Steam Oxidation Evaluation of Fe-Cr Alloys for Accident Tolerant Nuclear Fuel Cladding

被引:17
|
作者
Pint, B. A. [1 ]
Unocic, K. A. [1 ]
机构
[1] Oak Ridge Natl Lab, POB 2008, Oak Ridge, TN 37831 USA
来源
OXIDATION OF METALS | 2017年 / 87卷 / 3-4期
关键词
Nuclear energy; Fuel cladding; Steam oxidation; FeCr alloys; HIGH-TEMPERATURE OXIDATION; WATER-VAPOR; CANDIDATE MATERIALS; STAINLESS-STEELS; BEHAVIOR; ENVIRONMENTS; SEGREGATION; SYSTEM; OXYGEN; METAL;
D O I
10.1007/s11085-017-9754-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
New nuclear fuel cladding materials are being evaluated that can withstand steam environments ae1200 A degrees C for short (ae4 h) periods in case of a beyond design basis accident. This study focused on commercial and model Fe-Cr alloys, where there is considerable experience in fabricating and joining. Exposures in 1 bar steam and air for 4 h at 800-1300 A degrees C showed that the commercial Fe-Cr alloys were very sensitive to composition and only Fe-25.8%Cr-1%Mo formed a protective chromia scale at 1200 and 1300 A degrees C in steam. A model Fe-22.5%Cr + Mn,Si,Y alloy also formed a protective scale at 1200 A degrees C in steam. Analytical transmission electron microscopy of the reaction products revealed that (1) nominally equiaxed Cr2O3 formed at 1000-1200 A degrees C; (2) at 1000 A degrees C, there was a Mn inner and outer layer but at 1100 and 1200 A degrees C only an outer layer was observed; (3) an amorphous SiO2 inner layer was observed at 1000 and 1100 A degrees C, but the SiO2 was crystalline on the 22.5%Cr model alloy at 1200 A degrees C, which was confirmed by electron and X-ray diffraction; and (4) Fe was found throughout the Cr2O3 formed on alloys without Mn at 1200 A degrees C in steam and air, Fe-rich oxide near the gas interface and Fe-rich metal precipitates near the metal-oxide interface. A few Fe-rich precipitates were detected in oxides formed at 1100 A degrees C and none at 1000 A degrees C. The incorporation of Fe and crystallization of SiO2 at 1200 A degrees C may be detrimental to the formation of a protective chromia scale in steam at ae1200 A degrees C for this application and explain why such high Cr contents are needed for protective behavior.
引用
收藏
页码:515 / 526
页数:12
相关论文
共 50 条
  • [41] Accident-Tolerant Barriers for Fuel Road Cladding of CANDU Nuclear Reactor
    Diniasi, Diana
    Fulger, Manuela
    Butoi, Bogdan
    Dinca, Paul Pavel
    Golgovici, Florentina
    COATINGS, 2023, 13 (10)
  • [42] THEORETICAL ANALYSIS OF ALLOY OXIDATION WITH REFERENCE TO FE-CR ALLOYS
    WULF, GL
    MCGIRR, MB
    WALLWORK, GR
    CORROSION SCIENCE, 1969, 9 (10) : 739 - &
  • [43] Morphology of Fe-Cr alloys
    Ustinovshikov, Y
    Pushkarev, B
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 241 (1-2): : 159 - 168
  • [44] Material Selection for Accident Tolerant Fuel Cladding
    Pint, B. A.
    Terrani, K. A.
    Yamamoto, Y.
    Snead, L. L.
    METALLURGICAL AND MATERIALS TRANSACTIONS E-MATERIALS FOR ENERGY SYSTEMS, 2015, 2 (03): : 190 - 196
  • [45] TRANSFORMATIONS IN FE-CR ALLOYS
    WALLBRIDGE, JM
    PARR, JG
    JOURNAL OF THE IRON AND STEEL INSTITUTE, 1966, 204 : 119 - +
  • [46] Morphology of Fe-Cr alloys
    Physical-Technical Inst, Izhevsk, Russia
    Mater Sci Eng A Struct Mater Prop Microstruct Process, 1-2 (159-168):
  • [47] Current progress of Cr-coated zirconium alloy cladding for accident tolerant fuel
    Duan Z.
    Chen P.
    Zhou Y.
    Gao S.
    Jiao Y.
    Yin C.
    He L.
    He Jishu/Nuclear Techniques, 2022, 45 (03):
  • [48] Measurement of local mechanical properties for Cr-coated accident tolerant fuel cladding
    Hong, JongDae
    Ahn, Daehyeok
    Jang, Dongchan
    Oh, Hongryul
    Kim, JaeYong
    Kim, Hyochan
    Sevecek, Martin
    JOURNAL OF NUCLEAR MATERIALS, 2023, 579
  • [49] Accident Tolerant Nuclear Fuels and Cladding Materials
    Indrajit Charit
    JOM, 2018, 70 : 173 - 175
  • [50] Accident Tolerant Nuclear Fuels and Cladding Materials
    Charit, Indrajit
    JOM, 2018, 70 (02) : 173 - 175