-CAM
    FOUNDYLLER, C
    COMPUTER-AIDED ENGINEERING, 1994, 13 (02): : 58 - 58