The oxidation of a Co-15 wt% yttrium alloy in 1 atm O2 at 600-800°C

被引:10
|
作者
Niu, Y
Li, YS
Gesmundo, F
Viani, F
机构
[1] Univ Genoa, Dipartimento Ingn Chim & Proc, I-16129 Genoa, Italy
[2] Inst Corros & Protect Met, State Key Lab Corros, Shenyang 10015, Peoples R China
基金
中国国家自然科学基金;
关键词
rare-earth intermetallics; oxidation; corrosion;
D O I
10.1016/S0966-9795(99)00106-5
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The oxidation of a cobalt-based alloy containing 15 wt% yttrium (Y) as well as of pure yttrium has been studied in I arm of pure oxygen at 600-800 degrees C. The alloy always corrodes faster than pure cobalt and follows the parabolic rate law only approximately, forming an external scale of cobalt oxide which in its inner section contains particles of yttrium oxide. Beneath the external scales, a region of internal oxidation of yttrium having a depth much larger than predicted using the known solubility and diffusivity of oxygen in pure cobalt is also present. This anomalous depth is attributed to enhanced oxygen diffusion in the alloy along preferential paths associated with the localized internal oxidation of yttrium. No yttrium depletion is observed in the alloy beneath the front of internal oxidation. The scaling behavior of this alloy is interpreted by taking into account the limited solubility of yttrium in cobalt and the presence of the intermetallic compound Co-17 Y-2. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:293 / 298
页数:6
相关论文
共 50 条
  • [31] The sulfidation of Fe-15wt%Y and Fe-30wt%Y in H-2-H2S mixtures at 600-800 degrees C
    Niu, Y
    Gesmundo, F
    Castello, P
    Yan, R
    Viani, F
    Wu, W
    CORROSION SCIENCE, 1997, 39 (06) : 1093 - 1108
  • [32] Scaling behavior of four ternary Co-20Ni-based alloys containing 3/5 wt% Al or 8/15 wt% Cr in 1 Atm O2 at 800-900 °C
    Lv, Y. L.
    Ren, Y. J.
    Wang, W.
    Zhou, L. B.
    Chen, J.
    Huang, J.
    Tao, M. S.
    Niu, Y.
    CORROSION SCIENCE, 2022, 199
  • [33] Oxidation of powder metallurgical Ag-Cr alloys in 1 atm O2 at 700-800°C
    Song, JX
    Wu, WT
    Niu, Y
    Wang, CL
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2000, 19 (02) : 117 - 125
  • [34] An Anomalous Internal Oxidation of Dilute Cu-Ni Alloys at 800 °C under 1 atm O2
    Lu, L. Y.
    Liu, L. L.
    Wang, S.
    Niu, Y.
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2012, 31 (02) : 181 - 185
  • [35] Grain size effects on the oxidation of two ternary Cu-Ni-20wt.% Cr alloys at 700-800 °C in 1 atm O2
    Niu, Y
    Cao, ZQ
    Gesmundo, F
    Farné, G
    Randi, G
    Wang, CL
    CORROSION SCIENCE, 2003, 45 (06) : 1125 - 1142
  • [36] The corrosion of Fe-15wt% Y and of pure Y and Fe in H2-H2S mixtures under 10-8 atm S2 at 600-800°C
    Niu, Y
    Gesmundo, F
    Zeng, C
    Wu, W
    Viani, F
    Rizzo, F
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2, 1997, 251-2 : 97 - 104
  • [37] Corrosion of Fe-15wt% Y and of pure Y and Fe in H2-H2S mixtures under 10-8 atm S2 at 600-800 °C
    Academia Sinica, Shenyang, China
    Mater Sci Forum, part 1 (97-104):
  • [38] Oxidation of a Three-Phase Cu–45Ni–30Cr Alloy at 700–800°C Under 1 atm O2
    Z. Q. Cao
    F. Gesmundo
    M. Al-Omary
    Y. Niu
    Oxidation of Metals, 2002, 57 : 395 - 407
  • [39] Oxidation of a three-phase Cu-45Ni-30Cr alloy at 700-800°C under 1 atm O2
    Cao, ZQ
    Gesmundo, F
    Al-Omary, M
    Niu, Y
    OXIDATION OF METALS, 2002, 57 (5-6): : 395 - 407
  • [40] Oxidation of Two Ternary Fe–Cu–5 at.% Al Alloys in 1 atm of Pure O2 at 800°C
    J.H. Xiang
    Y. Niu
    F. Gesmundo
    Oxidation of Metals, 2004, 61 : 403 - 421