Influence of Hydrophobic Polystyrene Blocks on the Rehydration of Polystyrene-block-poly(methoxy diethylene glycol acrylate)-block-polystyrene Films Investigated by in Situ Neutron Reflectivity

被引:23
|
作者
Zhong, Qi [1 ,2 ,3 ]
Metwalli, Ezzeldin [3 ]
Rawolle, Monika [3 ]
Kaune, Gunar [4 ]
Bivigou-Koumba, Achille M. [5 ]
Laschewsky, Andre [5 ,7 ]
Papadakis, Christine M. [3 ]
Cubitt, Robert [6 ]
Wang, Jiping [1 ,2 ]
Mueller-Buschbaum, Peter [3 ]
机构
[1] Zhejiang Sci Tech Univ, Key Lab Adv Textile Mat & Mfg Technol, Minist Educ, Hangzhou 310018, Zhejiang, Peoples R China
[2] Zhejiang Sci Tech Univ, Engn Res Ctr Ecodyeing & Finishing Text, Minist Educ, Natl Base Int Sci & Technol Cooperat Text & Consu, Hangzhou 310018, Peoples R China
[3] Tech Univ Munich, Lehrstuhl Funkt Mat Fachgebiet Phys Weicher Mat, Phys Dept, D-85748 Garching, Germany
[4] Univ Halle Wittenberg, D-06120 Halle, Germany
[5] Univ Potsdam, Inst Chem, D-14476 Potsdam, Germany
[6] Inst Laue Langevin, F-38000 Grenoble, France
[7] Fraunhofer Inst Appl Polymer Res IAP, D-14469 Potsdam, Germany
基金
中国国家自然科学基金;
关键词
CORE-SHELL MICROGELS; PHASE-TRANSITION; N-ISOPROPYLACRYLAMIDE; SWELLING BEHAVIOR; PNIPAM MICROGELS; POLY(N-ISOPROPYLACRYLAMIDE); TEMPERATURE; WATER; COPOLYMERS; ACRYLATE);
D O I
10.1021/acs.macromol.5b02279
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The rehydration of thermoresponsive polystyrene-block-poly(methoxy diethylene glycol acrylate)-block-polystyrene (PS-b-PMDEGA-b-PS) films forming a lamellar microphase-separated structure is investigated by in situ neutron reflectivity in a D2O vapor atmosphere. The rehydration of collapsed PS-b-PMDEGA-b-PS films is realized by a temperature change from 45 to 23 degrees C and comprises (1) condensation and absorption of D2O, (2) evaporation of D2O, and (3) reswelling of the film due to internal rearrangement. The hydrophobic PS layers hinder the absorption of condensed D2O, and a redistribution of embedded D2O between the hydrophobic PS layers and the hydrophilic PMDEGA layers is observed. In contrast, the rehydration of semiswollen PS-b-PMDEGA-b-PS films (temperature change from 35 to 23 degrees C) shows two prominent differences: A thicker D2O layer condenses on the surface, causing a more enhanced evaporation of D2O. The rehydrated films differ in film thickness and volume fraction of D2O, which is due to the different thermal protocols, although the final temperature is identical.
引用
收藏
页码:317 / 326
页数:10
相关论文
共 50 条
  • [41] Changes in morphology and mechanical properties with composition for microphase-separated polystyrene-block-poly(ethylene-co-but-1-ene)-block-polystyrene triblock copolymers
    Umeda, H
    Sakurai, S
    Kitagawa, Y
    Suda, Y
    Masamoto, J
    Nomura, S
    KOBUNSHI RONBUNSHU, 1997, 54 (04) : 236 - 243
  • [42] Interfacial behavior of polystyrene-block-poly(t-butyl acrylate) star copolymers
    Bernard, Sophie
    Denoncourt, Kristina M.
    Joncheray, Thomas J.
    Kim, Young H.
    Matmour, Rachid
    El-Khouri, Rita J.
    Gnanou, Yves
    Ford, Warren T.
    Duran, Randolph S.
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2006, 231
  • [43] Morphological evoluation of poly(solketal methacrylate)-block-polystyrene copolymers in thin films
    Yu, Duk Man
    Smith, Darren
    Kim, Hyeyoung
    Mapas, Jose
    Rzayev, Javid
    Russell, Thomas
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2019, 258
  • [44] Kinetics and mechanism, of morphological transition from Lamella to cylinder microdomain in polystyrene-block-poly(ethylene-co-but-1-ene)block-polystyrene triblock copolymer
    Jeong, U
    Lee, HH
    Yang, LH
    Kim, JK
    Okamoto, S
    Aida, S
    Sakurai, S
    MACROMOLECULES, 2003, 36 (05) : 1685 - 1693
  • [45] Sulfonated polystyrene-block-poly(ethylene-ran-butylene)-block-polystyrene/sulfonated poly(ether sulfone) and hexagonal boron nitride electrolyte membrane for fuel cell applications
    Kulasekaran, Poonkuzhali
    Moorthy, Siva
    Deivanayagam, Paradesi
    Sekar, Karthikeyan
    Pushparaj, Hemalatha
    SOFT MATTER, 2022, 18 (47) : 8952 - 8960
  • [46] Morphology and surface properties of polystyrene-block-poly(N-isopropylacrylamide) films
    Dizajyekan, Elham Sabzi
    Nasiri, Morteza
    Abbasi, Farhang
    IRANIAN POLYMER JOURNAL, 2024, 33 (11) : 1637 - 1649
  • [47] Temperature-Dependent Order-to-Order Transition of Polystyrene-block-poly(ethylene-co-butylene)-block-polystyrene Triblock Copolymer under Multilayered Confinement
    Tan, Xiao
    Li, Jiang
    Guo, Shaoyun
    MACROMOLECULES, 2018, 51 (05) : 2099 - 2109
  • [48] Upper Critical Solution Temperature Switchable Micelles Based on Polystyrene-block-poly(methyl acrylate) Block Copolymers
    Can, Aydin
    Hoeppener, Stephanie
    Guillet, Pierre
    Gohy, Jean-Francois
    Hoogenboom, Richard
    Schubert, Ulrich S.
    JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 2011, 49 (17) : 3681 - 3687
  • [49] Efficiency, operational stability and biofouling of novel sulfomethylated polystyrene-block-poly(ethylene-ran-butylene)-block-polystyrene cation exchange membrane in microbial fuel cells
    Kook, Laszlo
    Zitka, Jan
    Szakacs, Szabolcs
    Rozsenberszki, Tamas
    Otmar, Miroslav
    Nemestothy, Nandor
    Belafi-Bako, Katalin
    Bakonyi, Peter
    BIORESOURCE TECHNOLOGY, 2021, 333
  • [50] Constructing Flexible Proton Exchange Membranes Through Alternate Deposition of Kevlar Nanofibers and Polydopamine Coating Polystyrene-Block-Poly(ethylene-ran-butylene)-Block-Polystyrene
    Song, Di
    Liu, Ke
    Zuo, Tingting
    Wei, Xiaoqing
    Hu, Shu
    Che, Quantong
    FIBERS AND POLYMERS, 2023, 24 (04) : 1183 - 1194