Experimental study on creep-fatigue behaviors of chinese P92 steel with consideration of several important factors

被引:30
|
作者
Mao, Jianfeng [1 ,4 ]
Li, Xiangyang [1 ]
Wang, Dasheng [2 ]
Zhong, Fengping [3 ]
Luo, Lijia [1 ,4 ]
Bao, Shiyi [1 ,4 ]
Ding, Zhenyu [1 ,4 ]
机构
[1] Zhejiang Univ Technol Hangzhou, Inst Proc Equipment & Control Engn, Hangzhou 310032, Peoples R China
[2] China Nucl Power Engn Co Ltd, State Key Lab Nucl Power Safety Monitoring Techno, Shenzhen 518172, Peoples R China
[3] Zhejiang Acad Special Equipment Sci, Hangzhou, Zhejiang, Peoples R China
[4] Minist Educ, Engn Res Ctr Proc Equipment & Remfg, Beijing, Peoples R China
基金
中国国家自然科学基金; 国家重点研发计划;
关键词
Creep fatigue interaction; Microstructure evolution; Pre-faigue damage; Strain-controlled test; Fracture morphology; LOW-CYCLE FATIGUE; 9-12-PERCENT CR STEEL; LIFE PREDICTION; DAMAGE; ATMOSPHERE; FREQUENCY; MODEL;
D O I
10.1016/j.ijfatigue.2020.105900
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this paper, the creep fatigue test at 550-650 degrees C of P92 steel is carried out, which not only reveals the damage evolution mechanism, but also analyzed the creep fatigue behaviors. The influence of temperature, load holding time and pre-fatigue damage on the creep fatigue behavior of P92 steel was studied in detail. The effects of the temperature and holding time on the hysteresis loops of stress-strain are evaluated quantitatively. Actually, the load holding time mainly affects the stress relaxation behavior. Secondly, pre-fatigue damage will replace the initial stage of cycle stress response and significantly reduce the duration of the stable stage. The linear cu-mulative damage model (LCD), strain range division model (SRD), strain energy density exhaustion model (SEDE) were used to predict the life of P92 steel. Actually, the SEDE model is found to be most suitable for the creep fatigue life prediction. Furthermore, the microstructure of the specimen and fracture at preand posttest was observed to explain the damage evolution mechanism of the creep fatigue interaction. The microstructure analysis shows that the main body of P92 steel is tempered martensite in lath shape, and a large number of M23C6 carbides are dispersed at the grain boundary. The M23C6 carbides have poor thermal stability, which will coarsen and connect after creep, reducing the material properties. The analysis of fracture morphology shows that the creep fatigue specimen with short-term load holding has notable characteristics of fatigue fracture, while the creep fatigue specimen with long-term load holding has notable characteristics of creep fracture.
引用
收藏
页数:15
相关论文
共 50 条
  • [41] Effect of holding duration at maximum and minimum stress on creep fatigue interaction of P92 steel
    Chen, Jia-jia
    Ji, Dong-Mei
    Cai, Xiao-dan
    Wang, Dao-lei
    Dai, Chen
    Wang, Jiong
    MATERIALS AT HIGH TEMPERATURES, 2020, 37 (01) : 51 - 60
  • [42] Characterizations of Creep-fatigue Crack Initiation and Growth Life for P92 using Circular Notched Round Bar Specimen
    Sugiura, R.
    Yokobori, A. T., Jr.
    Nakagawa, T.
    Adachi, T.
    Nonaka, I.
    Tabuchi, M.
    Hasegawa, Y.
    Matsuzaki, T.
    Creep-Fatigue Interactions: Test Methods and Models, 2011, 1539 : 67 - 86
  • [43] Experimental study on high temperature fracture toughness of P92 steel
    Jing H.
    Li S.
    Xu L.
    Zhao L.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (02): : 8 - 12,72
  • [44] Experimental and numerical analysis of creep and damage behavior of P92 steel by small punch tests
    Song, Kai
    Zhao, Lei
    Xu, Lianyong
    Han, Yongdian
    Jing, Hongyang
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2019, 100 : 181 - 190
  • [45] Assessment of prior fatigue damage and a new approach to predict remanent creep rupture of P92 steel
    Zhang, Chunan
    Zhang, Tianyu
    Wang, Xiaowei
    Wen, Jianfeng
    Jiang, Yong
    Gong, Jianming
    Tu, Shantung
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2023, 201
  • [46] Experimental and simulated characterization of creep behavior of P92 steel with prior cyclic loading damage
    Wei Zhang
    Xiaowei Wang
    Jianming Gong
    Yong Jiang
    Xin Huang
    Journal of Materials Science & Technology, 2017, 33 (12) : 1540 - 1548
  • [47] Experimental and simulated characterization of creep behavior of P92 steel with prior cyclic loading damage
    Zhang, Wei
    Wang, Xiaowei
    Gong, Jianming
    Jiang, Yong
    Huang, Xin
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2017, 33 (12) : 1540 - 1548
  • [48] Study on creep mechanical behaviour of P92 steel under multiaxial stress state
    Ni, Y. Z.
    Lan, X.
    Xu, H.
    Mao, X. P.
    MATERIALS AT HIGH TEMPERATURES, 2015, 32 (06) : 551 - 556
  • [49] Creep-fatigue of P92 in service-like tests with combined stress- and strain-controlled dwell times
    Sonntag, Nadja
    Juergens, Maria
    Skrotzki, Birgit
    Olbricht, Juergen
    INTERNATIONAL JOURNAL OF FATIGUE, 2023, 168
  • [50] High Temperature Fracture Parameters Representation and Time Dependent Failure Assessment Diagram Construction for P92 Steel Welded Joint Under Creep-fatigue Interaction
    Zhang G.
    Zhao Y.
    Zhou C.
    Liu Y.
    Liu T.
    Zhang L.
    Li J.
    Zhongguo Dianji Gongcheng Xuebao/Proceedings of the Chinese Society of Electrical Engineering, 2017, 37 (04): : 1160 - 1166